# US 2020/0268608 A1 · Glass articles with low-friction coatings

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0268608 A1
- Document ID: US20200268608A1
- Status: Published application
- Kind: A1
- Application number: 16/870,657
- Filed: 2020-05-08
- Published: 2020-08-27
- Earliest claimed: 2012-02-28
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Andrei Gennadyevich Fadeev; Theresa Chang; Dana Craig Bookbinder; Santona Pal; Chandan Kumar Saha; Steven Edward DeMartino; Christopher Lee Timmons; John Stephen Peanasky
- Web page: https://patentgrep.com/patent/US20200268608A1

## CPC

- A61J 1/1468: {Containers characterised by specific material properties}
- B65D 23/0821: {consisting mainly of polymeric materials (B65D23/0828 takes precedence)}
- C03C 17/005: {Coating the outside}
- C03C 17/30: with silicon-containing compounds
- C03C 17/32: with synthetic or natural resins (C03C17/30 takes precedence)
- C03C 17/42: at least one coating of an organic material and at least one non-metal coating
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 2217/78: Coatings specially designed to be durable, e.g. scratch-resistant
- C03C 2218/111: by dipping, immersion
- Y10T 428/1321: Polymer or resin containing [i.e., natural or synthetic]
- Y10T 428/24926: including ceramic, glass, porcelain or quartz layer
- Y10T 428/24942: including components having same physical characteristic in differing degree
- Y10T 428/265: 1 mil or less
- Y10T 428/31612: As silicone, silane or siloxane
- Y10T 428/31623: Next to polyamide or polyimide
- A61J: CONTAINERS SPECIALLY ADAPTED FOR MEDICAL OR PHARMACEUTICAL PURPOSES; DEVICES OR METHODS SPECIALLY ADAPTED FOR BRINGING PHARMACEUTICAL PRODUCTS INTO PARTICULAR PHYSICAL OR ADMINISTERING FORMS; DEVICES FOR ADMINISTERING FOOD OR MEDICINES ORALLY; BABY COMFORTERS; DEVICES FOR RECEIVING SPITTLE
- B65D: CONTAINERS FOR STORAGE OR TRANSPORT OF ARTICLES OR MATERIALS, e.g. BAGS, BARRELS, BOTTLES, BOXES, CANS, CARTONS, CRATES, DRUMS, JARS, TANKS, HOPPERS, FORWARDING CONTAINERS; ACCESSORIES, CLOSURES, OR FITTINGS THEREFOR; PACKAGING ELEMENTS; PACKAGES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

According to embodiments, a method of making a coated pharmaceutical container, may include: forming a glass tube; forming the glass tube into a pharmaceutical container comprising an interior surface and an exterior surface; and applying a coating to the exterior surface. The coating may have a coefficient of friction less than or equal to 0.7 relative to a second pharmaceutical container when tested in a vial-on-vial testing jig under a normal load of 30 N. The coated pharmaceutical container may be thermally stable after depyrogenation at a temperature of at least 260° C. for 30 minutes in air.

## Claims

### Claim 1

A method of making a coated pharmaceutical container, the method comprising the steps of:
forming a glass tube;
forming the glass tube into a pharmaceutical container comprising an interior surface and an exterior surface; and
applying a coating to the exterior surface;
wherein:
the coating has a coefficient of friction less than or equal to 0.7, wherein the coefficient of friction is a maximum coefficient of friction measured relative to a second pharmaceutical container in a vial-on-vial testing jig under a normal load of 30 N, the second pharmaceutical container formed from the same glass composition and comprising the same coating and subjected to the same environmental conditions prior to measurement as the pharmaceutical container; and
the coated pharmaceutical container is thermally stable after depyrogenation at a temperature of at least 260° C. for 30 minutes in air.

### Claim 2 (depends on 1)

The method of claim 1, wherein the coating has a thickness of less than or equal to 1 micron.

### Claim 3 (depends on 1)

The method of claim 1, wherein the coating has a thickness of less than or equal to 100 nm.

### Claim 4 (depends on 1)

The method of claim 1, wherein the applying the coating comprises a dipping process, a spraying process, or both.

### Claim 5 (depends on 1)

The method of claim 1, wherein the coating comprises a polymer.

### Claim 6 (depends on 5)

The method of claim 5, wherein the polymer comprises one or more of polyimides, fluoropolymers, silsesquioxane-based polymers, and silicone resins.

### Claim 7 (depends on 1)

The method of claim 1, wherein the applying the coating comprises:
applying a coupling agent layer in direct contact with the exterior surface; and
applying a polymer layer in direct contact with the coupling agent layer.

### Claim 8 (depends on 1)

The method of claim 1, further comprising a step of subjecting the pharmaceutical container to a depyrogenation cycle whereby the coefficient of friction does not increase by more than 30% after the depyrogenation cycle.

### Claim 9 (depends on 8)

The method of claim 8, wherein the depyrogenation cycle comprises heating the coated pharmaceutical container to a temperature of at least 250° C. for at least 30 minutes.

### Claim 10 (depends on 8)

The method of claim 8, wherein the depyrogenation cycle comprises heating the coated pharmaceutical container to a temperature of at least 250° C. for up to 72 hours.

