# US 2020/0347195 A1 · Polyolefin Films Having in-situ Formed Elongated Polyolefin Structures Therein

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0347195 A1
- Document ID: US20200347195A1
- Status: Published application
- Kind: A1
- Application number: 16/816,748
- Filed: 2020-03-12
- Published: 2020-11-05
- Earliest claimed: 2019-05-01
- Assignees: ExxonMobil Chemical Patents Inc.
- Applicants: ExxonMobil Chemical Patents Inc.
- Inventors: Nino Ruocco; Joseph A. Throckmorton; Tamara L. Blanton; Brain J. Rohde
- Web page: https://patentgrep.com/patent/US20200347195A1

## CPC

- C08J 5/18: Manufacture of films or sheets
- B29C 48/0018: {combined with shaping by orienting, stretching or shrinking, e.g. film blowing (B29C48/0017 takes precedence)}
- B29C 48/022: {characterised by the choice of material}
- B29C 48/08: flexible, e.g. films
- B29C 48/91: Heating, e.g. for cross linking
- B29C 48/9135: {of flat articles, e.g. using specially adapted supporting means}
- B29C 48/92: Measuring, controlling or regulating
- C08L 23/06: Polyethylene
- B29K 2023/06: {PE, i.e. polyethylene}
- B29K 2105/0088: {Blends of polymers}
- C08J 2323/06: Polyethene
- C08J 2323/08: Copolymers of ethene (C08J2323/16 takes precedence)
- C08J 2423/06: Polyethene
- C08J 2423/08: Copolymers of ethene (C08J2423/16 takes precedence)
- C08L 2203/16: used for films
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2205/03: containing three or more polymers in a blend
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

This invention relates to a method for forming a film including extruding the film from a polymer melt comprising a first polyolefin and 0.1 wt % to 30 wt % of a second polyolefin, wherein the second polyolefin has a density of at least 0.04 g/cm3 greater than a density of the first polyolefin, wherein a melt flow index of the first polyolefin is within 25% of a melt flow index of the second polyolefin, and wherein a polymer blend consisting of the first and second polyolefins in the same relative amounts as in the film has a multimodal differential scanning calorimetry melting profile above 40° C.; and stretching the film while the film is at a temperature above 25° C. and below the melting point of the second polyolefin to form elongated polyolefin structures in-situ in the film.

## Claims

### Claim 1

A method comprising:
1) extruding a film from a polymer melt comprising a first polyolefin and 0.1 wt % to 30 wt % of a second polyolefin, relative to a total weight of the first and second polyolefins, wherein the second polyolefin has a density of at least 0.04 g/cm3 greater than a density of the first polyolefin, wherein the melt flow index of the first polyolefin is within 25% of the melt flow index of the second polyolefin, and wherein a reference polymer blend consisting of the first and second polyolefins in the same relative amounts as in the film has a multimodal differential scanning calorimetry melting profile above 40° C.; and
2) stretching the film while the film is at a temperature from 25° C. to below the melting point of the second polyolefin to form elongated polyolefin structures in-situ in the film.

### Claim 2 (depends on 1)

The method of claim 1, wherein the second polyolefin is present at 0.1 wt % to 15 wt %.

### Claim 3 (depends on 1)

The method of claim 1 further comprising:
1a) cooling the film after extruding in step 1) and before stretching in step 2) to below the crystallization temperature of the second polyolefin.

### Claim 4 (depends on 3)

The method of claim 3 further comprising:
heating the film, after cooling in step 1a) and before stretching in step 2), at a rate of 30° C./min to 90° C./min up to the temperature from 25° C. to below the melting point of the second polyolefin.

### Claim 5 (depends on 1)

The method of claim 1, further comprising:
cooling the film after stretching in step 2) to a temperature of 0° C. to 40° C.

### Claim 6 (depends on 5)

The method of claim 5, wherein cooling is at a rate of 15° C./min to 100° C./min.

### Claim 7 (depends on 1)

The method of claim 1, wherein the stretching is at a stretching rate of 50 microns per second (μm/s) to 200 μm/s.

### Claim 8

The method of clam 1, wherein the film is stretch up to 800% in a machine direction.

### Claim 9 (depends on 1)

The method of claim 1, wherein the first polyolefin is a first ethylene polymer and the second polyolefin is a second ethylene polymer.

