# US 2020/0286691 A1 · Aramid fiber electrode and preparation method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0286691 A1
- Document ID: US20200286691A1
- Status: Published application
- Kind: A1
- Application number: 16/759,330
- Filed: 2018-07-04
- Published: 2020-09-10
- Earliest claimed: 2018-07-04
- Assignees: Soochow University; Zhangjiagang Institute of Industrial Technologies Soochow University
- Applicants: Soochow University; Zhangjiagang Institute of Industrial Technologies Soochow University
- Inventors: Aijuan GU; Hao FANG; Guozheng LIANG; Li YUAN
- Web page: https://patentgrep.com/patent/US20200286691A1

## CPC

- H01G 11/36: Nanostructures, e.g. nanofibres, nanotubes or fullerenes
- D06M 11/74: with carbon or graphite; with carbides; with graphitic acids or their salts
- D06M 11/83: with metals; with metal-generating compounds, e.g. metal carbonyls; Reduction of metal compounds on textiles
- D06M 13/11: Compounds containing epoxy groups or precursors thereof
- D06M 13/513: with at least one carbon-silicon bond
- D06M 15/37: Macromolecular compounds obtained otherwise than by reactions only involving carbon-to-carbon unsaturated bonds
- D06M 15/61: Polyamines {polyimines}
- D06M 23/08: Processes in which the treating agent is applied in powder or granular form (adhesives for multi-layer textile fabrics D06M17/00)
- H01G 11/24: characterised by structural features of the materials making up or comprised in the electrodes, e.g. form, surface area or porosity; characterised by the structural features of powders or particles used therefor
- H01G 11/40: Fibres
- H01G 11/86: specially adapted for electrodes (carbonisation or activation of carbon for the manufacture of electrodes H01G11/34)
- D06M 2101/36: Aromatic polyamides
- H01G 11/68: characterised by their material
- H01G 11/70: characterised by their structure
- Y02E 60/13: Energy storage using capacitors
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- D06M: TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS, FABRICS, FEATHERS OR FIBROUS GOODS MADE FROM SUCH MATERIALS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The invention discloses an aramid fiber electrode and a preparation method thereof. Silver nanoparticles, carbon nanotubes and polypyrrole were sequentially coated on the surface of the aramid fiber by chemical bonding, to prepare an aramid fiber electrode, two aramid fiber electrodes were wound with an electrolyte to obtain an aramid fiber electrochemical capacitor. Compared with the polymer fiber electrochemical capacitor prepared in the prior art, the aramid fiber electrochemical capacitor provided by the present invention has both high specific capacitance, high energy density, high mechanical performance, high stability, good flexibility and wearability. And other characteristics; the preparation method is controllable and suitable for large-scale applications.

## Claims

### Claim 1

A method for preparing an aramid fiber electrode, comprising the following steps:
(1) The aramid fiber bundles are immersed in an aqueous solution containing dopamine hydrochloride and trimethylolaminomethane hydrochloride, and then obtain polydopamine-coated aramid fiber bundles;
(2) Polyvinylpyrrolidone was added into silver ammonia solution to obtain solution C;
polydopamine-coated aramid fiber bundles were added into solution C, followed by adding dropwise an aqueous glucose solution, and then aramid fiber bundles coated with silver nanoparticles were obtained;
(3) Aramid fiber bundles coated with silver nanoparticles are added into an aqueous solution containing γ-(2,3-glycidoxy) propyltrimethoxysilane to get aramid fiber bundles coated by silver nanoparticles with epoxy groups on the surface;
(4) Aramid fiber bundles coated by silver nanoparticles with epoxy groups on the surface are added into ethanol containing carbon nanotubes with carboxyl groups, and then aramid fiber bundles with double-layered coatings of carbon nanotubes and silver nanoparticles were obtained;
(5) Aramid fiber bundles with double-layered coatings of carbon nanotubes and silver nanoparticles were added into an aqueous solution containing pyrrole, and then silver nitrate aqueous solution was added dropwise, through reaction aramid fiber electrode was obtained.

### Claim 2

A method for preparing aramid fiber bundles with double-layered coatings of carbon nanotubes and silver nanoparticles, comprising the following steps:
(1) The aramid fiber bundles are immersed in an aqueous solution containing dopamine hydrochloride and trimethylolaminomethane hydrochloride, and then obtain polydopamine-coated aramid fiber bundles;
(2) Polyvinylpyrrolidone was added into silver ammonia solution to obtain solution C;
polydopamine-coated aramid fiber bundles were added into solution C, followed by adding dropwise an aqueous glucose solution, and then aramid fiber bundles coated with silver nanoparticles were obtained;
(3) Aramid fiber bundles coated with silver nanoparticles are added into an aqueous solution containing γ-(2,3-glycidoxy) propyltrimethoxysilane to get aramid fiber bundles coated by silver nanoparticles with epoxy groups on the surface;
(4) Aramid fiber bundles coated by silver nanoparticles with epoxy groups on the surface are added into ethanol containing carbon nanotubes with carboxyl groups, and then aramid fiber bundles with double-layered coatings of carbon nanotubes and silver nanoparticles were obtained.