### Claim 11 (depends on 8)

The method of claim 8, wherein the depyrogenation cycle comprises heating the coated pharmaceutical container to a temperature of from about 250° C. to about 400° C. for a time period of from about 30 minutes to about 72 hours.

### Claim 12 (depends on 1)

The method of claim 1, the glass of the pharmaceutical container is borosilicate glass.

### Claim 13 (depends on 1)

The method of claim 1, the glass of the pharmaceutical container is alkali aluminosilicate glass.

### Claim 14 (depends on 1)

The method of claim 1, wherein the coating has a coefficient of friction that is at least 20% less than an uncoated glass pharmaceutical container, wherein the coefficient of friction of the uncoated glass pharmaceutical container is a maximum coefficient of friction measured relative to a second uncoated pharmaceutical container in a vial-on-vial testing jig under a normal load of 30 N, the second uncoated pharmaceutical container formed from the same glass composition and subjected to the same environmental conditions prior to measurement as the second uncoated pharmaceutical container.

### Claim 15

A method of making a coated pharmaceutical container, the method comprising the steps of:
applying a coating to an exterior surface of a pharmaceutical container, wherein the coating comprises a polymer; and
curing the coating by heating;
wherein:
the coating has a coefficient of friction less than or equal to 0.7, wherein the coefficient of friction is a maximum coefficient of friction measured relative to a second pharmaceutical container in a vial-on-vial testing jig under a normal load of 30 N, the second pharmaceutical container formed from the same glass composition and comprising the same coating and subjected to the same environmental conditions prior to measurement as the coated pharmaceutical container; and
the pharmaceutical container is thermally stable after depyrogenation at a temperature of at least 260° C. for 30 minutes in air.

### Claim 16 (depends on 15)

The method of claim 15, wherein the coating has a thickness of less than or equal to 1 micron.

### Claim 17 (depends on 15)

The method of claim 15, wherein the coating has a thickness of less than or equal to 100 nm.

### Claim 18 (depends on 15)

The method of claim 15, wherein the applying the coating comprises a dipping process, a spraying process, or both.

### Claim 19 (depends on 15)

The method of claim 15, wherein the polymer comprises one or more of polyimides, fluoropolymers, silsesquioxane-based polymers, and silicone resins.

### Claim 20 (depends on 15)

The method of claim 15, wherein the applying the coating comprises:
applying a coupling agent layer in direct contact with an exterior surface of the pharmaceutical container; and
applying a polymer layer in direct contact with the coupling agent layer.

### Claim 21 (depends on 15)

The method of claim 15, the glass of the pharmaceutical container is borosilicate glass.

### Claim 22 (depends on 15)

The method of claim 15, the glass of the pharmaceutical container is alkali aluminosilicate glass.

### Claim 23 (depends on 15)

The method of claim 15, wherein the coating has a coefficient of friction that is at least 20% less than an uncoated glass pharmaceutical container, wherein the coefficient of friction of the uncoated glass pharmaceutical container is a maximum coefficient of friction measured relative to a second uncoated pharmaceutical container in a vial-on-vial testing jig under a normal load of 30 N, the second uncoated pharmaceutical container formed from the same glass composition and subjected to the same environmental conditions prior to measurement as the second uncoated pharmaceutical container.

### Claim 24

A method of making a coated pharmaceutical container, the method comprising the steps of:
forming a glass tube;
forming the glass tube into a pharmaceutical container comprising an interior surface and an exterior surface;
applying a coating to the exterior surface; and
subjecting the pharmaceutical container to a lyophilization cycle, wherein:
the coating has a coefficient of friction that does not increase by more than 30% after the lyophilization cycle, wherein the coefficient of friction is a maximum coefficient of friction measured relative to a second pharmaceutical container in a vial-on-vial testing jig under a normal load of 30 N, the second pharmaceutical container formed from the same glass composition and comprising the same coating and subjected to the same environmental conditions prior to measurement as the pharmaceutical container; and
the coated pharmaceutical container is thermally stable after depyrogenation at a temperature of at least 260° C. for 30 minutes in air.

### Claim 25 (depends on 24)

The method of claim 24, wherein the lyophilization cycle comprises filling the pharmaceutical container with a liquid that contains protein and then freezing at a temperature of −100° C., followed by water sublimation for 20 hours at −15° C. under vacuum.

### Claim 26 (depends on 24)

The method of claim 24, wherein the coating has a thickness of less than or equal to 1 micron.

### Claim 27 (depends on 24)

The method of claim 24, wherein the coating has a thickness of less than or equal to 100 nm.

### Claim 28 (depends on 24)

The method of claim 24, wherein the applying the coating comprises a dipping process, a spraying process, or both.

### Claim 29 (depends on 24)

The method of claim 24, wherein the applying the coating comprises:
applying a coupling agent layer in direct contact with the exterior surface; and
applying a polymer layer in direct contact with the coupling agent layer.

### Claim 30 (depends on 24)

The method of claim 24, further comprising subjecting the pharmaceutical container to a depyrogenation cycle whereby the coefficient of friction does not increase by more than 30% after the depyrogenation cycle.