# US 2020/0288577 A1 · Electronic-Component Manufacturing Method and Electronic Components

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0288577 A1
- Document ID: US20200288577A1
- Status: Published application
- Kind: A1
- Application number: 16/626,574
- Filed: 2018-09-19
- Published: 2020-09-10
- Earliest claimed: 2017-11-21
- Assignees: Qualtec Co., Ltd.
- Applicants: Qualtec Co., Ltd.
- Inventors: Satoshi Oya; Seiichi Kaihara; Hiroshi Atarashi; Hirokazu Shikata
- Web page: https://patentgrep.com/patent/US20200288577A1

## CPC

- H05K 3/188: {by direct electroplating}
- C23C 18/1605: {by masking}
- C23C 18/1608: {from pretreatment step, i.e. selective pre-treatment}
- C23C 18/1612: {through irradiation means}
- C23C 18/1653: {Two or more layers with at least one layer obtained by electroless plating and one layer obtained by electroplating}
- C23C 18/1689: {After-treatment}
- C23C 18/1868: {Radiation, e.g. UV, laser}
- C23C 18/1893: {with use of organic or inorganic compounds other than metals, first}
- C23C 18/204: {Radiation, e.g. UV, laser}
- C23C 18/2086: {with use of organic or inorganic compounds other than metals, first}
- C23C 18/22: Roughening, e.g. by etching
- C23C 18/285: {Sensitising or activating with tin based compound or composition}
- C23C 18/30: Activating {or accelerating or sensitising with palladium or other noble metal}
- C23C 18/40: using reducing agents
- C25D 5/02: Electroplating of selected surface areas
- C25D 5/56: of plastics
- C25D 7/00: Electroplating characterised by the article coated
- H05K 3/107: {by filling grooves in the support with conductive material (H05K3/045, H05K3/101, H05K3/1258 and H05K3/465 take precedence)}
- H05K 3/381: {by special treatment of the substrate}
- H05K 3/0032: {of organic insulating material}
- H05K 3/045: {by making a conductive layer having a relief pattern, followed by abrading of the raised portions}
- H05K 3/108: {by semi-additive methods; masks therefor (characterised by metallic etch mask H05K3/062; electroplating methods or apparatus H05K3/241)}
- H05K 2201/0376: Flush conductors, i.e. flush with the surface of the printed circuit
- H05K 2201/09036: Recesses or grooves in insulating substrate
- H05K 2203/025: Abrading, e.g. grinding or sand blasting
- H05K 2203/11: Treatments characterised by their effect, e.g. heating, cooling, roughening
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

Provided are an electronic component manufacturing method by which even a platable layer made of a difficult-to-plate material can be easily plated with good adhesion without using a special chemical solution or a photolithography technique, and an electronic component which has a peel strength of 0.1 N/mm or greater as measured by a copper foil peel test. A picosecond laser beam having a pulse duration on the order of a picosecond or a femtosecond laser beam having a pulse duration on the order of a femtosecond is emitted at a surface of a platable layer (2) in order to roughen the surface, a wiring pattern is formed using a mask (13), and a plated part (12) is formed on the surface of the wiring pattern.

## Claims

### Claim at position 1

1-13. (canceled)

### Claim at position 2

14: A method of manufacturing an electronic component in which interconnects are formed on a front surface of a substrate, the electronic-component manufacturing method comprising:
a first step of shining either a picosecond laser beam in which the pulse-width units are picoseconds, or a femtosecond laser beam in which they are femtoseconds, on the front surface of the substrate to roughen the substrate front surface and to form thereon an interconnect pattern of squarish trenches;
a second step of forming a first metallization layer on the front surface of the substrate; and
a third step of polishing the first metallization layer to remove the first metallization layer apart from the interconnect pattern.

### Claim at position 3 (depends on 14)

15: The electronic-component manufacturing method set forth in claim 14, further comprising:
a fourth step, following said third step, of forming a second metallization layer onto the first metallization layer; and
a fifth step of baking the substrate at 80 to 200° C.

### Claim at position 4 (depends on 14)

16: The electronic-component manufacturing method set forth in claim 14, further comprising:
a fourth step, following said third step, of forming a second metallization layer by electrolytic Cu plating onto the first metallization layer; wherein
said second step forms the first metallization layer by electroless Cu plating.

### Claim at position 5 (depends on 14)

17: The electronic-component manufacturing method set forth in claim 14, wherein the substrate is of a material being any of an acrylic resin, PET, PTFE, glass, an epoxy resin, a liquid-crystal polymer, or a polyimide resin.

