# US 2020/0287087 A1 · Group iii nitride semiconductor light emitting element and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0287087 A1
- Document ID: US20200287087A1
- Status: Published application
- Kind: A1
- Application number: 16/497,564
- Filed: 2018-03-23
- Published: 2020-09-10
- Earliest claimed: 2017-03-27
- Assignees: Dowa Electronics Materials Co., Ltd.
- Applicants: DOWA Electronics Materials Co., Ltd.
- Inventors: Yasuhiro WATANABE
- Web page: https://patentgrep.com/patent/US20200287087A1

## CPC

- H10H 20/835: {Reflective materials}
- H10H 20/01335: {the light-emitting regions comprising nitride materials}
- H10H 20/812: within the light-emitting regions, e.g. having quantum confinement structures
- H10H 20/815: having stress relaxation structures, e.g. buffer layers
- H10H 20/816: having carrier transport control structures, e.g. highly-doped semiconductor layers or current-blocking structures
- H10H 20/8162: {Current-blocking structures}
- H10H 20/825: containing nitrogen, e.g. GaN
- H10H 20/8252: {characterised by the dopants}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2908: {Nitrides}
- H10P 14/2921: {being crystalline insulating materials}
- H10P 14/3216: {Nitrides}
- H10P 14/3251: {consisting of three or more layers}
- H10P 14/3416: {Nitrides}
- H10P 14/3442: {N-type}
- H10P 14/3444: {P-type}
- H10H 20/032: {of electrodes}
- H10H 20/8215: {characterised by crystalline imperfections, e.g. dislocations; characterised by the distribution of dopants, e.g. delta-doping}
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Provided are a group III nitride semiconductor light emitting element and a method of manufacturing the same. A group III nitride semiconductor light emitting element of the present disclosure comprises in this order, in a substrate, an n-type semiconductor layer, a light emitting layer, a p-type electron blocking layer, a p-type contact layer made of AlxGa1-xN, and a p-side reflection electrode, wherein a center emission wavelength of light emitted from the light emitting layer is 270 nm or greater and 330 nm or smaller, the p-type contact layer is in contact with the p-side reflection electrode, and has a thickness of 20 nm or greater and 80 nm or smaller, and the Al composition ratio x of the p-type contact layer satisfies the following Formula: 2.09−0.006×λp≤x≤2.25−0.006×λp where λp is the center emission wavelength in nanometer.

## Claims

### Claim 1

A group III nitride semiconductor light emitting element comprising, in this order:
a substrate;
an n-type semiconductor layer;
a light emitting layer;
a p-type electron blocking layer;
a p-type contact layer made of AlxGa1-xN; and
a p-side reflection electrode,
wherein a center emission wavelength of light emitted from the light emitting layer is 270 nm or greater and 330 nm or smaller,
the p-type contact layer is in contact with the p-side reflection electrode, and the p-type contact layer has a thickness of 20 nm or greater and 80 nm or smaller, and
an Al composition ratio x of the p-type contact layer satisfies the following Formula (1):
2.09−0.006×λp≤x≤2.25−0.006×λp Formula (1)
in Formula (1), λp is the center emission wavelength in nanometer.

### Claim 2 (depends on 1)

The group III nitride semiconductor light emitting element of claim 1,
wherein the center emission wavelength of light emitted from the light emitting layer is 270 nm or greater and 310 nm or smaller.

### Claim 3 (depends on 1)

The group III nitride semiconductor light emitting element of claim 1, wherein the p-type contact layer has a high concentration region having a Mg concentration of 3×1020 atoms/cm3 or greater on a side contacting the p-side reflection electrode.

### Claim 4 (depends on 1)

The group III nitride semiconductor light emitting element of claim 1, wherein the Al composition ratio x of the p-type contact layer satisfies the following Formula (2):
2.14−0.006×λp≤x≤2.24−0.006×λp Formula (2)
in Formula (2), λp is the center emission wavelength in nanometer.

### Claim 5

A method of manufacturing a group III nitride semiconductor light emitting element, comprising:
a step of forming an n-type semiconductor layer, a light emitting layer, and a p-type electron blocking layer on a substrate in this order;
a p-type contact layer formation step of forming a p-type contact layer made of AlxGa1-xN on the p-type electron blocking layer;
a step of forming a p-side reflection electrode directly on the p-type contact layer;
wherein the light emitting layer is formed such that a center emission wavelength therefrom is 270 nm or greater and 330 nm or smaller,
the p-type contact layer formation step comprises forming the p-type contact layer such that the p-type contact layer has a thickness of 20 nm or greater and 80 nm or smaller, and an Al composition ratio x of the p-type contact layer satisfies the following Formula (1):
2.09−0.006×λp≤x≤2.25−0.006×λp Formula (1)
in Formula (1), λp is the center emission wavelength in nanometer.

### Claim 6 (depends on 5)

The method of manufacturing a group III nitride semiconductor light emitting element of claim 5,
wherein the light emitting layer is formed such that a center emission wavelength therefrom is 270 nm or greater and 310 nm or smaller.

### Claim 7 (depends on 5)

The method of manufacturing a group III nitride semiconductor light emitting element of claim 5, wherein the p-type contact layer formation step comprises:
a first step of growing a crystal of a layer made of AlxGa1-xN by supplying a group III source gas, a group V source gas, and a Mg source gas; and
a second step of reducing a flow rate of the group III source gas to one fourth or less of the flow rate of the group III source gas in the first step immediately after an end of the first step, while continuing to supply the group V source gas and the Mg source gas continuously from the first step for 1 minute or longer and 20 minutes or shorter.