### Claim 3 (depends on 1)

The method according to claim 1, wherein in step (1), the mass ratio of dopamine hydrochloride, trimethylolaminomethane hydrochloride and aramid fiber bundles is (0.1-1):(0.05-0.5):(0.1-1); in step (2), the mass ratio of silver nitrate, polyvinylpyrrolidone, glucose and polydopamine coated aramid fiber bundles is (0.5-5):(0.05-0.5):(1-10):(0.1-1); in step (3), the mass ratio of γ-(2,3-epoxypropoxy) propyl trimethoxy silicon alkane and aramid fiber bundles coated with silver nanoparticles is (0.5-5):(0.1-1); in step (4), the mass ratio of carbon nanotubes with carboxyl groups to aramid fiber bundles coated with silver nanoparticles containing epoxy groups is (0.5-5):(0.1-1).

### Claim 4 (depends on 1)

The method according to claim 1, wherein in step (1), pH value of the aqueous solution containing dopamine hydrochloride and trimethylolaminomethane hydrochloride was 8.5, the reaction is carried out with shaking at room temperature for 5 to 48 hours; in step (2), the reaction is a shaking reaction at room temperature for 10 to 60 min; in step (3), the reaction is a shaking reaction at 50 to 100° C. for 1 to 10 hours; in step (4), the reaction is a shaking reaction at 50 to 80° C. for 5 to 24 hours.

### Claim 5 (depends on 1)

The method according to claim 1, wherein in step (1), after the reaction is finished, the fibers are taken out, washed and dried to obtain polydopamine coated aramid fiber bundles; in step (2), after the reaction is finished, the fibers are taken out, washed and dried to obtain aramid fiber bundles coated with silver nanoparticles; in step (3), after the reaction is finished, the fibers are taken out, washed and dried to obtain aramid fiber bundles coated by silver nanoparticles with epoxy groups on the surface; in step (4), after the reaction is finished, the fibers are taken out, washed and dried to obtain aramid fiber bundles with double-layered coatings of carbon nanotubes and silver nanoparticles.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the aramid fiber includes polyparaphenylene terephthalamide fiber, isophthaloyl metaphenylene diamine fibers, polyparabenamide fibers, or a combination thereof, the carbon nanotubes include multi-walled carbon nanotubes, single-walled carbon nanotubes, and carbon nanotube bundles, or a combination thereof.

### Claim 7 (depends on 1)

The method according to claim 1, wherein in step (5), the mass ratio of silver nitrate, pyrrole, and aramid fiber bundles with double-layered coatings of carbon nanotubes and silver nanoparticles is (0.2-4):(0.1-2):(0.1-1); the reaction is carried out at room temperature for 5 to 48 hours with shaking; after the reaction is finished, the fibers are taken out, washed and dried to obtain aramid fiber electrode.

### Claim 8 (depends on 1)

The aramid fiber electrode prepared according to the preparation method of claim 1.

### Claim 9 (depends on 2)

The aramid fiber bundles with double-layered coatings of carbon nanotubes and silver nanoparticles prepared according to the preparation method of claim 2.

### Claim 10

(canceled)

### Claim 11 (depends on 2)

The method according to claim 2, wherein in step (1), the mass ratio of dopamine hydrochloride, trimethylolaminomethane hydrochloride and aramid fiber bundles is (0.1-1):(0.05-0.5):(0.1-1); in step (2), the mass ratio of silver nitrate, polyvinylpyrrolidone, glucose and polydopamine coated aramid fiber bundles is (0.5-5):(0.05-0.5):(1-10):(0.1-1); in step (3), the mass ratio of γ-(2,3-epoxypropoxy) propyl trimethoxy silicon alkane and aramid fiber bundles coated with silver nanoparticles is (0.5-5):(0.1-1); in step (4), the mass ratio of carbon nanotubes with carboxyl groups to aramid fiber bundles coated with silver nanoparticles containing epoxy groups is (0.5-5):(0.1-1).

### Claim 12 (depends on 2)

The method according to claim 2, wherein in step (1), pH value of the aqueous solution containing dopamine hydrochloride and trimethylolaminomethane hydrochloride was 8.5, the reaction is carried out with shaking at room temperature for 5 to 48 hours; in step (2), the reaction is a shaking reaction at room temperature for 10 to 60 min; in step (3), the reaction is a shaking reaction at 50 to 100° C. for 1 to 10 hours; in step (4), the reaction is a shaking reaction at 50 to 80° C. for 5 to 24 hours.

### Claim 13 (depends on 2)

The method according to claim 2, wherein in step (1), after the reaction is finished, the fibers are taken out, washed and dried to obtain polydopamine coated aramid fiber bundles; in step (2), after the reaction is finished, the fibers are taken out, washed and dried to obtain aramid fiber bundles coated with silver nanoparticles; in step (3), after the reaction is finished, the fibers are taken out, washed and dried to obtain aramid fiber bundles coated by silver nanoparticles with epoxy groups on the surface; in step (4), after the reaction is finished, the fibers are taken out, washed and dried to obtain aramid fiber bundles with double-layered coatings of carbon nanotubes and silver nanoparticles.

### Claim 14 (depends on 2)

The method according to claim 2, wherein the aramid fiber includes polyparaphenylene terephthalamide fiber, isophthaloyl metaphenylene diamine fibers, polyparabenamide fibers, or a combination thereof, the carbon nanotubes include multi-walled carbon nanotubes, single-walled carbon nanotubes, and carbon nanotube bundles, or a combination thereof.