# US 2020/0287215 A1 · Positive active material for rechargeable lithium battery, method of preparing the same and rechargeable lithium battery including the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0287215 A1
- Document ID: US20200287215A1
- Status: Published application
- Kind: A1
- Application number: 16/809,460
- Filed: 2020-03-04
- Published: 2020-09-10
- Earliest claimed: 2019-03-05
- Assignees: Samsung SDI Co., Ltd.
- Applicants: Samsung SDI Co., Ltd.
- Inventors: Young-Ki KIM; Jungjoon PARK; Soonrewl LEE; Youngjoo CHAE; Ickkyu CHOI; Mingzi HONG; Soonkie HONG
- Web page: https://patentgrep.com/patent/US20200287215A1

## CPC

- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/366: {as layered products}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/027: {Negative electrodes}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A positive active material for a rechargeable lithium battery includes a first compound represented by Chemical Formula 1, and a second compound having a smaller particle diameter than the first compound and represented by Chemical Formula 2, wherein the first compound and the second compound have a Ni content of about 50 at % to about 60 at % based on a total amount of metal elements excluding Li. A rechargeable lithium battery including the first compound and the second compound satisfies Relation 1: Vs<V1≤3.6. [Relation 1] In Relation 1, V1 is a voltage value at a point where a tangent line to a value corresponding to 50% of the first peak value intersects the line dQ/dV=0, and Vs is a charge start voltage, as determined from a differential capacity (dQ/dV)-voltage charge/discharge plot.

## Claims

### Claim 1

A positive active material for a rechargeable lithium battery, the positive active material comprising:
a first compound represented by Chemical Formula 1, and
a second compound having a smaller particle diameter than the first compound and represented by Chemical Formula 2,
wherein the first compound and the second compound each have a Ni content of about 50 at % to about 60 at % based on the total amount of metal elements excluding Li, and
a rechargeable lithium battery comprising the first compound and the second compound satisfies Relation 1, as determined from a differential capacity (dQ/dV)-voltage charge/discharge plot:
LiaNixCoyM1zO2 [Chemical Formula 1]
LiaNixCoyM2zO2 [Chemical Formula 2]
wherein, in Chemical Formula 1 and Chemical Formula 2, 0.9≤a≤1.05, 0.5≤x≤0.6, 0.05≤y≤0.35, 0.05≤z≤0.35, x+y+z=1, and M1 and M2 are each independently at least one metal element selected from Mn, Al, Cr, Fe, V, Mg, Ti, Zr, Nb, Mo, W, Cu, Zn, Ga, In, Sn, La, and Ce,
Vs<V1≤3.6 [Relation 1]
wherein, in Relation 1, V1 is a voltage value at a point where a tangent line to a value corresponding to 50% of the first peak value of the differential capacity (dQ/dV)-voltage charge/discharge plot intersects the line dQ/dV=0, and Vs is a charge start voltage.

### Claim 2 (depends on 1)

The positive active material of claim 1, wherein the charge start voltage (Vs) of the rechargeable lithium battery is less than or equal to about 3.55 V.

### Claim 3 (depends on 1)

The positive active material of claim 1, wherein the voltage (V1) is less than or equal to about 3.58 V.

### Claim 4 (depends on 1)

The positive active material of claim 1, wherein the voltage (V1) is about 3.50 V to about 3.58 V.

### Claim 5 (depends on 1)

The positive active material of claim 1, wherein a differential capacity (dQ/dV)-voltage charge/discharge plot has at least two peak values in the range of about 3.60 V to about 3.85 V, and the second peak value is larger than the first peak value.

### Claim 6 (depends on 5)

The positive active material of claim 5, wherein the first peak value is about 450 mAhg−1V−1 to about 550 mAhg−1V−1, and the second peak value is about 550 mAhg−1V−1 to about 650 mAhg−1V−1.

### Claim 7 (depends on 1)

The positive active material of claim 1, wherein at least one of the first compound and the second compound comprises a core and a surface layer surrounding the core,
a Ni atom concentration (at %) based on the total amount of metal elements excluding Li is higher in the surface layer than in the core, and
a cation mixing of the positive active material is less than or equal to about 3%.

### Claim 8 (depends on 7)

The positive active material of claim 7, wherein the surface layer is a region corresponding to a depth of about 200 nm from the surface of the first compound or the second compound.

### Claim 9 (depends on 1)

The positive active material of claim 1, wherein the first compound has an average particle diameter (D50) of about 15 μm to about 20 μm.

### Claim 10 (depends on 1)

The positive active material of claim 1, wherein the second compound has an average particle diameter (D50) of about 2 μm to about 5 μm.

### Claim 11 (depends on 1)

The positive active material of claim 1, wherein the second compound has a needle-shape, a sheet-shape, or a combination thereof.

### Claim 12 (depends on 1)

The positive active material of claim 1, wherein the first compound and the second compound are mixed in a weight ratio of about 90:10 to about 50:50.

### Claim 13

A method of preparing a positive active material, the method comprising:
mixing Compound 1A represented by Chemical Formula 1A, Compound 2A represented by Chemical Formula 2A having a smaller particle diameter than Compound 1A, and a lithium salt to prepare a mixture;
first heat-treating the mixture under a rapid temperature-increasing condition to prepare a first fired product comprising residual lithium; and
second heat-treating the first fired product to prepare the positive active material:
NixCoyM1z(OH)2 [Chemical Formula 1A]
NixCoyM2z(OH)2 [Chemical Formula 2A]
wherein, in Chemical Formula 1A and Chemical Formula 2A, 0.5≤x≤0.6, 0.05≤y≤0.35, 0.05≤z≤0.35, x+y+z=1, and M1 and M2 are each independently selected from Mn, Al, Cr, Fe, V, Mg, Ti, Zr, Nb, Mo, W, Cu, Zn, Ga, In, Sn, La, and Ce.

### Claim 14 (depends on 13)

The method of claim 13, wherein Compound 1A and Compound 2A are mixed in a weight ratio of about 90:10 to about 50:50.

### Claim 15 (depends on 13)

The method of claim 13, wherein in the mixture, a mole ratio of Li/(Ni+Co+Mn) is greater than or equal to about 0.99.

### Claim 16 (depends on 13)

The method of claim 13, wherein the first heat-treating comprises a process of maintaining the mixture at about 800° C. to about 1000° C. for about 1 hour to about 4 hours.

### Claim 17 (depends on 13)

The method of claim 13, wherein Compound 2A has a needle-shape, a sheet-shape, or a combination thereof.

### Claim 18 (depends on 1)

A rechargeable lithium battery, comprising:
a positive electrode comprising the positive active material of claim 1;
a negative electrode comprising a negative active material; and
an electrolyte.