# US 2020/0287220 A1 · Method for producing gas diffusion electrode substrate and fuel cell

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0287220 A1
- Document ID: US20200287220A1
- Status: Published application
- Kind: A1
- Application number: 16/494,846
- Filed: 2018-03-30
- Published: 2020-09-10
- Earliest claimed: 2017-04-03
- Assignees: Toray Industries, Inc.
- Applicants: Toray Industries, Inc.
- Inventors: Katsuya Sode; Michio Wakatabe; Yusuke Iwasaki
- Web page: https://patentgrep.com/patent/US20200287220A1

## CPC

- H01M 4/8807: {Gas diffusion layers}
- H01M 8/0234: Carbonaceous material
- H01M 4/88: Processes of manufacture
- H01M 4/8882: {Heat treatment, e.g. drying, baking}
- H01M 8/0239: Organic resins; Organic polymers
- H01M 8/0243: in the form of mixtures
- H01M 8/0245: in the form of layered or coated products
- H01M 8/0284: Organic resins; Organic polymers
- H01M 8/10: Fuel cells with solid electrolytes
- H01M 2008/1095: {Fuel cells with polymeric electrolytes}
- Y02E 60/50: Fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention provides a method for efficiently producing a gas diffusion electrode substrate having excellent adhesion property. This method is a method for producing a gas diffusion electrode substrate having a porous layer on at least one surface of an electroconductive porous substrate which includes the steps of a coating step wherein a coating solution containing electroconductive particles, a water-repellant material, a dispersion medium, and a surfactant is coated on the electroconductive porous substrate, a drying step wherein heating is conducted at a temperature lower than the temperature of a first heat treatment step, the first heat treatment step wherein the heating is conducted at a temperature lower than the melting point of the water-repellant material, and a second heat treatment step wherein the heating is conducted at a temperature higher than the melting point of the water-repellant material, wherein the coating solution contains at least 0.09 part by weight and up to 0.27 part by weight of the water-repellant material in relation to 1 part by weight of the electroconductive particles, the first heat treatment step is conducted by heating for a time of 0.2 minute to 3.0 minutes, and the second heat treatment step is conducted by heating for a time of up to 2.9 minutes.

## Claims

### Claim 1

A method for producing a gas diffusion electrode substrate having a porous layer on at least one surface of an electroconductive porous substrate, the method comprising the steps of:
a coating step wherein a coating solution containing electroconductive particles, a water-repellant material, a dispersion medium, and a surfactant is coated on the electroconductive porous substrate;
a drying step wherein the coated electroconductive porous substrate is heated at a temperature lower than the temperature of a first heat treatment step;
the first heat treatment step wherein the heating is conducted at a temperature lower than the melting point of the water-repellant material; and
a second heat treatment step wherein the heating is conducted at a temperature higher than the melting point of the water-repellant material; wherein:
the coating solution contains at least 0.09 part by weight and up to 0.27 part by weight of the water-repellant material in relation to 1 part by weight of the electroconductive particles,
the first heat treatment step is conducted by heating for a time of 0.2 minute to 3.0 minutes, and
the second heat treatment step is conducted by heating for a time of up to 2.9 minutes.

### Claim 2 (depends on 1)

A method for producing a gas diffusion electrode substrate according to claim 1 wherein the second heat treatment step is conducted by heating to a temperature of at least 330° C. and up to 364° C. for a time of at least 0.2 minute and up to 2.7 minutes.

### Claim 3 (depends on 1)

A method for producing a gas diffusion electrode substrate according to claim 1 wherein the first heat treatment step is conducted by heating for a time of at least 0.2 minute and up to 1.5 minutes, and
the second heat treatment step is conducted by heating to a temperature of at least 365° C. for a time of at least 0.2 minute and up to 1.5 minutes.

### Claim 4 (depends on 1)

A method for producing gas diffusion electrode substrate according to claim 1 wherein the water-repellant material is polytetrafluoroethylene (PTFE).

### Claim 5 (depends on 1)

A fuel cell prepared by using the gas diffusion electrode substrate prepared by using the method according to claim 1.