# US 2020/0266444 A1 · Negative electrode active material for lithium secondary battery, method for manufacturing the same, and lithium secondary battery comprising the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0266444 A1
- Document ID: US20200266444A1
- Status: Published application
- Kind: A1
- Application number: 16/793,799
- Filed: 2020-02-18
- Published: 2020-08-20
- Earliest claimed: 2019-02-18
- Assignees: SK Innovation Co., Ltd.; Unist (Ulsan National Institute of Science and Technology)
- Applicants: SK Innovation Co., Ltd.; Unist (Ulsan National Institute of Science and Technology)
- Inventors: Joon Sup KIM; Jee Hee LEE; Nam Hyeong KIM; Jae Kyung SUNG; Tae Yong LEE; Jae Phil CHO
- Web page: https://patentgrep.com/patent/US20200266444A1

## CPC

- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/364: {as mixtures}
- H01M 4/366: {as layered products}
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/58: of inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy; of polyanionic structures, e.g. phosphates, silicates or borates
- H01M 4/625: {Carbon or graphite}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Provided is a negative electrode active material for a lithium secondary battery according to the present invention, including a carbon-based particle including pores in an inner portion and/or a surface thereof; and a silicon-based coating layer positioned on a pore surface and/or a pore-free surface of the carbon-based particle and containing silicon carbon compound.

## Claims

### Claim 1

A negative electrode active material for a lithium secondary battery, the negative electrode active material comprising:
a carbon-based particle including pores in an inner portion and/or a surface thereof; and
a silicon-based coating layer positioned on a pore surface and/or a pore-free surface of the carbon-based particle and containing silicon carbon compound.

### Claim 2 (depends on 1)

The negative electrode active material of claim 1, wherein the silicon carbon compound satisfies SiCx (0<x≤2).

### Claim 3 (depends on 1)

The negative electrode active material of claim 1, further comprising a carbon coating layer positioned on the silicon-based coating layer.

### Claim 4 (depends on 1)

The negative electrode active material of claim 1, wherein the silicon-based coating layer includes a silicon carbon compound matrix and Si nano-particles dispersed in the matrix.

### Claim 5 (depends on 1)

The negative electrode active material of claim 1, wherein the silicon-based coating layer further includes Si nano-particles having an average particle diameter of 3 nm or more and 10 nm or less.

### Claim 6 (depends on 1)

The negative electrode active material of claim 1, wherein a degree of crystallinity of the silicon component contained in the silicon-based coating layer is 5% or more and 40% or less, based on the degree of crystallinity obtained by dividing a peak area of crystalline silicon by the sum of a peak area of amorphous silicon and a peak area of crystalline silicon in the Raman spectrum.

### Claim 7 (depends on 1)

The negative electrode active material of claim 1, wherein a weight ratio of carbon:silicon contained the silicon-based coating layer is 1:5 to 15.

### Claim 8 (depends on 1)

The negative electrode active material of claim 1, wherein when the negative electrode active material is left in air at 25° C. and 1 atm for 24 hours, a thickness of the oxide film (SiOx, 0<x≤2) formed on the surface of the silicon-based coating layer is 1% or more and 40% or less of the total thickness of the silicon-based coating layer including the oxide film after exposure to air.

### Claim 9 (depends on 1)

The negative electrode active material of claim 1, wherein the carbon-based particle includes pores in the inner portion and the surface thereof.

### Claim 10 (depends on 1)

The negative electrode active material of claim 1, wherein the pores of the carbon-based particle have an average particle diameter of 30 nm or more and 900 nm or less.

### Claim 11 (depends on 10)

The negative electrode active material of claim 10, wherein the number of pores most adjacent to one pore positioned in the inner portion of the carbon-based particle is 5 to 6 based on a cross section of the carbon-based particle.

### Claim 12 (depends on 1)

The negative electrode active material of claim 1, wherein the carbon-based particle has a BET specific surface area of 50 m2/g or more and 100 m2/g or less.

### Claim 13 (depends on 1)

The negative electrode active material of claim 1, wherein the silicon-based coating layer has a thickness of 5 nm or more and 100 nm or less.

### Claim 14 (depends on 1)

The negative electrode active material of claim 1, wherein the silicon-based coating layer is formed by a chemical vapor deposition (CVD) method.

### Claim 15

A method of preparing a negative electrode active material for a lithium secondary battery, the method comprising:
(a) a step of mixing, stirring, and then firing a first carbon precursor and a ceramic particle for forming pores with each other;
(b) a step of preparing a carbon-based particle including pores in an inner portion and/or a surface thereof by mixing an etching solution of the ceramic particle for forming pores and pulverizing; and
(c) a step of forming a silicon-based coating layer containing silicon carbon compound on a pore surface and/or a pore-free surface of the carbon-based particle by chemical vapor deposition (CVD).

### Claim 16 (depends on 15)

The method of claim 15, wherein the silicon carbon compound satisfies SiCx (0<x≤2).

### Claim 17 (depends on 15)

The method of claim 15, further comprising, after the step (c), (d) a step of mixing, stirring, and then firing a second carbon precursor with the carbon-based particle.

### Claim 18 (depends on 15)

The method of claim 15, wherein in the step (c), the silicon-based coating layer is formed by chemical vapor deposition (CVD) while simultaneously injecting a silicon precursor and a carbon precursor under an inert atmosphere.

### Claim 19 (depends on 15)

The method of claim 15, wherein the ceramic particle for forming pores has an average particle diameter of 30 nm or more and 900 nm or less.

### Claim 20 (depends on 15)

The method of claim 15, wherein in the step (c), the silicon-based coating layer is deposited at a thickness of 5 nm or more and 100 nm or less.

### Claim 21 (depends on 17)

The method of claim 17, wherein a firing temperature in the step (a) and/or the step (d) is 600° C. or more and 1500° C. or less.

### Claim 22 (depends on 17)

The method of claim 17, wherein at the time of stirring in the step (a) and/or the step (d), a solvent is sprayed.

### Claim 23 (depends on 1)

A lithium secondary battery comprising the negative electrode active material of claim 1.