# US 2020/0270480 A1 · One part thermal-curing acrylate adhesive precursor and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0270480 A1
- Document ID: US20200270480A1
- Status: Published application
- Kind: A1
- Application number: 16/629,697
- Filed: 2018-07-06
- Published: 2020-08-27
- Earliest claimed: 2017-07-13
- Assignees: 3M Innovative Properties Company
- Applicants: 3M Innovative Properties Company
- Inventors: Lingjie Tong
- Web page: https://patentgrep.com/patent/US20200270480A1

## CPC

- C09J 4/00: Adhesives based on organic non-macromolecular compounds having at least one polymerisable carbon-to-carbon unsaturated bond {; adhesives, based on monomers of macromolecular compounds of groups C09J183/00 - C09J183/16}
- C08F 220/1811: {C10or C11-(Meth)acrylate, e.g. isodecyl (meth)acrylate, isobornyl (meth)acrylate or 2-naphthyl (meth)acrylate}
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

The present invention provides a one-part thermal-curing acrylate adhesive precursor, calculated by 100 wt. % of said one-part thermal-curing acrylate adhesive precursor, comprising: 20 to 85 wt. % of polyurethane modified acrylate oligomer; 5 to 25 wt. % of methacrylic acid; 5 to 65 wt. % of acrylate monomer; 0.5 to 5 wt. % of adhesion promoter; and 1 to 12 wt. % of initiator. The present invention also provides a preparation method for said one-part thermal-curing acrylate adhesive precursor. According to the technical scheme of the present invention, a one-part acrylate adhesive precursor with excellent adhesive properties, which can be thermal-cured, is provided.

## Claims

### Claim 1

A one-part thermal-curing acrylate adhesive precursor, calculated by 100 wt. % of said one-part thermal-curing acrylate adhesive precursor, comprising:
20 to 85 wt. % of polyurethane modified acrylate oligomer;
5 to 25 wt. % of methacrylic acid;
5 to 65 wt. % of acrylate monomer;
0.5 to 5 wt. % of adhesion promoter; and
1 to 12 wt. % of initiator.

### Claim 2 (depends on 1)

The one-part thermal-curing acrylate adhesive precursor according to claim 1, wherein said one-part thermal-curing acrylate adhesive precursor does not contain a solvent.

### Claim 3 (depends on 1)

The one-part thermal-curing acrylate adhesive precursor according to claim 1, wherein the number-average molecular weight of said polyurethane modified acrylate oligomer is within the range of 2200 to 3800 grams/mole.

### Claim 4 (depends on 1)

The one-part thermal-curing acrylate adhesive precursor according to claim 1, wherein said polyurethane modified acrylate oligomer is an aliphatic polyurethane acrylate.

### Claim 5 (depends on 1)

The one-part thermal-curing acrylate adhesive precursor according to claim 1, wherein said acrylate monomer is one or more selected from the group consisting of tetrahydrofurfuryl methacrylate, isobornyl methacrylate and trimethylolpropane formal acrylate.

### Claim 6 (depends on 1)

The one-part thermal-curing acrylate adhesive precursor according to claim 1, wherein said adhesion promoter is one or more selected from the group consisting of acrylate phosphate and derivatives thereof, methacrylate phosphate and derivatives thereof, ethylene glycol methacrylate phosphate and alkyl acrylate phosphate.

### Claim 7 (depends on 1)

The one-part thermal-curing acrylate adhesive precursor according to claim 1, wherein said initiator is a thermal initiator.

### Claim 8 (depends on 7)

The one-part thermal-curing acrylate adhesive precursor according to claim 7, wherein said thermal initiator is one or more selected from the group consisting of benzoyl peroxide and isopropylbenzene hydroperoxide.

### Claim 9

A method for preparing a one-part thermal-curing acrylate adhesive precursor, comprising: mixing 20 to 85 wt. % of polyurethane modified acrylate oligomer, 5 to 25 wt. % of methacrylic acid, 5 to 65 wt. % of acrylate monomer, 0.5 to 5 wt. % of adhesion promoter and 1 to 12 wt. % of initiator, calculated by 100 wt. % of said one-part thermal-curing acrylate adhesive precursor.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the mixing is carried out at a temperature below 30° C.

### Claim 11 (depends on 9)

The method according to claim 9, wherein during the mixing process no solvent is added.

### Claim 12 (depends on 9)

The method according to claim 9, wherein the number-average molecular weight of said polyurethane modified acrylate oligomer is within the range of 2200 to 3800 grams/mole.

### Claim 13 (depends on 9)

The method according to claim 9, wherein said polyurethane modified acrylate oligomer is an aliphatic polyurethane acrylate.

### Claim 14 (depends on 9)

The method according to claim 9, wherein said acrylate monomer is one or more selected from the group consisting of tetrahydrofurfuryl methacrylate, isobornyl methacrylate and trimethylolpropane formal acrylate.

### Claim 15 (depends on 9)

The method according to claim 9, wherein said adhesion promoter is one or more selected from the group consisting of acrylate phosphate and derivatives thereof, methacrylate phosphate and derivatives thereof, ethylene glycol methacrylate phosphate and alkyl acrylate phosphate.

### Claim 16 (depends on 9)

The method according to claim 9, wherein said initiator is a thermal initiator.

### Claim 17 (depends on 9)

The method according to claim 9, wherein said thermal initiator is one or more selected from the group consisting of benzoyl peroxide and isopropylbenzene hydroperoxide.