# US 2020/0307057 A1 · Method to fabricate glassy-metal polymer composites

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0307057 A1
- Document ID: US20200307057A1
- Status: Published application
- Kind: A1
- Application number: 16/862,924
- Filed: 2020-04-30
- Published: 2020-10-01
- Earliest claimed: 2017-10-30
- Assignees: Khalifa University of Science and Technology
- Applicants: Khalifa University of Science and Technology
- Inventors: Saeed Mohammed Salem Alhassan Alkhazraji; Mariam Hamad Rashed Mohamed Rashed Alrashed
- Web page: https://patentgrep.com/patent/US20200307057A1

## CPC

- B29C 48/022: {characterised by the choice of material}
- D01F 1/10: Other agents for modifying properties
- B29C 48/05: Filamentary, e.g. strands
- B29C 48/29: in liquid form
- B29C 48/525: Conical screws
- B29K 2023/065: {HDPE, i.e. high density polyethylene}
- B29K 2025/04: {Polymers of styrene}
- B29K 2505/12: Iron
- D01F 1/103: {Agents inhibiting growth of microorganisms}
- D01F 6/04: from polyolefins
- D01F 6/22: from polystyrene
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

A method for the production of a glassy metal polymer composite is disclosed. The method comprises adding a polymer and a metal to an extruder, wherein the extruder is heated to an extrusion temperature greater than the melting point of the polymer and the melting point of the metal; mixing the metal and the polymer in the extruder for a predefined residence time; and co-extruding the composite from the extruder.

## Claims

### Claim 1

A method for the production of a glassy-metal polymer composite comprising the steps of:
adding a polymer and a metal to an extruder, wherein the extruder is heated to an extrusion temperature greater than the melting point of the polymer and the melting point of the metal; mixing the metal and the polymer in the extruder for a predefined residence time; and co-extruding the composite from the extruder.

### Claim 2 (depends on 1)

The method of claim 1, wherein the melting point of the metal is lower than the melting point of the polymer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the melting point of the metal does not exceed the melting point of the polymer by 35° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein the composite in form of a melt is extruded at room temperature after a minimum residence time of 10 minutes

### Claim 5 (depends on 1)

The method of claim 1, wherein the extruder has an extruder barrel with conical screws and a feedstock of polymer is added to the extruder, wherein the extruder barrel is firstly fed with a fraction of the feedstock of polymer to form a polymer layer on the surface of the conical screws

### Claim 6 (depends on 5)

The method of claim 5, wherein, for the remaining fraction of polymer, the metal is fed with the polymer concurrently for metals with low melt viscosity.

### Claim 7 (depends on 5)

The method of claim 5, wherein, for the remaining fraction of polymer, the metal is fed to the barrel after the polymer, for metals with high melt viscosity.

### Claim 8 (depends on 7)

The method of claim 7, wherein the metal is fed to the barrel after the polymer at a gradual pace of five to fifteen seconds between each feed

### Claim 9 (depends on 1)

The method of claim 1, wherein the extruder is twin-screw extruder with a heated mixing barrel having twin counter-rotating conical screws.

### Claim 10 (depends on 1)

The method of claim 1, wherein the metal is selected from group XIII of the periodic table not exceeding 35° C. from polymer melting point.

### Claim 11 (depends on 1)

The method of claim 1, wherein the metal can be a liquid metal and/or low melt eutectic metal.

### Claim 12

The method of any of the above claims, wherein the extruder is a screw extruder and has a rotation speed of 100 rotations per minute

### Claim 13 (depends on 1)

The method of claim 1, wherein the glassy-metal polymer composite is one of In-HDPE and In-PS composite.

### Claim 14 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13)

Molded article comprising a glassy metal-polymer composites produced by the method of any one of the claims 1 to 13.

### Claim 15 (depends on 14)

The molded articles of claim 14, wherein the articles are fibers.

### Claim 16 (depends on 14, 15)

The molded articles of claim 14 or 15, wherein the degree of crystallinity is a maximum of 13%.