# US 2020/0287212 A1 · Method of producing positive electrode active material for nonaqueous electrolyte secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0287212 A1
- Document ID: US20200287212A1
- Status: Published application
- Kind: A1
- Application number: 16/881,940
- Filed: 2020-05-22
- Published: 2020-09-10
- Earliest claimed: 2016-03-31
- Assignees: Nichia Corporation
- Applicants: Nichia Corporation
- Inventors: Kenichi KOBAYASHI; Yukiko SANO
- Web page: https://patentgrep.com/patent/US20200287212A1

## CPC

- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- C01G 53/40: Complex oxides containing nickel and at least one other metal element
- C01G 53/42: containing alkali metals, e.g. LiNiO2
- C01G 53/502: containing lithium and cobalt
- C01G 53/84: Hydroxides
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2004/03: obtained by SEM
- C01P 2004/51: Particles with a specific particle size distribution
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/40: Electric properties
- H01M 10/052: Li-accumulators
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method of producing a positive electrode active material for a nonaqueous electrolyte secondary battery, the method includes preparing nickel-containing composite oxide particles having a ratio 1D90/1D10 of a 90% particle size 1D90 to a 10% particle size 1D10 in volume-based cumulative particle size distribution is 3 or less; mixing the composite oxide particles and a lithium compound to obtain a first mixture; subjecting the first mixture to a first heat treatment at a first temperature and a second heat treatment at a second temperature higher than the first temperature to obtain a first heat-treated product; and subjecting the first heat-treated material to a dispersion treatment.

## Claims

### Claim 1

A method of producing a positive electrode active material for a nonaqueous electrolyte secondary battery, comprising:
providing nickel-containing composite oxide particles having a ratio 1D90/1D10 of a 90% particle size 1D90 to a 10% particle size 1D10 in volume-based cumulative particle size distribution of 3 or less;
mixing the composite oxide particles and a lithium compound to obtain a first mixture;
subjecting the first mixture to a first heat treatment at a first temperature and a second heat treatment at a second temperature higher than the first temperature to obtain a first heat-treated material; and
dissociating from the first heat-treated material the positive electrode active material,
wherein the positive electrode active material comprises lithium-transition metal composite oxide particles being single particles,
wherein the lithium-transition metal composite oxide particles have a ratio 2D90/2D10 of a 90% particle size 2D90 to a 10% particle size 2D10 in volume-based cumulative particle size distribution is 4 or less, and
wherein a molar ratio of nickel in a composition of the lithium-transition metal composite oxide to a total molar number of metals other than lithium is 0.3 to 0.6.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the lithium-transition metal composite oxide further contains cobalt and a molar ratio of cobalt in the composition to a total molar number of metals other than lithium is 0.4 or less.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the lithium-transition metal composite oxide further contains at least one of Mn or Al and a molar ratio of total molar number of Mn and Al in the composition to a total molar number of metals other than lithium is 0.5 or less.

### Claim 4 (depends on 1)

The method according to claim 1, wherein a molar ratio of lithium in the composition to a total molar number of metals other than lithium is 1.0 to 1.3.

### Claim 5 (depends on 1)

The method according to claim 1, wherein a molar ratio of oxygen in the composition to a total molar number of metals other than lithium is 1.9 to 2.1.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the lithium-transition metal composite oxide particles have a composition represented by the following formula (1):
LipNixCoyM1zO2+α (1)
wherein p, x, y, z, and a satisfy 1.0≤p≤1.3, 0.3≤x≤0.6, 0≤y≤0.4, 0≤z≤0.5, x+y+z=1, and −0.1≤α≤0.1, and M1 represents at least one of Mn and Al.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the first temperature is in a range of 850° C. to 950° C., and the second temperature is in a range of 980° C. to 1,100° C.

### Claim 8 (depends on 1)

The method according to claim 1, further comprising:
mixing the positive electrode active material dissociated from the first heat-treated material and a lithium compound to obtain a second mixture; and
subjecting the second mixture to a heat treatment to obtain a second heat-treated material.

### Claim 9 (depends on 7)

The method according to claim 7, further comprising:
mixing the positive electrode active material dissociated from the first heat-treated material and a lithium compound to obtain a second mixture; and
subjecting the second mixture to a heat treatment to obtain a second heat-treated material.

### Claim 10 (depends on 1)

The method according to claim 1, wherein
the composite oxide particles have a 50% particle size 1D50 in volume-based cumulative particle size distribution is in a range of 1 μm to 4 μm, and
the lithium-transition metal composite oxide particles are configured such that the 50% particle size 2D50 in volume-based cumulative particle size distribution is in a range of 1 μm to 3 μm.

### Claim 11 (depends on 7)

The method according to claim 7, wherein
the composite oxide particles have a 50% particle size 1D50 in volume-based cumulative particle size distribution is in a range of 1 μm to 4 μm, and
the lithium-transition metal composite oxide particles are configured such that the 50% particle size 2D50 in volume-based cumulative particle size distribution is in a range of 1 μm to 3 μm.

### Claim 12 (depends on 8)

The method according to claim 8, wherein
the composite oxide particles have a 50% particle size 1D50 in volume-based cumulative particle size distribution is in a range of 1 μm to 4 μm, and
the lithium-transition metal composite oxide particles are configured such that the 50% particle size 2D50 in volume-based cumulative particle size distribution is in a range of 1 μm to 3 μm.

### Claim 13 (depends on 9)

The method according to claim 9, wherein
the composite oxide particles have a 50% particle size 1D50 in volume-based cumulative particle size distribution is in a range of 1 μm to 4 μm, and
the lithium-transition metal composite oxide particles are configured such that the 50% particle size 2D50 in volume-based cumulative particle size distribution is in a range of 1 μm to 3 μm.

### Claim 14 (depends on 6)

The method according to claim 6, wherein p in formula (1) satisfies 1.1≤p≤1.2.