# US 2020/0298372 A1 · Thermal treatment and shot peening method for wheel

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0298372 A1
- Document ID: US20200298372A1
- Status: Published application
- Kind: A1
- Application number: 16/693,880
- Filed: 2019-11-25
- Published: 2020-09-24
- Earliest claimed: 2019-03-22
- Assignees: CITIC Dicastal Co., Ltd.
- Applicants: CITIC Dicastal CO., LTD.
- Inventors: Tieqiang CHEN; Chunhai LIU
- Web page: https://patentgrep.com/patent/US20200298372A1

## CPC

- B24C 1/10: for compacting surfaces, e.g. shot-peening (for deforming sheet metal, tubes or profiles B21D31/06; as a metallurgical treatment C21D7/00, C22F1/00)
- B60B 1/006: {specially adapted for light-weight wheels, e.g. of strollers or wheel-chairs (B60B1/003 takes precedence)}
- B60B 3/00: Disc wheels, i.e. wheels with load-supporting disc body (non- metallic B60B5/00; wheel cover discs B60B7/00 {; disc wheels comprising rail-engaging elements B60B17/0006})
- B60B 2310/208: by forging
- B60B 2310/542: Quenching
- B60B 2310/622: Shot-peening
- B60B 2360/104: Aluminum
- B24C: ABRASIVE OR RELATED BLASTING WITH PARTICULATE MATERIAL
- B60B: VEHICLE WHEELS (making wheels or wheel parts by rolling B21H1/00, by forging, hammering or pressing B21K1/28); CASTORS; AXLES FOR WHEELS OR CASTORS; INCREASING WHEEL ADHESION

## Abstract

A thermal treatment and shot peening method for a wheel, including: heating a wheel blank to T1, and preserving the heat for t1; fast heating the wheel blank to T2, and preserving the heat for t2; performing quenching treatment, wherein a quenching medium is at temperature of T3, and the quenching transfer time is t3; performing aging treatment at aging temperature of T4, and preserving the heat for t4; performing first-stage shot peening; and performing second-stage shot peening.

## Claims

### Claim 1

A thermal treatment and shot peening method for a wheel, comprising the following steps:
S1, heating a wheel blank to T1, and preserving the heat for t1;
S2, fast heating the wheel treated in S1 to T2, and preserving the heat for t2;
S3, quenching the wheel treated in S2, wherein a quenching medium is at temperature T3, and the quenching transfer time is t3;
S4, performing aging treatment on the wheel treated in S3 at aging temperature of T4, and preserving the heat for t4;
S5, performing first-stage shot peening on the wheel treated in S4 under the following conditions: a shot diameter is d1, a nozzle distance is D1, an impact angle is A1, a shot flow is F1 and a shot speed is V1; and
S6, performing second-stage shot peening on the wheel treated in S5 under the following conditions: a shot diameter is d2, a nozzle distance is D2, an impact angle is A2, a shot flow is F2 and a shot speed is V2.

### Claim 2 (depends on 1)

The thermal treatment and shot peening method for a wheel according to claim 1, wherein the shot diameter dl is greater than the shot diameter d2.

### Claim 3 (depends on 1)

The thermal treatment and shot peening method for a wheel according to claim 1, wherein the T1 is 350 to 450 DEG C., and the t1 is 150 to 300 min; the T2 is 470 to 550 DEG C., and the t2 is 100 to 200 min; and the T3 is 50 to 80 DEG C., and the t3 is 10 to 20 min.

### Claim 4 (depends on 2)

The thermal treatment and shot peening method for a wheel according to claim 2, wherein the T1 is 350 to 450 DEG C., and the t1 is 150 to 300 min; the T2 is 470 to 550 DEG C., and the t2 is 100 to 200 min; and the T3 is 50 to 80 DEG C., and the t3 is 10 to 20 min.

### Claim 5 (depends on 4)

The thermal treatment and shot peening method for a wheel according to claim 4, wherein the d1 is 0.7 to 0.9 mm; the D1 is 155 to 165 mm; the A1 is 30 to 90 degrees; the F1 is 6.5 to 8.2 kg/min; the V1 is 110 to 150 m/s; the d2 is 0.2 to 0.5 mm; the D2 is 145 to 165 mm; the A2 is 30 to 90 degrees; the F2 is 3.5 to 5.5 kg/min; and the V2 is 100 to 120 m/s.

### Claim 6 (depends on 5)

The thermal treatment and shot peening method for a wheel according to claim 5, wherein the shot is a cast steel shot.

### Claim 7 (depends on 1)

The thermal treatment and shot peening method for a wheel according to claim 1, wherein the quenching medium is water or a water-based organic polymer.

### Claim 8 (depends on 2)

The thermal treatment and shot peening method for a wheel according to claim 2, wherein the quenching medium is water or a water-based organic polymer.