# US 2020/0346440 A1 · Multilayer Films And Methods Of Making The Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0346440 A1
- Document ID: US20200346440A1
- Status: Published application
- Kind: A1
- Application number: 16/760,002
- Filed: 2018-10-26
- Published: 2020-11-05
- Earliest claimed: 2017-11-28
- Assignees: ExxonMobil Chemical Patents Inc.
- Applicants: ExxonMobil Chemical Patents Inc.
- Inventors: Chiao-Kiat Pey
- Web page: https://patentgrep.com/patent/US20200346440A1

## CPC

- B32B 27/08: of synthetic resin
- B32B 1/00: Layered products having a non-planar shape
- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 27/32: comprising polyolefins {(comprising vinyl (co)polymers or acrylic (co)polymers B32B27/30)}
- B32B 27/327: {comprising polyolefins obtained by a metallocene or single-site catalyst}
- B32B 2250/03: 3 layers
- B32B 2250/05: 5 or more layers
- B32B 2250/24: All layers being polymeric
- B32B 2250/242: All polymers belonging to those covered by group B32B27/32
- B32B 2250/246: All polymers belonging to those covered by groups B32B27/32 and B32B27/30
- B32B 2255/26: Polymeric coating
- B32B 2270/00: Resin or rubber layer containing a blend of at least two different polymers
- B32B 2307/31: Heat sealable
- B32B 2307/514: Oriented
- B32B 2307/516: mono-axially
- B32B 2307/518: bi-axially
- B32B 2307/544: Torsion strength; Torsion stiffness
- B32B 2307/546: Flexural strength; Flexion stiffness
- B32B 2307/558: Impact strength, toughness
- B32B 2307/72: Density
- B32B 2307/7244: Oxygen barrier
- B32B 2307/7246: Water vapor barrier
- B32B 2307/732: Dimensional properties
- B32B 2323/04: Polyethylene
- B32B 2327/18: PTFE, i.e. polytetrafluoroethylene
- B32B 2439/06: Bags, sacks, sachets
- B32B 2439/70: Food packaging
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM

## Abstract

Disclosed are multilayer films with at least one MDO substrate.

## Claims

### Claim 1

A multilayer film, comprising a machine direction oriented (MDO) substrate and a sealant, the MDO substrate comprising a substrate outer layer, a substrate inner layer, and a substrate core layer between the substrate outer layer and the substrate inner layer, wherein:
(a) the substrate core layer comprises a first polyethylene and a second polyethylene, the first polyethylene having (i) a density of about 0.900 to about 0.925 g/cm3, (ii) a melt index (MI), I2.16, of from about 0.1 to about 10.0 g/10 min, (iii) a melt index ratio (MIR), I21.6/I2.16, of from about 15 to about 45, (iv) a weight average molecular weight (Mw) of from about 20,000 to about 200,000; (v) a molecular weight distribution (MWD) of from about 2.0 to about 5.0; and (vi) a z-average molecular weight (Mz) to weight average molecular weight (Mw) (Mz/Mw) ratio of from about 1.7 to about 3.5; the second polyethylene having a higher density than the first polyethylene; and
(b) at least one of the substrate outer layer and the substrate inner layer comprises a third polyethylene, the third polyethylene having a density of about 0.910 to about 0.945 g/cm3, an MI, I2.16, of about 0.1 to about 15 g/10 min, an MWD of about 2.5 to about 5.5, and an MIR, I21.6/I2.16, of about 25 to about 100;
wherein the multilayer film has at least one of the following properties: (i) an average tensile at break of at least about 36 MPa; (ii) an average 1% Secant Modulus of at least about 620 MPa; and (iii) a non-breakage rate of about 100%.

### Claim 2 (depends on 1)

The multilayer film of claim 1, wherein the weight amount ratio between the first polyethylene and the second polyethylene in the substrate core layer is from about 1:5 to about 4:5.

### Claim 3 (depends on 1)

The multilayer film of claim 1, wherein the second polyethylene has a density of about 0.940 to about 0.945 g/cm3, an MI, I2.16, of about 0.1 to about 15 g/10 min, an MWD of about 2.5 to about 5.5, and an MIR, I21.6/I2.16, of about 25 to about 100.

### Claim 4 (depends on 1)

The multilayer film of claim 1, wherein the second polyethylene is the same as the third polyethylene.

### Claim 5 (depends on 1)

The multilayer film of claim 1, wherein the substrate core layer further comprises a fourth polyethylene having a density of at least about 0.940 g/cm3, the fourth polyethylene different from the second polyethylene.

### Claim 6

(canceled)

### Claim 7 (depends on 1)

The multilayer film of claim 1, wherein the substrate outer layer and the substrate inner layer are identical.

### Claim 8 (depends on 1)

The multilayer film of claim 1, wherein the thickness ratio between the substrate outer layer, the substrate core layer, and the substrate inner layer is from about 1:2:1 to about 1:6:1.

### Claim 9 (depends on 1)

The multilayer film of claim 1, wherein the sealant comprises a sealant outer layer, a sealant inner layer, and a sealant core layer between the sealant outer layer and the sealant inner layer, each comprising polyethylene.

### Claim 10 (depends on 9)

The multilayer film of claim 9, wherein the sealant inner layer has a density lower than that of the sealant outer layer.

### Claim 11 (depends on 9)

The multilayer film of claim 9, wherein the thickness ratio between the sealant outer layer, the sealant core layer, and the sealant inner layer is from about 1:2:1 to about 1:6:1.