### Claim at position 6 (depends on 14)

18: The electronic-component manufacturing method set forth in claim 14, wherein:
the femtosecond laser beam is of 500 nm to 530 nm wavelength, and the femtosecond laser beam has a pulse width of 1 femtosecond to 1000 femtoseconds; and
the picosecond laser beam is of 500 nm to 530 nm wavelength, and the picosecond laser beam has a pulse width of 1 picosecond to 10 picoseconds.

### Claim at position 7 (depends on 14)

19: The electronic-component manufacturing method set forth in claim 14, wherein said first step roughens the front surface of the substrate to an arithmetic mean roughness Ra of not less than 0.2 μm.

### Claim at position 8 (depends on 14)

20: The electronic-component manufacturing method set forth in claim 14, wherein said second step forms the first metallization layer by electroless Cu plating utilizing a plating solution in the strong alkali region, with formalin being the reducing agent.

### Claim at position 9

21: A method of manufacturing an electronic component in which interconnects are formed on a front surface of a substrate, the electronic-component manufacturing method comprising:
a first step of forming a mask onto the front surface of the substrate;
a second step of shining either a picosecond laser beam in which the pulse-width units are picoseconds, or a femtosecond laser beam in which they are femtoseconds, superficially on the mask to form an interconnect pattern of squarish trenches in the mask and the substrate;
a third step of applying a catalyst superficially on the interconnect pattern of squarish trenches and superficially on the mask;
a fourth step of employing an alkaline solution to exfoliate the mask; and
a fifth step of forming on the front surface of the substrate a metallization layer in accordance with the applied catalyst.

### Claim at position 10 (depends on 21)

22: The electronic-component manufacturing method set forth in claim 21, wherein said fifth step forms the metallization layer by electroless Cu plating.

### Claim at position 11 (depends on 21)

23: The electronic-component manufacturing method set forth in claim 21, wherein the substrate is of a material being any of an acrylic resin, PET, PTFE, glass, an epoxy resin, a liquid-crystal polymer, or a polyimide resin.

### Claim at position 12 (depends on 21)

24: The electronic-component manufacturing method set forth in claim 21, wherein:
the femtosecond laser beam is of 500 nm to 530 nm wavelength, and the femtosecond laser beam has a pulse width of 1 femtosecond to 1000 femtoseconds; and
the picosecond laser beam is of 500 nm to 530 nm wavelength, and the picosecond laser beam has a pulse width of 1 picosecond to 10 picoseconds.

### Claim at position 13 (depends on 21)

25: The electronic-component manufacturing method set forth in claim 21, wherein in said second step, the picosecond laser beam or the femtosecond laser beam is shone on the front surface of the substrate to roughen the front surface to an arithmetic mean roughness Ra of not less than 0.2 μm.

### Claim at position 14 (depends on 21)

26: The electronic-component manufacturing method set forth in claim 21, wherein said fifth step forms the metallization layer by electroless Cu plating utilizing a plating solution in the strong alkali region, with formalin being the reducing agent.

### Claim at position 15 (depends on 21)

27: The electronic-component manufacturing method set forth in claim 21, wherein the mask in said first step contains an acrylic polymer of the alkaline-soluble type.

### Claim at position 16 (depends on 21)

28: The electronic-component manufacturing method set forth in claim 21, wherein in said third step the catalyst is an SnPd catalyst.

### Claim at position 17 (depends on 21)

29: The electronic-component manufacturing method set forth in claim 21, wherein the mask includes a colorant, a dye, or a pigment.

### Claim at position 18 (depends on 21)

30: The electronic-component manufacturing method set forth in claim 21, wherein in said second step patterning of the interconnect pattern is carried out based on marks formed on the substrate or the mask.

### Claim at position 19 (depends on 21)

31: The electronic-component manufacturing method set forth in claim 21, wherein said second step of shining a laser beam superficially on the mask to form an interconnect pattern of squarish trenches in the mask and the substrate at the same time roughens the front surface of the substrate.

### Claim at position 20

32: An electronic component in which interconnects are formed on a front surface of a substrate, the electronic component characterized in that:
the substrate contains a material selected from acrylic resins, PET, PTFE, glass, epoxy resins, liquid-crystal polymers, and polyimide resins;
the front surface of the substrate corresponding to the interconnects is laser-beam-irradiation roughened;
the interconnects are Cu metallization formed by Cu plating; and
the Cu metallization protrudes from the surface of the substrate in a rectangular form or a trapezoidal form when viewed sideways.

### Claim at position 21 (depends on 32)

33: The electronic component set forth in claim 32, wherein the Cu metallization is constituted by electrolessly plated first Cu metallization, and by electrolytically plated second Cu metallization.