# US 2020/0287137 A1 · Processing of perovskite films using inks with complexing agents

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0287137 A1
- Document ID: US20200287137A1
- Status: Published application
- Kind: A1
- Application number: 16/808,175
- Filed: 2020-03-03
- Published: 2020-09-10
- Earliest claimed: 2019-03-06
- Assignees: Tandem PV
- Applicants: Tandem PV, Inc.
- Inventors: Colin David Bailie; Chris Eberspacher; Matthew Cornyn Kuchta
- Web page: https://patentgrep.com/patent/US20200287137A1

## CPC

- H10K 71/12: using liquid deposition, e.g. spin coating
- H01G 9/2059: {comprising an organic dye as the active light absorbing material, e.g. adsorbed on an electrode or dissolved in solution}
- H10K 71/13: using printing techniques, e.g. ink-jet printing or screen printing
- H10K 71/40: Thermal treatment, e.g. annealing in the presence of a solvent vapour
- H10K 71/441: {in the presence of solvent vapors, e.g. solvent vapour annealing}
- H10K 85/50: Organic perovskites; Hybrid organic-inorganic perovskites [HOIP], e.g. CH3NH3PbI3
- H10K 2102/102: {comprising tin oxides, e.g. fluorine-doped SnO2}
- Y02E 10/542: Dye sensitized solar cells
- Y02E 10/549: Organic PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method can comprise providing an ink comprising reactants, a complexing agent, and a solvent, depositing the ink onto a substrate to form a wet film, drying the wet film to form a precursor layer, and annealing the precursor layer to form a perovskite film. The reactants can comprise a first and a second cation, a first metal, and a first and a second anion, wherein the first and second cations are different from each other, and the first and second anions are different from each other. The complexing agent can comprise a heterocyclic donor material. The perovskite film can comprise a mixed-cation mixed-halide perovskite material, and less than 5% by mass of the complexing agent. The perovskite film can also be formed using a one-step process.

## Claims

### Claim 1

A method, comprising:
providing an ink comprising reactants, a complexing agent, and a solvent, wherein:
the reactants comprise a first and a second cation, a first metal, and a first and a second anion, wherein the first and second cations are different from each other, and the first and second anions are different from each other;
the complexing agent comprises a heterocyclic donor material;
depositing the ink onto a substrate to form a wet film;
drying the wet film to form a precursor layer; and
annealing the precursor layer to form a perovskite film, wherein:
the perovskite film comprises a mixed-cation mixed-halide perovskite material;
the perovskite film comprises less than 5% by mass of the complexing agent; and
the perovskite film is formed using a one-step process.

### Claim 2 (depends on 1)

The method of claim 1, wherein the heterocyclic donor material is selected from the group consisting of oxygen donors, nitrogen donors, nitrogen-oxygen donors, phosphorous donors, sulfur donors, and selenium donors.

### Claim 3 (depends on 1)

The method of claim 1, wherein the heterocyclic donor material is selected from the group consisting of a material listed in Table 1.

### Claim 4 (depends on 1)

The method of claim 1, wherein the heterocyclic donor material is selected from the group consisting of pyridine, 4-substituted pyridines, quinoline, and iso-quinoline derivatives.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first and second cations are each selected from the group consisting of methylammonium, formamidinium, Cs, K, and Rb.

### Claim 6 (depends on 1)

The method of claim 1, wherein the first metal is selected from the group consisting of lead and tin.

### Claim 7 (depends on 1)

The method of claim 1, wherein:
the reactants further comprises a second metal;
the first metal is lead; and
the second metal is tin.

### Claim 8 (depends on 1)

The method of claim 1, wherein the first and second anions are each selected from the group consisting of bromide, iodide and chloride.

### Claim 9 (depends on 1)

The method of claim 1, wherein:
the first cation comprises formamidinium and the second cation comprises Cs;
the first metal comprises Pb; and
the first anion comprises bromide and the second anion comprises iodide.

### Claim 10 (depends on 1)

The method of claim 1, wherein the mixed-cation mixed-halide perovskite material comprises:
the first and the second cation, wherein each are selected from the group consisting of methylammonium, formamidinium, Cs, K and Rb;
the first metal selected from the group consisting of Pb and Sn; and
the first and the second anion, wherein each are selected from the group consisting of bromide, iodide, and chloride.

### Claim 11 (depends on 1)

The method of claim 1, wherein the mixed-cation mixed-halide perovskite material comprises formamidinium cesium lead iodide bromide.

### Claim 12 (depends on 1)

The method of claim 1, wherein the mixed-cation mixed-halide perovskite material comprises FA0.85Cs0.15Pb(I0.85Br0.15)3, where FA is formamidinium.

