# US 2020/0287237 A1 · Copper Ionic Conductor Film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0287237 A1
- Document ID: US20200287237A1
- Status: Published application
- Kind: A1
- Application number: 16/296,027
- Filed: 2019-03-07
- Published: 2020-09-10
- Earliest claimed: 2019-03-07
- Assignees: International Business Machines Corporation
- Applicants: International Business Machines Corporation
- Inventors: Teodor K. Todorov; Douglas M. Bishop; John Collins; Frances M. Ross
- Web page: https://patentgrep.com/patent/US20200287237A1

## CPC

- H01M 10/0562: Solid materials
- H01G 11/56: Solid electrolytes, e.g. gels; Additives therein
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/13915: containing halogen atoms, e.g. LiCoOxFy
- H01M 4/582: {Halogenides}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Copper ionic conductor films and method of making the same are provided. In one aspect, a method of forming a crystalline ionic conductor film includes: depositing a mixture of sources for components of the crystalline ionic conductor film onto a substrate, the components including: i) Cu, ii) a component A selected from: Rb, Cs, K, Na and/or Li, and iii) a component B selected from: F, Cl, Br and/or I; and annealing the mixture under conditions sufficient to form the crystalline ionic conductor film on the substrate having a formula: CuxAyBz, wherein 0<x<20, 0<y<10, and 0<z<30. A device having a crystalline ionic conductor film as an electrolyte and method of forming the device are also provided.

## Claims

### Claim 1

A method of forming a crystalline ionic conductor film, the method comprising the steps of:
depositing a mixture of sources for components of the crystalline ionic conductor film onto a substrate, the components comprising: i) copper (Cu), ii) a component A selected from the group consisting of: rubidium (Rb), caesium (Cs), potassium (K), sodium (Na), lithium (Li), and combinations thereof, and iii) a component B selected from the group consisting of: fluorine (F), chlorine (Cl), bromine (Br), iodine (I), and combinations thereof; and
annealing the mixture under conditions sufficient to form the crystalline ionic conductor film on the substrate comprising a metal halide having a formula:
CuxAyBz,
wherein 0<x<20, 0<y<10, and 0<z<30.

### Claim 2 (depends on 1)

The method of claim 1, wherein the conditions comprise a temperature that is less than a melting point of the mixture.

### Claim 3 (depends on 1)

The method of claim 1, wherein the conditions comprise a temperature of from about 50° C. to about 200° C. and ranges therebetween.

### Claim 4 (depends on 1)

The method of claim 1, wherein the conditions comprise a duration of from about 2 minutes to about 360 minutes and ranges therebetween.

### Claim 5 (depends on 1)

The method of claim 1, wherein the ionic conductor film comprises rubidium copper iodide chloride.

### Claim 6 (depends on 5)

The method of claim 5, wherein the rubidium copper iodide chloride has a formula Rb4Cu16I7Cl13.

### Claim 7 (depends on 1)

The method of claim 1, wherein the crystalline ionic conductor film has an ionic conductivity of greater than about 0.34 Siemens per centimeter (S/cm).

### Claim 8 (depends on 1)

The method of claim 1, wherein the crystalline ionic conductor film has an ionic conductivity of from about 0.34 S/cm to about 1 S/cm and ranges therebetween.

### Claim 9 (depends on 1)

The method of claim 1, wherein the steps are performed in an ambient of inert gas.

### Claim 10 (depends on 9)

The method of claim 9, wherein the inert gas is selected from the group consisting of: nitrogen, argon, and combinations thereof.

### Claim 11 (depends on 1)

The method of claim 1, wherein the mixture is deposited onto the substrate using a vacuum evaporation process.

### Claim 12 (depends on 1)

The method of claim 1, wherein the sources are selected from the group consisting of: copper fluoride (CuF2), copper bromide (CuBr2), copper iodide (CuI), copper chloride (CuCl2), rubidium fluoride (RbF), rubidium bromide (RbBr), rubidium iodide (RbI), rubidium chloride (RbCl), caesium fluoride (CsF), caesium bromide (CsBr), caesium iodide (CsI), caesium chloride (CsCl), potassium fluoride (KF), potassium bromide (KBr), potassium iodide (KI), potassium chloride (KCl), sodium fluoride (NaF), sodium bromide (NaBr), sodium iodide (NaI), sodium chloride (NaCl), lithium fluoride (LiF), lithium bromide (LiBr), lithium iodide (LiI), lithium chloride (LiCl), and combinations thereof.

### Claim 13 (depends on 1)

The method of claim 1, further comprising the step of:
combining the sources to form a blend.

### Claim 14 (depends on 13)

The method of claim 13, further comprising the steps of:
melting the blend;
cooling the blend to form a solid product;
grinding the solid product into a powder;
re-melting the powder to form a melted product; and
quenching the melted product to form the mixture of the sources.

### Claim 15 (depends on 14)

The method of claim 14, further comprising the step of:
repeating the melting, cooling, grinding, re-melting and quenching.

### Claim 16 (depends on 14)

The method of claim 14, wherein the melting is performed at a temperature of from about 200° C. to about 350° C. and ranges therebetween, for a duration of from about 1 minute to about 10 minutes and ranges therebetween.

### Claim 17

A method of forming a device, the method comprising the steps of:
providing a substrate comprising a cathode;
forming an electrolyte on the substrate by: depositing a mixture of sources for components of the crystalline ionic conductor film onto a substrate, the components comprising: i) Cu, ii) a component A selected from the group consisting of: Rb, Cs, K, Na, Li, and combinations thereof, and iii) a component B selected from the group consisting of: F, Cl, Br, I, and combinations thereof; and annealing the mixture under conditions sufficient to form a crystalline ionic conductor film as the electrolyte on the substrate comprising a metal halide having a formula: CuxAyBz, wherein 0<x<20, 0<y<10, and 0<z<30; and
forming an anode on the electrolyte.

### Claim 18 (depends on 17)

The method of claim 17, wherein the conditions comprise a temperature that is less than a melting point of the mixture.

### Claim 19

A device, comprising:
a substrate comprising a cathode;
an electrolyte disposed on the substrate, the electrolyte comprising a crystalline ionic conductor film having a formula: CuxAyBz, wherein A is selected from the group consisting of: Rb, Cs, K, Na, Li, and combinations thereof, wherein B is selected from the group consisting of: F, Cl, Br, I, and combinations thereof, and wherein 0<x<20, 0<y<10, and 0<z<30; and
an anode disposed on the electrolyte.

### Claim 20 (depends on 19)

The device of claim 19, wherein the crystalline ionic conductor film has an ionic conductivity of greater than about 0.34 S/cm.