# US 2020/0270181 A1 · Multi-component mortar system in a mixing bag

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0270181 A1
- Document ID: US20200270181A1
- Status: Published application
- Kind: A1
- Application number: 16/493,086
- Filed: 2018-04-12
- Published: 2020-08-27
- Earliest claimed: 2017-04-12
- Assignees: Sika Technology AG
- Applicants: Sika Technology AG
- Inventors: Mohamed CADER; Camille LANNEVERE; Maxime LIARD; Didier LOOTENS
- Web page: https://patentgrep.com/patent/US20200270181A1

## CPC

- C04B 40/065: {Two or more component mortars}
- C04B 28/04: Portland cements
- C04B 28/06: Aluminous cements (monolithic refractories or refractory mortars C04B35/66)
- C04B 28/16: containing anhydrite {, e.g. Keene's cement}
- C04B 2111/72: Repairing or restoring existing buildings or building materials
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A ready-to-use multi-component mortar system in a mixing bag including a component A which is solid and comprises cement and/or aluminium silicate, and a component B which is an aqueous solution, emulsion or suspension, wherein the mixing bag is a flexible bag including at least two separate sealed chambers which are isolated from each other by a removable or frangible seal and the components A and B of the multi-component mortar system are separately situated in the separate sealed chambers of the mixing bag without any contact to each other.

## Claims

### Claim 1

A ready-to-use multi-component mortar system in a mixing bag comprising
a component A which is solid and comprises cement and/or aluminium silicate, and
a component B which is an aqueous solution, emulsion or suspension,
wherein the mixing bag is a flexible bag comprising at least two separate sealed chambers which are isolated from each other by a removable or frangible seal and the components A and B of the multi-component mortar system are separately situated in the separate sealed chambers of the mixing bag without contact to each other.

### Claim 2 (depends on 1)

The mortar system according to claim 1, wherein component A comprises sand and at least part of the sand has a particle size of at least 100 μm.

### Claim 3 (depends on 1)

The mortar system according to claim 1, wherein component A and/or component B comprise calcium aluminate cement.

### Claim 4 (depends on 1)

The mortar system according to claim 1, wherein component A comprises at least one accelerator.

### Claim 5 (depends on 4)

The mortar system according to claim 4, wherein the accelerator is selected from the group consisting of alkali hydroxide, earth alkali hydroxide, alkali oxide, earth alkali oxide, lithium carbonate, lithium sulfate and organic amine.

### Claim 6 (depends on 1)

The mortar system according to claim 1, wherein the surface tension of component B is from 30 to 45 mN/m, measured at 23° C. with the Wilhelmy plate method and/or the viscosity of component B is in the range of 15 to 2,000 Pas, at a shear rate of 1 s−1, measured at 23° C. with the plate-plate rheometer Physica MCR 301, Anton Paar, Austria and the Software Rheoplus, with a plate diameter of 25 mm and 2 mm gap.

### Claim 7 (depends on 1)

The mortar system according to claim 1, wherein component B is selected from the group consisting of
component B1, which is an aqueous suspension comprising a water-insoluble organic polymer,
component B2, which is an aqueous suspension comprising a set-inhibited calcium aluminate cement,
component B3, which is an aqueous emulsion comprising an epoxy resin, and
component B4, which is an aqueous solution, emulsion or suspension comprising an alkali silicate.

### Claim 8 (depends on 7)

The mortar system according to claim 7, wherein component B is a component B1 wherein the water-insoluble organic polymer is selected from the group consisting of homo- or copolymers of acrylic esters, copolymers of styrene and butadiene, copolymers of styrene with acrylic esters, and homo- or copolymers of vinyl acetate.

### Claim 9 (depends on 7)

The mortar system according to claim 7, wherein component B is a component B2 containing from 20 to 60 weight-% calcium aluminate cement and a phosphate-based set-inhibitor.

### Claim 10 (depends on 7)

The mortar system according to claim 7, wherein component B is a component B3 wherein the epoxy resin is a liquid resin based on bisphenol-A- or bisphenol-F- or bisphenol-A/F-diglycidyl ether.

### Claim 11 (depends on 1)

The mortar system according to any claim 1, wherein the at least two separate sealed chambers of the mixing bag are isolated from each other by a frangible seal, which breaks when the chamber containing component B is pressed together carefully by hand without causing any rupture of the outer walls of the mixing bag.

### Claim 12 (depends on 1)

A method of producing a mortar comprising the steps of
providing a mortar system according to claim 1,
removing or breaking the seal between the at least two separate sealed chambers containing component A and component B,
combining component B with component A through the leak between the two chambers,
mixing component A and component B by shaking, kneading and/or squeezing the mixing bag thoroughly.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the bag is opened after combining and mixing of the components, the mixed mortar is pressed out of the bag and applied.

### Claim 14 (depends on 1)

A method of repairing or refurbishing a product, comprising applying the mortar system according to claim 1 to the product.

### Claim 15 (depends on 13)

The mortar applied according to the method of claim 13 with a compressive strength of more than 1 MPa after 4 hours measured according to EN 196-1.