# US 2020/0270422 A1 · Method for producing modified polyester resin reinforced with carbon fiber

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0270422 A1
- Document ID: US20200270422A1
- Status: Published application
- Kind: A1
- Application number: 15/931,662
- Filed: 2020-05-14
- Published: 2020-08-27
- Earliest claimed: 2015-01-25
- Assignees: Ftex Incorporated
- Applicants: Ftex, Incorporated
- Inventors: Takashi FUJIMAKI
- Web page: https://patentgrep.com/patent/US20200270422A1

## CPC

- C08K 7/06: Elements
- C08G 63/91: Polymers modified by chemical after-treatment
- C08J 5/042: {with carbon fibres}
- C08J 5/10: characterised by the additives used in the polymer mixture
- C08K 3/04: Carbon
- C08K 5/1515: Three-membered rings
- C08L 67/00: Compositions of polyesters obtained by reactions forming a carboxylic ester link in the main chain (of polyester-amides C08L77/12; of polyester-imides C08L79/08); Compositions of derivatives of such polymers
- C08L 69/00: Compositions of polycarbonates; Compositions of derivatives of polycarbonates
- C08J 2367/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds; (C08J2367/06 takes precedence)
- C08J 2463/00: Characterised by the use of epoxy resins; Derivatives of epoxy resins
- C08K 2201/003: Additives being defined by their diameter
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A method for producing a modified polyester resin reinforced with carbon fiber, comprising reacting a mixture containing (A) 100 parts by weight of a thermoplastic polyester, (B) 5 to 150 parts by weight of a carbon fiber, (C) 0.1 to 2 parts by weight of a coupling agent consisting of a polyfunctional epoxy compound having two or more epoxy groups in a molecule and having a weight-average molecular weight of 2,000 to 10,000, (D) 0.01 to 1 part by weight of a coupling reaction catalyst, and (E) a spreader of 0.01 to 1 part by weight at a temperature equal to or more than a melting point of the thermoplastic polyester to increase a melt viscosity.

## Claims

### Claim 1

A method for producing a molded product of a modified polyester resin reinforced with carbon fiber, comprising
reacting a mixture composed of (A) 100 parts by weight of a thermoplastic polyester, (B) 5 to 150 parts by weight of a carbon fiber, (C) 0.1 to 2 parts by weight of a coupling agent consisting of a polyfunctional epoxy compound having two or more epoxy groups in a molecule and having a weight-average molecular weight of 2,000 to 10,000, (D) 0.01 to 1 part by weight of a coupling reaction catalyst and (E) 0.01 to 1 part by weight of a spreader at a temperature equal to or more than a melting point of the thermoplastic polyester by a reactive extrusion method to prepare a modified polyester resin reinforced with carbon fiber having an MFR in accordance with JIS K6760 (at 260° C. and under a load of 2.16 kg) of 20 g/10 minutes or less; and
subsequently molding the modified polyester resin reinforced with carbon fiber into a sheet, a board, or a profile extruded product.

### Claim 2

A method for producing a foamed product of a modified polyester resin reinforced with carbon fiber, comprising:
reacting a mixture composed of (A) 100 parts by weight of a thermoplastic polyester, (B) 5 to 150 parts by weight of a carbon fiber, (C) 0.1 to 2 parts by weight of a coupling agent consisting of a polyfunctional epoxy compound having two or more epoxy groups in a molecule and having a weight-average molecular weight of 2,000 to 10,000, (D) 0.01 to 1 part by weight of a coupling reaction catalyst and (E) 0.01 to 1 part by weight of a spreader at a temperature equal to or more than a melting point of the thermoplastic polyester by a reactive extrusion method to prepare a modified polyester resin reinforced with carbon fiber having an MFR in accordance with JIS K6760 (at 260° C. and under a load of 2.16 kg) of 20 g/10 minutes or less; and
subsequently foam-molding the modified polyester resin reinforced with carbon fiber by using a foaming gas of one or more kinds selected from the group consisting of a chemical forming gas, a volatile gas, and an inert gas.