# US 2020/0291239 A1 · Method of milling minerals in the presence of a poly (itaconate)

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0291239 A1
- Document ID: US20200291239A1
- Status: Published application
- Kind: A1
- Application number: 16/342,431
- Filed: 2017-11-08
- Published: 2020-09-17
- Earliest claimed: 2016-11-14
- Assignees: Coatex
- Applicants: Coatex
- Inventors: Henri GRONDIN; Christian JACQUEMET; Benoit MAGNY
- Web page: https://patentgrep.com/patent/US20200291239A1

## CPC

- C08F 122/02: Acids; Metal salts or ammonium salts thereof {, e.g. maleic acid or itaconic acid}
- C09C 3/041: {Grinding}
- C08F 2/10: Aqueous solvent
- C08F 2/38: Polymerisation using regulators, e.g. chain terminating agents {, e.g. telomerisation}
- C08F 8/00: Chemical modification by after-treatment (graft polymers, block polymers, crosslinking with unsaturated monomers or with polymers C08F251/00 - C08F299/00; of conjugated diene rubbers C08C)
- C08F 8/44: Preparation of metal salts or ammonium salts
- C08F 222/02: Acids; Metal salts or ammonium salts thereof {, e.g. maleic acid or itaconic acid}
- C08K 3/32: Phosphorus-containing compounds
- C09C 1/021: {Calcium carbonates}
- C09C 1/025: {Calcium sulfates}
- C09C 1/027: {Barium sulfates}
- C09C 1/3063: {Treatment with low-molecular organic compounds}
- C09C 1/3072: {Treatment with macro-molecular organic compounds}
- C09C 1/3623: {Grinding}
- C09C 1/42: Clays
- D21D 99/00: Subject matter not provided for in other groups of this subclass
- D21H 19/64: Inorganic compounds
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C09C: TREATMENT OF INORGANIC MATERIALS, OTHER THAN FIBROUS FILLERS, TO ENHANCE THEIR PIGMENTING OR FILLING PROPERTIES (treatment of materials specially adapted to enhance their filling properties in mortars, concrete or artificial stone C04B14/00, C04B18/00, C04B20/00); PREPARATION OF CARBON BLACK {; PREPARATION OF INORGANIC MATERIALS WHICH ARE NO SINGLE CHEMICAL COMPOUNDS AND WHICH ARE MAINLY USED AS PIGMENTS OR FILLERS}
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- D21D: TREATMENT OF THE MATERIALS BEFORE PASSING TO THE PAPER-MAKING MACHINE
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR

## Abstract

The invention relates to a method for producing particles of mineral material comprising grinding of at least one mineral material in the presence of water. The grinding according to the invention is carried out in the presence of at least one polymer obtained by a radical polymerization reaction of a partial sodium salt of itaconic acid and partial decarboxylation of the polymer obtained followed by partial or total neutralization of the decarboxylated polymer. The invention also relates to an aqueous composition comprising particles of ground mineral material and such a polymer, in particular a mass-loading composition for the production of paper or a paper-coating-colour composition.

## Claims

### Claim at position 1

1: A method for producing mineral material particles, the method comprising grinding, in the presence of water, at least one mineral material in the presence of at least one polymer obtained:
(a) by a radical polymerization reaction in the presence of sodium hypophosphite, at a temperature above 50° C., of a partial sodium salt of itaconic acid and partial decarboxylation of the polymer obtained, to obtain a decarboxylated polymer; and
(b) partial or total neutralization of the decarboxylated polymer with a derivative comprising sodium.

### Claim at position 2 (depends on 1)

2: The method according to claim 1, wherein the particles have a size of less than 50 μm.

### Claim at position 3 (depends on 1)

3: The method according to claim 1, wherein
only one mineral material or two or three mineral substances are used; or
the mineral material is synthetic or of natural origin.

### Claim at position 4 (depends on 1)

4: The method according to claim 1, wherein the polymerization reaction is carried out:
in water, in a solvent, alone or in a mixture with water; or
in the presence of at least one radical generating compound; or
in the presence of at least one other chain transfer agent.

