# US 2020/0286897 A1 · Gap fill methods for dram

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0286897 A1
- Document ID: US20200286897A1
- Status: Published application
- Kind: A1
- Application number: 16/804,226
- Filed: 2020-02-28
- Published: 2020-09-10
- Earliest claimed: 2019-03-04
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Priyadarshi Panda; Seshadri Ganguli; Sang Ho Yu; Sung-Kwan Kang; Gill Yong Lee; Sanjay Natarajan; Rajib Lochan Swain; Jorge Pablo Fernandez
- Web page: https://patentgrep.com/patent/US20200286897A1

## CPC

- H10B 12/053: {the transistor being at least partially in a trench in the substrate (vertical transistor in combination with a capacitor formed in a substrate trench H10B12/0383)}
- H10D 30/60: Insulated-gate field-effect transistors [IGFET] (H10D30/40 takes precedence)
- H10B 12/488: {Word lines}
- H10D 64/513: {within recesses in the substrate, e.g. trench gates, groove gates or buried gates}
- H10B 12/34: {the transistor being at least partially in a trench in the substrate}
- H10B: ELECTRONIC MEMORY DEVICES
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

Methods of forming memory devices are described. Some embodiments of the disclosure utilize a low temperature anneal process to reduce bottom voids and seams in low melting point, low resistance metal buried word lines. Some embodiments of the disclosure utilize a high density dielectric cap during a high temperature anneal process to reduce bottom voids in buried word lines.

## Claims

### Claim 1

A method of forming a memory device, the method comprising:
providing a substrate having plurality of trenches thereon, each trench having a trench depth;
depositing a conformal gate oxide layer on the substrate;
forming a thickness of a first metal layer on the conformal gate oxide layer, the thickness being less than or equal to about 90% of the trench depth;
performing a low temperature anneal of the substrate;
forming a thickness of a second metal layer on the first metal layer, the thickness of the second metal layer at least filling the trench; and
recessing the second metal layer to a predetermined depth to form a recessed metal layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein forming the first metal layer comprises depositing a conformal work-function metal layer on the conformal gate oxide layer and depositing a first metal layer on the conformal work-function metal layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first and second metal layers comprise Ru or Ir.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first metal layer fills less than or equal to about 50% of the trench depth.

### Claim 5 (depends on 1)

The method of claim 1, wherein the low temperature anneal is performed at a temperature of less than or equal to about 700° C. for a period of less than or equal to about 10 minutes.

### Claim 6 (depends on 1)

The method of claim 1, wherein after annealing the substrate, the first metal layer contains substantially no seams or voids.

### Claim 7 (depends on 1)

The method of claim 1, wherein the memory device contains substantially no bottom void.

### Claim 8

A method of forming a memory device, the method comprising:
providing a substrate having plurality of trenches thereon, each trench having a trench depth;
depositing a conformal gate oxide layer on the substrate;
forming a thickness of a metal layer on the conformal gate oxide layer, the thickness at least filling the trench;
performing a low temperature anneal of the substrate;
recessing the metal layer to a predetermined depth to form a recessed metal layer;
depositing a high density dielectric layer on the recessed metal layer;
performing a high temperature anneal of the substrate; and
removing the high density dielectric layer.

### Claim 9 (depends on 8)

The method of claim 8, wherein forming the metal layer comprises depositing a conformal work-function metal layer on the conformal gate oxide layer and depositing a metal layer on the conformal work-function metal layer.

### Claim 10 (depends on 8)

The method of claim 8, wherein the metal layer comprises Ru or Ir.

### Claim 11 (depends on 8)

The method of claim 8, wherein the low temperature anneal is performed at a temperature of less than or equal to about 600° C. for a period of less than or equal to about 10 minutes.

### Claim 12 (depends on 8)

The method of claim 8, wherein after the low temperature anneal, the metal layer contains substantially no seams or voids.

### Claim 13 (depends on 8)

The method of claim 8, wherein the predetermined depth is in a range of about 80 nm to about 90 nm.

### Claim 14 (depends on 8)

The method of claim 8, wherein the high temperature anneal is performed at a temperature of greater than or equal to about 800° C. for a period of less than or equal to about 1 minute.

### Claim 15 (depends on 8)

The method of claim 8, wherein the memory device contains substantially no bottom void.

### Claim 16

A method of forming a memory device, the method comprising:
providing a substrate having plurality of trenches thereon, each trench having a trench depth;
depositing a conformal gate oxide layer on the substrate;
forming a thickness of a metal layer on the conformal gate oxide layer, the thickness being less than or equal to 90% of the trench depth;
performing a low temperature anneal of the substrate;
forming an additional thickness of the metal layer, the total thickness of the metal layer at least filling the trench;
recessing the metal layer to a predetermined depth to form a recessed metal layer;
depositing a high density dielectric layer on the recessed metal layer;
performing a high temperature anneal of the substrate; and
removing the high density dielectric layer.

### Claim 17 (depends on 16)

The method of claim 16, wherein forming the metal layer comprises depositing a conformal work-function metal layer on the conformal gate oxide layer and depositing a metal layer on the conformal work-function metal layer.

### Claim 18 (depends on 16)

The method of claim 16, wherein the metal layer comprises Ru or Ir.

### Claim 19 (depends on 16)

The method of claim 16, wherein the low temperature anneal is performed at a temperature of less than or equal to about 600° C. for a period of less than or equal to about 10 minutes, and the high temperature anneal is performed at a temperature of greater than or equal to about 800° C. for a period of less than or equal to about 1 minute.

### Claim 20 (depends on 16)

The method of claim 16, wherein the memory device contains substantially no bottom void.