### Claim 13 (depends on 1)

The method of claim 1, wherein each of the first and second anions, the metal, and the first and second cations have concentration ratios in the ink that are less than 5% different from targeted concentration ratios in the perovskite film.

### Claim 14 (depends on 1)

The method of claim 1, wherein each of the first and second anions, the first metal, and the first and second cations have concentration ratios in the ink that are less than 5% different from concentration ratios in a stoichiometric perovskite film.

### Claim 15 (depends on 1)

The method of claim 1, wherein:
the complexing agent has greater than 0.05 molar solubility relative to the reactants;
the complexing agent has a complex binding strength to the first metal greater than that of dimethylformamide (DMF) and less than that of dimethylsulfoxide (DMSO); and
the complexing agent has a boiling point less than 200° C.

### Claim 16 (depends on 1)

The method of claim 1, wherein the solvent is selected from the group consisting of an anhydrous solvent, a polar solvent, dimethylformamide (DMF), dimethylacetamide (DMAC), and combinations thereof.

### Claim 17 (depends on 1)

The method of claim 1, wherein the depositing, drying or annealing steps, or the depositing, drying and annealing steps, are performed in dehumidified air with less than 5% RH.

### Claim 18 (depends on 1)

The method of claim 1, wherein the depositing, drying or annealing steps, or the depositing, drying and annealing steps are performed in an atmosphere comprising less than 1% oxygen.

### Claim 19 (depends on 1)

The method of claim 1, wherein the depositing step is performed using spin-coating, slot-die coating, blade coating, dip coating, spraying, screen printing, ink-jet printing, gravure printing, offset printing, or waterfall coating.

### Claim 20 (depends on 1)

The method of claim 1, wherein the drying step is performed in an environment of nitrogen forced convection, an environment of air forced convection, or a low-pressure environment with pressure from 0.01 Pa to 3000 Pa.

### Claim 21 (depends on 1)

The method of claim 1, wherein the drying step is performed in an environment with a controlled partial pressure of the solvent.

### Claim 22 (depends on 1)

The method of claim 1, wherein the annealing step is performed at a temperature from 70° C. to 350° C.

### Claim 23 (depends on 1)

The method of claim 1, wherein the perovskite film is formed without the use of any anti-solvents.

### Claim 24 (depends on 1)

The method of claim 1, wherein an equivalent ratio of the complexing agent relative to the first metal concentration in the ink is from 0.5 to 5.

### Claim 25 (depends on 1)

The method of claim 1, wherein the first metal molarity in the ink is from 0.25 to 1.5 moles of the first metal per liter of the ink.

### Claim 26 (depends on 1)

The method of claim 1, wherein the perovskite film comprises an undetectable amount of the complexing agent when measured by x-ray diffraction (XRD), x-ray photoelectron spectroscopy (XPS), or Fourier transform infrared spectroscopy (FTIR).

### Claim 27

A method, comprising:
providing an ink comprising reactants, a complexing agent, and a solvent, wherein:
the reactants comprise a first and a second cation, a first metal, and a first and a second anion, wherein the first and second cations are different from each other, and the first and second anions are different from each other;
depositing the ink onto a substrate to form a wet film;
drying the wet film to form a precursor layer; and
annealing the precursor layer to form a perovskite film, wherein:
the perovskite film comprises a mixed-cation mixed-halide perovskite material;
the perovskite film comprises less than 5% by mass of the complexing agent; and
the perovskite film is formed using a one-step process.

### Claim 28 (depends on 27)

The method of claim 27, wherein the complexing agent comprises:
a molar solubility greater than 0.05 to at least one of the reactants;
a complex binding strength to the first metal greater than that of dimethylformamide (DMF) and less than that of dimethylsulfoxide (DMSO); and
a boiling point less than 200° C.

### Claim 29

A method, comprising:
providing an ink comprising reactants, a complexing agent, and a solvent, wherein:
the reactants comprise a first and a second cation, a first metal, and a first and a second anion, wherein the first and second cations are different from each other, and the first and second anions are different from each other;
the complexing agent comprises:
a molar solubility greater than 0.05 to at least one of the reactants;
a complex binding strength to the first metal greater than that of dimethylformamide (DMF) and less than that of dimethylsulfoxide (DMSO); and
a boiling point less than 200° C.;
depositing the ink onto a substrate to form a wet film;
drying the wet film to form a precursor layer; and
annealing the precursor layer to form a perovskite film, wherein the perovskite film comprises:
a mixed-cation mixed-halide perovskite material; and
less than 5% by mass of the complexing agent.