### Claim at position 5 (depends on 1)

5: The method according to claim 1, wherein:
the first acidity of itaconic acid is partially salified and the second acidity of itaconic acid is not salified; or
the first acidity of itaconic acid is totally salified and the second acidity of itaconic acid is not salified; or
the first acidity of itaconic acid is totally salified and the second acidity of itaconic acid is partially salified.

### Claim at position 6 (depends on 1)

6: The method according to claim 1, wherein the polymer:
has a weight average molecular mass MW (measured by CES) less than 20,000 g/mol; or
has a weight average molecular mass MW (measured by CES) greater than 1,000 g/mol or greater than 1,200 g/mol; or
has an IP polymolecularity index of less than 4.

### Claim at position 7 (depends on 1)

7: The method according to claim 1, wherein:
the itaconic acid polymer is partially decarboxylated; or
from 5 to 90 mol % of the second acidity of the polymer are decarboxylated.

### Claim at position 8 (depends on 1)

8: The method according to claim 1, wherein:
the itaconic acid polymer is totally neutralized or neutralized to 40 mol; or
the polymer is neutralized with sodium hydroxide, sodium carbonate, or sodium bicarbonate.

### Claim at position 9 (depends on 1)

9: The method according to claim 1, wherein:
the aqueous suspension of mineral material particles having a median size of 1.5±0.15 μm has a cationic demand less than or equal in absolute value to 5μ-equivalent per g of suspension of particles in water at a concentration of 65 to 75% by weight; or
the aqueous suspension of mineral material particles with a median size of 0.7±0.15 μm has a cationic demand less than or equal in absolute value to 13μ-equivalent per g of suspension of particles in water at a concentration of 65 to 75% by weight.

### Claim at position 10 (depends on 1)

10: An aqueous composition, comprising mineral material particles produced by the method of claim 1.

### Claim at position 11 (depends on 10)

11: The composition according to claim 10, wherein:
an aqueous suspension of mineral material particles with a median size of 1.5±0.15 μm has a cationic demand less than or equal in absolute value to 5μ-equivalent per g of suspension of particles in water at a concentration of 65 to 75% by weight; or
an aqueous suspension of mineral material particles with a median size of 0.7±0.15 μm has a cationic demand less than or equal in absolute value to 13μ-equivalent per g of suspension of particles in water at a concentration of 65 to 75% by weight.

### Claim at position 12 (depends on 10)

12: The composition according to claim 10, further comprising at least one cellulosic material and optionally at least one additive.

### Claim at position 13

13: A method for producing a paper-mass-loading composition or a paper-coating colour composition, the method comprising grinding, in the presence of water, at least one mineral material in the presence of at least one polymer obtained:
(a) by a radical polymerization reaction in the presence of sodium hypophosphite, at a temperature above 50° C., of a partial sodium salt of itaconic acid and partial decarboxylation of the polymer obtained, to obtain a decarboxylated polymer; and then
(b) partial or total neutralization of the decarboxylated polymer with a derivative comprising sodium,
to form an aqueous suspension of particles of mineral material.

### Claim at position 14

14: A grinding aid for particles of mineral material, the grinding aid comprising a polymer obtained:
(a) by a radical polymerization reaction in the presence of sodium hypophosphite, at a temperature above 50° C., of a partial sodium salt of itaconic acid and partial decarboxylation of the polymer obtained, to obtain a decarboxylated polymer; then
(b) partial or total neutralization of the decarboxylated polymer with a derivative comprising sodium.

### Claim at position 15 (depends on 14)

15: The grinding aid according to claim 14, wherein the particles have a size of less than 50 μm.

### Claim at position 16 (depends on 10)

16: A method, comprising of producing paper with the aqueous composition of claim 10.

### Claim at position 17 (depends on 16)

17: The method according to claim 16, wherein an amount of cationic agent in the aqueous composition is reduced compared to a conventional papermaking process.