# US 2020/0287213 A1 · Positive Electrode Active Material for Lithium Secondary Battery, Method of Preparing the Same, and Positive Electrode for Lithium Secondary Battery and Lithium Secondary Battery which Include the Positive Electrode Active Material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0287213 A1
- Document ID: US20200287213A1
- Status: Published application
- Kind: A1
- Application number: 16/754,582
- Filed: 2018-10-19
- Published: 2020-09-10
- Earliest claimed: 2017-10-20
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Seo Hee Ju
- Web page: https://patentgrep.com/patent/US20200287213A1

## CPC

- H01M 4/366: {as layered products}
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- C01B 35/121: {of alkali metal}
- C01G 53/504: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.5, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.5
- C01G 53/506: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.8, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.8
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 4/628: {Inhibitors, e.g. gassing inhibitors, corrosion inhibitors}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/4235: {Safety or regulating additives or arrangements in electrodes, separators or electrolyte (H01M10/4242 takes precedence)}
- C01P 2004/80: Particles consisting of a mixture of two or more inorganic phases
- C01P 2006/40: Electric properties
- H01M 2004/028: {Positive electrodes}
- H01M 2300/0008: Phosphoric acid-based
- H01M 2300/0011: Sulfuric acid-based
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A positive electrode active material includes a nickel-containing lithium transition metal oxide containing nickel in an amount of 60 mol % or more based on a total number of moles of transition metals excluding lithium, and a lithium-containing inorganic compound layer formed on a surface of the nickel-containing lithium transition metal oxide, wherein the positive electrode active material has a first peak in a range of 5 eV or less, a second peak in a range of 7 eV to 13 eV, and a third peak in a range of 20 eV to 30 eV when intensity is measured by X-ray photoelectron spectroscopy, and the first peak has a maximum value of 80% to 120% with respect to the third peak. A method of preparing the positive electrode active material, and a positive electrode and a lithium secondary battery are also provided.

## Claims

### Claim 1

A positive electrode active material comprising:
a nickel-containing lithium transition metal oxide containing nickel in an amount of 60 mol % or more based on a total number of moles of transition metals excluding lithium; and
a lithium-containing inorganic compound layer formed on a surface of the nickel-containing lithium transition metal oxide,
wherein the positive electrode active material has a first peak in a range of 5 eV or less, a second peak in a range of 7 eV to 13 eV, and a third peak in a range of 20 eV to 30 eV when intensity is measured by X-ray photoelectron spectroscopy, and the first peak has a maximum value of 80% to 120% with respect to the third peak.

### Claim 2 (depends on 1)

The positive electrode active material of claim 1, wherein the nickel-containing lithium transition metal oxide is represented by Formula 1:
Li1+a(NibCOcXdM1e)1−aO2 [Formula 1]
wherein, in Formula 1,
X is at least one selected from the group consisting of manganese (Mn) and aluminum (Al),
M1 is at least one selected from the group consisting of zirconium (Zr), boron (B), cobalt (Co), Al, tungsten (W), magnesium (Mg), cerium (Ce), tantalum (Ta), titanium (Ti), strontium (Sr), barium (Ba), hafnium (Hf), fluorine (F), phosphorus (P), lanthanum (La), and yttrium (Y), and
0≤a≤0.1, 0.6≤b≤1.0, 0≤c≤0.3, 0≤d≤0.3, and 0≤e≤0.1.

### Claim 3 (depends on 1)

The positive electrode active material of claim 1, wherein the lithium-containing inorganic compound layer comprises at least one selected from the group consisting of Li3BO3, Li3PO4, LiPO3, LiP2O7, α-Li4B2O5, β-Li4B2O5, Li6B4O9, α-LiBO2, Li2B4O7, Li3B7O12, LiB3O5, and Li2B8O13.

### Claim 4 (depends on 1)

The positive electrode active material of claim 1, wherein the lithium-containing inorganic compound layer has a thickness of 1 nm to 200 nm.

### Claim 5 (depends on 1)

The positive electrode active material of claim 1, wherein electrical conductivity, which is measured after the positive electrode active material is prepared in a form of a pellet by compressing the positive electrode active material at a rolling load of greater than 0 kN and equal to or less than 20 kN, is in a range of 5 mS/cm to 30 mS/cm.

### Claim 6

A method of preparing a positive electrode active material, the method comprising:
mixing an aqueous inorganic acid solution with a nickel-containing lithium transition metal oxide containing nickel in an amount of 60 mol % or more based on a total number of moles of transition metals excluding lithium to prepare a suspension having a pH of 8 to 12;
forming a lithium-containing inorganic compound by reacting the lithium transition metal oxide with inorganic acid included in the aqueous inorganic acid solution; and
drying and heat-treating the suspension to form a lithium-containing inorganic compound layer on a surface of the lithium transition metal oxide.

### Claim 7 (depends on 6)

The method of claim 6, wherein the aqueous inorganic acid solution has a pH of greater than 6 and equal to or less than 10.

### Claim 8 (depends on 6)

The method of claim 6, wherein the aqueous inorganic acid solution comprises at least one selected from the group consisting of boric acid, phosphoric acid, hydrochloric acid, nitric acid, sulfuric acid, carbonic acid, hydrofluoric acid, and hydrobromic acid.

### Claim 9 (depends on 6)

The method of claim 6, wherein the nickel-containing lithium transition metal oxide is mixed in an amount of 50 parts by weight to 90 parts by weight based on 100 parts by weight of the aqueous inorganic acid solution.

### Claim 10 (depends on 6)

The method of claim 6, wherein the heat treatment is performed at 200° C. to 500° C.

### Claim 11 (depends on 1)

A positive electrode for a lithium secondary battery, the positive electrode comprising the positive electrode active material of claim 1.

### Claim 12 (depends on 11)

A lithium secondary battery comprising the positive electrode of claim 11.

### Claim 13 (depends on 1)

The positive electrode active material of claim 1, wherein the nickel-containing lithium transition metal oxide containing nickel is present in an amount of 60 mol % to 99 mol % based on the total number of the moles of the transitional metals excluding the lithium.