# US 2020/0287174 A1 · Method of forming a package

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0287174 A1
- Document ID: US20200287174A1
- Status: Published application
- Kind: A1
- Application number: 16/883,085
- Filed: 2020-05-26
- Published: 2020-09-10
- Earliest claimed: 2004-12-10
- Assignees: Murata Manufacturing Co., Ltd.
- Applicants: Murata Manufacturing Co., Ltd.
- Inventors: Kazuhito HATTA; Mashio SHIBUYA
- Web page: https://patentgrep.com/patent/US20200287174A1

## CPC

- H01M 50/124: having a layered structure
- B29C 65/02: by heating, with or without pressure
- B29C 65/08: using ultrasonic vibrations {(non-plastics element to plastics elements B29C65/645)}
- B29C 65/18: using heated tools
- B29C 66/1122: {Single lap to lap joints, i.e. overlap joints (B29C66/45, B29C66/472, B29C66/52272 take precedence)}
- B29C 66/32: {Measures for keeping the burr form under control; Avoiding burr formation; Shaping the burr (deburring welded articles B29C37/04)}
- B29C 66/41: {Joining substantially flat articles (B29C66/47 and subgroups take precedence); Making flat seams in tubular or hollow articles (B29C66/51 and subgroups take precedence)}
- B29C 66/433: {Casing-in, i.e. enclosing an element between two sheets by an outlined seam (for bookbinding B42C11/06; for packaging B65B; by laminating B32B37/00; enclosing tubular articles between substantially flat elements B29C66/53261)}
- B29C 66/71: {characterised by the composition of the plastics material of the parts to be joined (welding bar compositions B29C65/125)}
- B29C 66/72321: {consisting of metals or their alloys}
- B29C 66/7352: {Thickness, e.g. very thin}
- B29C 66/83221: {cooperating reciprocating tools, each tool reciprocating along one axis}
- B32B 5/142: {Variation across the area of the layer}
- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 15/08: of synthetic resin
- B32B 15/085: comprising polyolefins
- B32B 15/088: comprising polyamides
- B32B 15/09: comprising polyesters
- B32B 15/20: comprising aluminium or copper {(B32B15/016 and B32B15/017 take precedence)}
- B32B 27/32: comprising polyolefins {(comprising vinyl (co)polymers or acrylic (co)polymers B32B27/30)}
- B32B 27/34: comprising polyamides
- B32B 27/36: comprising polyesters
- H01M 4/06: Electrodes for primary cells
- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/623: {fluorinated polymers}
- H01M 4/625: {Carbon or graphite}
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 6/02: Details (of electrodes H01M4/00; of non-active parts H01M50/00)
- H01M 6/164: {by the solvent}
- H01M 6/166: {by the solute}
- H01M 6/181: {with polymeric electrolytes}
- H01M 10/0431: {Cells with wound or folded electrodes (H01M10/045 takes precedence)}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0565: Polymeric materials, e.g. gel-type or solid-type
- H01M 10/0568: characterised by the solutes
- H01M 10/0569: characterised by the solvents
- H01M 10/0587: of accumulators having only wound construction elements, i.e. wound positive electrodes, wound negative electrodes and wound separators
- H01M 50/126: comprising three or more layers
- H01M 50/133: Thickness
- H01M 50/141: for protecting against humidity
- H01M 50/44: Fibrous material
- H01M 50/46: Separators, membranes or diaphragms characterised by their combination with electrodes
- B29C 66/112: {Single lapped joints}
- B29C 66/131: {Single flanged joints, i.e. one of the parts to be joined being rigid and flanged in the joint area}
- B29C 66/53461: {joining substantially flat covers and/or substantially flat bottoms to open ends of container bodies}
- B29C 66/549: {said hollow-preforms being interconnected during their moulding process, e.g. by a hinge}
- B29C 66/81431: {comprising a single cavity, e.g. a groove}
- B29K 2023/12: {PP, i.e. polypropylene}
- B29K 2623/12: {PP, i.e. polypropylene}
- B29K 2655/00: Use of specific polymers obtained by polymerisation reactions only involving carbon-to-carbon unsaturated bonds, not provided for in a single one of main groups {B29K2623/00 - B29K2649/00, e.g. having a vinyl group,} for preformed parts, e.g. for inserts
- B29K 2705/02: Aluminium
- B29L 2031/3468: {Batteries, accumulators or fuel cells (battery cases B29L2031/7146)}
- B29L 2031/7146: {Battery-cases}
- B32B 2250/03: 3 layers
- B32B 2255/06: on metal layer
- B32B 2274/00: Thermoplastic elastomer material
- B32B 2323/10: Polypropylene
- B32B 2367/00: Polyesters, e.g. PET, i.e. polyethylene terephthalate
- B32B 2457/10: Batteries
- B32B 2553/00: Packaging equipment or accessories not otherwise provided for
- H01M 50/178: for pouch or flexible bag cells
- H01M 50/417: Polyolefins
- H01M 50/55: on the same side of the cell
- H01M 50/553: Terminals adapted for prismatic, pouch or rectangular cells
- H01M 50/562: characterised by the material
- H01M 50/566: by welding, soldering or brazing
- H01M 2220/30: Batteries in portable systems, e.g. mobile phone, laptop
- H01M 2300/0037: Mixture of solvents
- H01M 2300/0082: Organic polymers
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method of forming a package is provided and includes providing two laminate edge portions of the package, each of which includes a foil layer between first and second resin layers; and welding together the respective first resin layers at a first position spaced apart from the edges while not welding the respective first resin layers at the edges, wherein the edge portions include edges from which electrode terminals extend such that portions of the electrode terminals are exposed beyond the edges, and wherein the edge portions are between a sealing portion and exposed portions of positive and negative electrode terminals.

