- Number: US 2020/0286726 A1
- Document ID: US20200286726A1
- Status: Published application
- Kind: A1
- Application number: 16/801,910
- Filed: 2020-02-26
- Published: 2020-09-10
- Earliest claimed: 2019-03-08
- Assignees: ASM IP Holding B.V.
- Applicants: ASM IP Holding B.V.
- Inventors: Eric James Shero; Paul Ma; Bed Prasad Sharma; Shankar Swaminathan
- Web page: https://patentgrep.com/patent/US20200286726A1

## CPC

- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- C23C 16/345: {Silicon nitride}
- C23C 16/45536: {Use of plasma, radiation or electromagnetic fields}
- C23C 16/45553: {characterized by the use of precursors specially adapted for ALD}
- H01J 37/32724: {Temperature}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/6506: {Formation of intermediate materials}
- H10P 14/6514: {by exposure to a plasma}
- H10P 14/6532: {by exposure to a plasma}
- H10P 72/7604: {the wafers being placed on a susceptor, stage or support}
- H10W 20/069: {by forming self-aligned vias or self-aligned contact plugs}
- H01J 37/32899: {Multiple chambers, e.g. cluster tools}
- H01J 2237/3321: CVD [Chemical Vapor Deposition]
- H10P 14/6681: {the precursor containing a compound comprising Si}
- H10P 72/0461: {characterised by the presence of two or more transfer chambers}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for selectively depositing silicon nitride on a first material relative to a second material is disclosed. An exemplary method includes treating the first material, and then selectively depositing a layer comprising silicon nitride on the second material relative to the first material. Exemplary methods can further include treating the deposited silicon nitride.

## Claims

### Claim 1

A method of forming a structure, the method comprising the steps of:
providing a substrate within a reaction chamber, the substrate comprising a surface comprising a first material and a second material, the first material comprising an oxide and the second material comprising a nitride;
treating the first material with a plasma treatment; and
selectively depositing a layer comprising silicon nitride on the second material relative to the first material.

### Claim 2 (depends on 1)

The method of claim 1, wherein the step of selectively depositing comprises atomic layer deposition.

### Claim 3 (depends on 1)

The method of claim 1, wherein a temperature of a susceptor within the reaction chamber during the step of selectively depositing is between about 100° C. and about 500° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein the step of treating comprises generating a plasma comprising noble gas species and hydrogen species.

### Claim 5 (depends on 4)

The method of claim 4, wherein the noble gas comprises argon.

### Claim 6 (depends on 4)

The method of claim 4, wherein a source gas for the hydrogen species comprises hydrogen.

### Claim 7 (depends on 1)

The method of claim 1, wherein a plasma for the plasma treatment is formed using a noble gas and a gas comprising hydrogen and wherein a ratio of the noble gas to gas comprising hydrogen ranges from about 0.1:1 to about 1:0.1.

### Claim 8 (depends on 1)

The method of claim 1, further comprising a step of densifying the layer comprising silicon nitride.

### Claim 9 (depends on 8)

The method of claim 8, wherein the step of densifying comprises exposing the layer comprising silicon nitride to a plasma comprising one or more noble gases.

### Claim 10 (depends on 9)

The method of claim 9, wherein the step of densifying comprises exposing the layer comprising silicon nitride to a plasma comprising helium.

### Claim 11 (depends on 10)

The method of claim 10, wherein a ratio of argon to helium is between about 0.1:0.9 and about 0.9:0.1.

### Claim 12 (depends on 1)

The method of claim 1, wherein the first material comprises an oxide selected from the group consisting of a Group IV oxide and a metal oxide.

### Claim 13 (depends on 1)

The method of claim 1, wherein the second material comprises a nitride selected from the group consisting of a Group IV nitride and a metal nitride.

### Claim 14 (depends on 1)

A structure formed according to the method of claim 1.

### Claim 15 (depends on 14)

The structure of claim 14 comprising a self-aligned contact nitride.

### Claim 16 (depends on 15)

The structure of claim 15 comprising the layer comprising silicon nitride overlying and in contact with the self-aligned contact nitride.

### Claim 17

A method of forming a structure, the method comprising the steps of:
providing a substrate within a reaction chamber, the substrate comprising a surface comprising a first material and a second material, the first material comprising an oxide and the second material comprising a nitride;
treating the first material with a plasma treatment formed using a noble gas and a gas comprising hydrogen;
selectively depositing a layer comprising silicon nitride on the second material relative to the first material; and
densifying the layer comprising silicon nitride.

### Claim 18 (depends on 17)

The method of claim 17, wherein the step of selectively depositing comprises atomic layer deposition.

### Claim 19 (depends on 17)

A structure formed according to the method of claim 17.

### Claim 20 (depends on 19)

The structure of claim 19 comprising a self-aligned contact nitride.