### Claim 12

(canceled)

### Claim 13

(canceled)

### Claim 14

(canceled)

### Claim 15

A multilayer film, comprising an MDO substrate and a sealant, wherein the MDO substrate comprises a substrate outer layer, a substrate inner layer, and a substrate core layer between the substrate outer layer and the substrate inner layer, wherein:
(a) the substrate core layer comprises a first polyethylene, a second polyethylene, and a fourth polyethylene, wherein the first polyethylene has (i) a density of about 0.900 to about 0.925 g/cm3, (ii) a melt index (MI), I2.16, of from about 0.1 to about 10.0 g/10 min, (iii) a melt index ratio (MIR), I21.6/I2.16, of from about 15 to about 45, (iv) a weight average molecular weight (Mw) of from about 20,000 to about 200,000; (v) a molecular weight distribution (MWD) of from about 2.0 to about 5.0; and (vi) a z-average molecular weight (Mz) to weight average molecular weight (Mw) (Mz/Mw) ratio of from about 1.7 to about 3.5; wherein the second polyethylene has a higher density than the first polyethylene; the second polyethylene having a density of about 0.940 to about 0.945 g/cm3, an MI, I2.16, of about 0.1 to about 15 g/10 min, an MWD of about 2.5 to about 5.5, and an MIR, I21.6/I2.16, of about 25 to about 100; wherein the fourth polyethylene has a density of at least about 0.940 g/cm3, the fourth polyethylene different from the second polyethylene; wherein the weight amount ratio between the first polyethylene and the second polyethylene in the substrate core layer is about 2:3 to about 4:5; and
(b) each of the substrate outer layer and the substrate inner layer comprises about 100 wt % of the second polyethylene, based on total weight of polymer in the layer;
wherein the thickness ratio between the substrate outer layer, the substrate core layer, and the substrate inner layer is about 1:4:1;
wherein the sealant comprises a sealant outer layer, a sealant inner layer, and a sealant core layer between the sealant outer layer and the sealant inner layer, each comprising polyethylene, wherein the sealant inner layer has a density lower than that of the sealant outer layer;
wherein the thickness ratio between the sealant outer layer, the sealant core layer, and the sealant inner layer is 1:2:1;
wherein the substrate inner layer is attached to the sealant outer layer and the thickness ratio between the substrate and the sealant is about 1:5 to about 1:6;
wherein the multilayer film has at least one of the following properties: (i) an average tensile at break of at least about 36 MPa; (ii) an average 1% Secant Modulus of at least about 620 MPa; and (iii) a non-breakage rate of about 100%.

### Claim 16 (depends on 15)

A laminate comprising the multilayer film of claim 15.

### Claim 17 (depends on 16)

A seal comprising the laminate of claim 16.

### Claim 18 (depends on 17)

The seal of claim 17, wherein the seal is formed by using a polytetrafluoroethylene coated fabric one-sided adhesive tape with liner.

### Claim 19

A method for making a multilayer film comprising an MDO substrate and a sealant, comprising the steps of:
(a) preparing a substrate outer layer, a substrate inner layer, and a substrate core layer between the substrate outer layer and the substrate inner layer, wherein the substrate core layer comprises a first polyethylene and a second polyethylene, and at least one of the substrate outer layer and the substrate inner layer comprises a third polyethylene;
(b) preparing an MDO substrate comprising the layers in step (a); and
(c) forming a film comprising the substrate in step (b);
wherein the first polyethylene has (i) a density of about 0.900 to about 0.925 g/cm3, (ii) a melt index (MI), I2.16, of from about 0.1 to about 10.0 g/10 min, (iii) a melt index ratio (MIR), I21.6/I2.16, of from about 15 to about 45, (iv) a weight average molecular weight (Mw) of from about 20,000 to about 200,000; (v) a molecular weight distribution (MWD) of from about 2.0 to about 5.0; and (vi) a z-average molecular weight (Mz) to weight average molecular weight (Mw) (Mz/Mw) ratio of from about 1.7 to about 3.5; the second polyethylene has a higher density than the first polyethylene; and the third polyethylene has a density of about 0.910 to about 0.945 g/cm3, an MI, I2.16, of about 0.1 to about 15 g/10 min, an MWD of about 2.5 to about 5.5, and an MIR, I21.6/I2.16, of about 25 to about 100;
wherein the multilayer film has at least one of the following properties: (i) an average tensile at break of at least about 36 MPa; (ii) an average 1% Secant Modulus of at least about 620 MPa; and (iii) a non-breakage rate of about 100%.

### Claim 20 (depends on 19)

The method of claim 19, further comprising after step (b) a step of preparing a sealant comprising a sealant outer layer, a sealant inner layer, and a sealant core layer between the sealant outer layer and the sealant inner layer.

### Claim 21 (depends on 19)

The method of claim 19, wherein at least one of the substrate and the sealant is formed by blown extrusion, cast extrusion, coextrusion, blow molding, casting, or extrusion blow molding.

### Claim 22 (depends on 19)

The method of claim 19, wherein the film in step (c) is formed by laminating the sealant to the substrate, so that the substrate inner layer is attached to the sealant outer layer.

### Claim 23

(canceled)

### Claim 24 (depends on 19)

The method of claim 19, further comprising after step (c) a step of forming a seal comprising the film in step (c).

### Claim 25 (depends on 24)