## Claims

### Claim 1

(canceled)

### Claim 2

A method of forming a battery comprising:
providing a cell;
enclosing at least a portion of the cell with a laminate film that includes an exterior layer, a metal layer, and an interior layer; and
welding a portion of the laminate film to form a welded portion; wherein
when a thickness of the interior layer before the step of welding is p, a thickness of the laminate film before the step of welding is t, and a thickness of the welded portion is t1,
a following equation is satisfied:
t×2−p×2+5<t1<t×2−5(μm).

### Claim 3 (depends on 2)

The method according to claim 2, wherein
the step of welding includes compressing and heating to form the welded portion and does not include directly welding an edge portion of the laminate film such that the edge portion is a non-compressed portion; and
in the step of welding, a portion of the interior layer in the welded portion flows into the interior layer of the edge portion.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the step of welding forms a welded layer of the interior layer that increases in thickness towards an end portion of the welded layer.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the thickness of the welded layer in the welded portion is greater than 5 μm.

### Claim 6 (depends on 5)

The method according to claim 5, further comprising providing an electrode terminal coated with a sealant, wherein
the electrode terminal and the sealant extend outside the non-compressed portion of the laminate film that has not been direct-welded.

### Claim 7 (depends on 6)

The method according to claim 6, wherein
the step of welding includes thermal welding; and
the welded portion includes no electrode terminal.

### Claim 8 (depends on 2)

The method according to claim 2, wherein the thickness t1 is thinner than a thickness t2 of an edge portion of the laminate film.

### Claim 9 (depends on 8)

The method according to claim 8, wherein thicknesses t1, t2, and t satisfy a following equation:
t1<t×2<t2.

### Claim 10 (depends on 9)

The method according to claim 9, wherein
the welded portion and the edge portion have a y-shape in cross-section that includes a trunk attached to two arms;
the welded portion defines the trunk; and
the edge portion defines the two arms.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the welded portion extends along a peripheral portion of the cell or the laminate film.

### Claim 12 (depends on 11)

The method according to claim 11, further comprising:
providing an electrode terminal that extends from the cell; and
coating a sealant on both sides of the electrode terminal.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the electrode terminal and the sealant extend outside a non-compressed portion of the laminate film that has not been direct-welded.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the cell is a lithium ion cell.

### Claim 15 (depends on 14)

The method according to claim 14, wherein the exterior layer includes one or both of a nylon and a polyethylene terephthalate (PET).

### Claim 16 (depends on 14)

The method according to claim 14, wherein the metal layer includes aluminum.

### Claim 17 (depends on 14)

The method according to claim 14, wherein the interior layer includes a polypropylene.

### Claim 18 (depends on 10)

The method according to claim 10, wherein the step of welding includes welding the laminate film and an additional laminate film to form the welded portion.

### Claim 19 (depends on 18)

The method according to claim 18, wherein the welded portion extends along a peripheral portion of the cell or the laminate film.

### Claim 20 (depends on 19)

The method according to claim 19, wherein
the step of welding includes compressing and heating to form the welded portion and does not include directly welding an edge portion of the laminate film such that the edge portion is a non-compressed portion; and
in the step of welding, a portion of the interior layer in the welded portion flows into the interior layer of the edge portion.

### Claim 21 (depends on 20)

The method according to claim 20, wherein the step of welding forms a welded layer of the interior layer of the welded portion that increases in thickness towards an end portion of the welded layer.

### Claim 22 (depends on 21)

The method according to claim 21, wherein the thickness of the welded layer in the welded portion is greater than 5 μm.

### Claim 23 (depends on 22)

The method according to claim 22, wherein the cell is a lithium ion cell.

### Claim 24 (depends on 23)

The method according to claim 23, further comprising providing an electrode terminal coated with a sealant, wherein
the electrode terminal and the sealant extend outside the non-compressed portion.

### Claim 25 (depends on 24)

The method according to claim 24, wherein the welded portion includes no electrode terminal.

### Claim 26 (depends on 10)

The method according to claim 10, further comprising, before the step of welding, folding the laminate film such that two parts of the laminate film overlap.

### Claim 27 (depends on 26)

The method according to claim 26, wherein the step of welding forms a welded layer of the interior layer that increases in thickness towards an end portion of the welded layer.

### Claim 28 (depends on 27)

The method according to claim 27, wherein the thickness of the welded layer in the welded portion is greater than 5 μm.

### Claim 29 (depends on 28)

The method according to claim 28, wherein the cell is a lithium ion cell.