### Claim 10 (depends on 1)

The method of claim 1, wherein the reference blend has a monomodal molecular weight distribution.

### Claim 11 (depends on 1)

The method of claim 1, wherein the elongated polyolefin structures have a length of 0.1 microns to 10 microns according to a Ruland streak method analysis of SAXS scattering data.

### Claim 12 (depends on 1)

The method of claim 1, wherein the film has a degree of misorientation of 0.05 to 0.5 according to a Ruland streak method analysis of SAXS scattering data.

### Claim 13 (depends on 1)

The method of claim 1, wherein the polymer melt further comprises one or more additives selected from the group consisting of: a stabilization agent, an anti-static agent, a crosslink agent, a crosslink promoter, a release agent, an adhesion promoter, a plasticizer, and an anti-agglomeration agent.

### Claim 14

A composition comprising:
a film comprising a first polyolefin and 0.1 wt % to 30 wt % of a second polyolefin, wherein the second polyolefin has a density of at least 0.04 g/cm3 greater than a density of the first polyolefin, wherein a melt flow index of the first polyolefin is within 25% of a melt flow index of the second polyolefin, and wherein a reference polymer blend consisting of the first and second polyolefins in the same relative amounts as in the film, reference blend, has a multimodal differential scanning calorimetry melting profile above 40° C., wherein elongated polyolefin structures are present in the film.

### Claim 15 (depends on 14)

The composition of claim 14, wherein the first polyolefin is a first ethylene polymer and the second polyolefin is a second ethylene polymer.

### Claim 16 (depends on 14)

The composition of claim 14, wherein the reference blend has a monomodal molecular weight distribution.

### Claim 17 (depends on 14)

The composition of claim 14, wherein the elongated polyolefin structures have a length of 0.1 microns to 10 microns according to a Ruland streak method analysis of SAXS scattering data.

### Claim 18 (depends on 14)

The composition of claim 14, wherein the film has a degree of misorientation of 0.05 to 0.5 according to a Ruland streak method analysis of SAXS scattering data.

### Claim 19 (depends on 14)

The composition of claim 14, wherein the film further comprises one or more additives selected from the group consisting of: a stabilization agent, an anti-static agent, a crosslink agent, a crosslink promoter, a release agent, an adhesion promoter, a plasticizer, and an anti-agglomeration agent.

### Claim 20

A method to form a film comprising:
A) forming a polymer melt comprising two or more polyolefins into a film, wherein the polymer melt comprises:
1) 99.9 wt % to 70 wt % of a first polyolefin having:
i) a density of 0.850 g/cm3 to 0.930 g/cm3,
ii) a melt flow index of 0.2 g/10 min to 10 g/10 min, and
iii) a melting temperature Tm of about 50° C. to about 100° C.; and
2) 0.1 wt % to 30 wt % of a second polyolefin having:
i) a density of 0.890 g/cm3 to 0.970 g/cm3, where the density is at least 0.04 g/cm3 greater than the density of the first polyolefin,
ii) a melt flow index of 0.2 g/10 min to 10 g/10 min, and
iii) a Tm of about 80° C. to about 150° C.;
wherein:
I) the melt flow index of the first polyolefin is within 25% of the melt flow index of the second polyolefin,
II) a reference polymer blend consisting of the first and second polyolefins in the same relative amounts as in the composition has a multimodal differential scanning calorimetry melting profile where all peaks are above 40° C.,
III) a melting temperature of the second polyolefin minus a melting temperature of the first polyolefin is about 25° C. to about 100° C.,
IV) the polymer melt is present in a molten state, and
V) optionally, the polymer melt contains less than 1 wt % of added filler, based on the total weight of the first and second polyolefins; and
B) thereafter stretching the film up to 800% in a machine direction at 25 μm/s to 200 μm/s while the film is at a temperature from 25° C. to below the Tm of the second polyolefin to form elongated polyolefin structures in the film;
C) optionally, before stretching in step B), the film can be heated to the stretching temperature at a rate of 15° C./min to 100° C./min; and
D) optionally after stretching in step B), the film can be cooled or quenched to a temperature of 0° C. to 40° C. at a rate of 15° C./min to 100° C./min;
wherein the elongated polyolefin structures have:
I) a length of 0.1 microns to 10 microns, and
II) a degree of misorientation of 0.05 to 0.5.