# US 2020/0347469 A1 · High-strength steel having excellent low-yield-ratio characteristics, and manufacturing method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0347469 A1
- Document ID: US20200347469A1
- Status: Published application
- Kind: A1
- Application number: 16/957,333
- Filed: 2018-12-24
- Published: 2020-11-05
- Earliest claimed: 2017-12-24
- Assignees: Posco
- Applicants: Posco
- Inventors: Hwan-Gyo Jung
- Web page: https://patentgrep.com/patent/US20200347469A1

## CPC

- C21D 8/00: Modifying the physical properties of ferrous metals or ferrous alloys by deformation combined with, or followed by, heat treatment (hardening articles or materials formed by forging or rolling with no further heating beyond that required for the formation C21D1/02)
- C21D 6/00: Heat treatment of ferrous alloys
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 6/004: {containing Cr and Ni}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 9/46: for sheet metals
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/06: containing aluminium
- C22C 38/20: with copper
- C22C 38/22: with molybdenum or tungsten
- C22C 38/26: with niobium or tantalum
- C22C 38/28: with titanium or zirconium
- C22C 38/32: with boron
- C22C 38/38: with more than 1.5% by weight of manganese
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/58: with more than 1.5% by weight of manganese
- C21D 2211/002: Bainite
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- C21D 2211/009: Pearlite
- Y02P 10/20: Recycling
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A high-strength steel having excellent low-yield-ratio characteristics, according to one embodiment of the present invention, comprises, by wt %, 0.06-0.12% of C, 0.2-0.5% of Si, 1.5-2.0% of Mn, 0.003-0.05% of Al, 0.01% or less of N, 0.02% or less of P, 0.003% or less of S, 0.05-0.5% of Cr, 0.05-0.5% of Mo, 0.01-0.05% of Nb, 0.0005-0.005% of Ca and the balance of Fe and other inevitable impurities, and comprises polygonal ferrite as a microstructure, wherein the area fraction of the polygonal ferrite is 10-30% and the average hardness of the polygonal ferrite can be 180 Hv or less.

## Claims

### Claim 1

A high-strength steel material having an excellent low yield ratio characteristic, the steel material comprising, by wt %:
0.06 to 0.12% of C, 0.2 to 0.5% of Si, 1.5 to 2.0% of Mn, 0.003 to 0.05% of Al, 0.01% or less of N, 0.02% or less of P, 0.003% of less of S, 0.05 to 0.5% of Cr, 0.05 to 0.5% of Mo, 0.01 to 0.05% of Nb, and 0.0005 to 0.005% of Ca, with a balance of Fe and other unavoidable impurities, and
polygonal ferrite as a microstructure,
wherein the polygonal ferrite has an area fraction of 10 to 30% and an average hardness of 180 Hv or less.

### Claim 2 (depends on 1)

The high-strength steel material having an excellent low yield ratio of claim 1, further comprising: a residual structure having an average hardness of 200 Hv or more,
wherein the residual structure includes acicular ferrite, bainite, pearlite, and martensite.

### Claim 3 (depends on 2)

The high-strength steel material having an excellent low yield ratio of claim 2, wherein a sum of area fractions of the pearlite and the martensite is 10% or less relative to a total area.

### Claim 4 (depends on 1)

The high-strength steel material having an excellent low yield ratio of claim 1, further comprising, by wt o, one or two or more of: 0.05 to 0.3% of Ni, 0.05 to 0.3% of Cu, 0.005 to 0.02% of Ti, and 0.0005 to 0.0015% of B.

### Claim 5 (depends on 1)

The high-strength steel material having an excellent low yield ratio of claim 1, wherein the steel material has a Charpy impact energy at −30° C. of 200 J or more.

### Claim 6 (depends on 1)

The high-strength steel material having an excellent low yield ratio of claim 1, wherein the steel material has a yield ratio of 90% or less.

### Claim 7 (depends on 1)

The high-strength steel material having an excellent low yield ratio of claim 1, wherein the steel material has a tensile strength of 500 MPa or more.

### Claim 8

A method of manufacturing a high-strength steel material having an excellent low yield ratio characteristic, the method comprising:
reheating a slab including, by wt %: 0.06 to 0.12% of C, 0.2 to 0.5% of Si, 1.5 to 2.0% of Mn, 0.003 to 0.05% of Al, 0.01% or less of N, 0.02% or less of P, 0.003% or less of S, 0.05 to 0.5% of Cr, 0.05 to 0.5% of Mo, 0.01 to 0.05% of Nb, and 0.0005 to 0.005% of Ca, with a balance of Fe and other unavoidable impurities at a temperature range of 1100 to 1160° C.;
roughly rolling the reheated slab at an end temperature of 1050° C. or higher;
starting finish rolling of the roughly rolled slab in a temperature range of 980° C. or lower and ending the finish rolling in a temperature range of (Ar3+50° C.) to 900° C.;
first cooling the finish-rolled steel material down to a temperature range of (Ar3−40° C.) to (Ar3−70° C.) at a first cooling rate; and
second cooling the first cooled steel material down to a temperature range of 350 to 400° C. at a second cooling rate.

### Claim 9 (depends on 8)

The method of manufacturing a high-strength steel material having an excellent low yield ratio characteristic of claim 8, wherein an effective reduction ratio of the finish rolling is 65% or more.

### Claim 10 (depends on 8)

The method of manufacturing a high-strength steel material having an excellent low yield ratio characteristic of claim 8, wherein the second cooling rate is higher than the first cooling rate by 10 to 40° C./s.

### Claim 11 (depends on 8)

The method of manufacturing a high-strength steel material having an excellent low yield ratio characteristic of claim 8, wherein a start temperature of the first cooling is (Ar3+10° C.) to (Ar3+30° C.)

### Claim 12 (depends on 8)

The method of manufacturing a high-strength steel material having an excellent low yield ratio characteristic of claim 8, wherein the first cooling rate is 10 to 20° C./s.

### Claim 13 (depends on 8)

The method of manufacturing a high-strength steel material having an excellent low yield ratio characteristic of claim 8, wherein the second cooling is performed directly after the first cooling.

### Claim 14 (depends on 8)

The method of manufacturing a high-strength steel material having an excellent low yield ratio characteristic of claim 8, wherein the second cooling rate is 30 to 50° C./s.

### Claim 15 (depends on 8)

The method of manufacturing a high-strength steel material having an excellent low yield ratio characteristic of claim 8, wherein the second cooled steel material is air-cooled down to room temperature.

### Claim 16 (depends on 8)

The method of manufacturing a high-strength steel material having an excellent low yield ratio characteristic of claim 8, wherein the slab further includes, by wt %, one or two or more of: 0.05 to 0.3% of Ni, 0.05 to 0.3% of Cu, 0.005 to 0.02% of Ti, and 0.0005 to 0.0015% of B.