# US 2020/0266441 A1 · Positive electrode active material for nonaqueous secondary battery, and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0266441 A1
- Document ID: US20200266441A1
- Status: Published application
- Kind: A1
- Application number: 16/795,539
- Filed: 2020-02-19
- Published: 2020-08-20
- Earliest claimed: 2019-02-20
- Assignees: Nichia Corporation
- Applicants: Nichia Corporation
- Inventors: Kumi YOSHIHARA; Kosuke SHIMOKITA; Kiyoto IKEBATA; Takashi SUGIMOTO
- Web page: https://patentgrep.com/patent/US20200266441A1

## CPC

- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- C01G 53/504: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.5, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.5
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/364: {as mixtures}
- H01M 4/366: {as layered products}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/52: containing elements as dopants
- C01P 2002/54: one element only
- C01P 2004/03: obtained by SEM
- C01P 2004/45: Aggregated particles or particles with an intergrown morphology
- C01P 2004/51: Particles with a specific particle size distribution
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2004/62: Submicrometer sized, i.e. from 0.1-1 micrometer
- C01P 2006/40: Electric properties
- H01M 4/0497: {Chemical precipitation}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Provided is a positive-electrode active material for a nonaqueous electrolyte secondary battery, including a lithium transition metal composite oxide particle having a layered structure and containing nickel, and an oxide containing lithium and aluminum and an oxide containing lithium and boron adhering to a surface of the lithium transition metal composite oxide particle. The lithium transition metal composite oxide particle includes a secondary particle formed by aggregation of primary particles containing a solid solution of aluminum in a surface layer. The lithium transition metal composite oxide particles have a composition with a difference of more than 0.22 mol % and less than 0.6 mol % between a ratio of the number of moles of aluminum in the solid solution in the surface layer of the primary particles relative to a total number of moles of metal other than lithium and a ratio of the number of moles of aluminum present in a region other than the surface layer of the primary particles relative to the total number of moles of metal other than lithium.

## Claims

### Claim 1

A positive-electrode active material for a nonaqueous electrolyte secondary battery comprising:
a lithium transition metal composite oxide particle having a layered structure and containing nickel; and an oxide containing lithium and aluminum and an oxide containing lithium and boron adhering to a surface of the lithium transition metal composite oxide particle, wherein
the lithium transition metal composite oxide particle comprises a secondary particle formed by aggregation of primary particles containing a solid solution of aluminum in a surface layer, and wherein
the positive-electrode active material has a composition with a difference of more than 0.22 mol % and less than 0.6 mol % between a ratio of a number of moles of aluminum in the solid solution in the surface layer of the primary particles relative to a total number of moles of metal other than lithium in the lithium transition metal composite oxide particle and a ratio of a number of moles of aluminum present in a region other than the surface layer of the primary particles relative to the total number of moles of metal other than lithium in the lithium transition metal composite oxide particle.

### Claim 2 (depends on 1)

The positive-electrode active material for a nonaqueous electrolyte secondary battery according to claim 1, wherein
a content of the oxide containing lithium and aluminum relative to the lithium transition metal composite oxide particle is 0.1 mol % to 0.8 mol % in terms of aluminum, and wherein
a content of the oxide containing lithium and boron relative to the lithium transition metal composite oxide particle is 0.3 mol % to 2.0 mol % in terms of boron.

### Claim 3 (depends on 1)

The positive-electrode active material for a nonaqueous electrolyte secondary battery according to claim 1, wherein
the lithium transition metal composite oxide particle has a composition in which a ratio of a number of moles of nickel to the total number of moles of metal other than lithium is 0.33 or more and 0.95 or less.

### Claim 4 (depends on 1)

The positive-electrode active material for a nonaqueous electrolyte secondary battery according to claim 1, wherein
the lithium transition metal composite oxide particle has a composition comprising cobalt, and wherein a ratio of a number of moles of cobalt to the total number of moles of metal other than lithium in the composition is 0.02 or more and 0.33 or less.

### Claim 5 (depends on 1)

The positive-electrode active material for a nonaqueous electrolyte secondary battery according to claim 1, wherein
the lithium transition metal composite oxide particle has a composition comprising manganese, and wherein a ratio of a number of moles of manganese to the total number of moles of metal other than lithium in the composition is 0.01 or more and 0.33 or less.

### Claim 6 (depends on 1)

The positive-electrode active material for a nonaqueous electrolyte secondary battery according to claim 1, wherein
the lithium transition metal composite oxide has a composition represented by the following formula:
LiaNibCocMndAleM1tO2
wherein 1.0≤a≤1.5, 0.33≤b≤0.95, 0.02≤c≤0.33, 0.01≤d≤0.33, 0.0022≤e≤0.05, 0≤f≤0.02, and b+c+d=1, and M1 is at least one selected from the group consisting of Zr, Ti, Mg, Ta, Nb, and Mo.

### Claim 7 (depends on 1)

The positive-electrode active material for a nonaqueous electrolyte secondary battery according to claim 1, wherein
the oxide containing lithium and aluminum has a volume-based particle diameter distribution in which a total volume percentage of particles having a particle diameter of 0.4 μm to 3.0 μm is greater than 50%.

### Claim 8 (depends on 2)

The positive-electrode active material for a nonaqueous electrolyte secondary battery according to claim 2, wherein
the lithium transition metal composite oxide has a composition represented by the following formula:
LiaNibCocMndAleM1fO2
wherein 1.0≤a≤1.5, 0.33≤b≤0.95, 0.02≤c≤0.33, 0.01≤d≤0.33, 0.0022≤e≤0.05, 0≤f≤0.02, and b+c+d=1, and M1 is at least one selected from the group consisting of Zr, Ti, Mg, Ta, Nb, and Mo.

### Claim 9 (depends on 1)

The positive-electrode active material for a nonaqueous electrolyte secondary battery according to claim 1, wherein a volume average particle diameter of the lithium transition metal composite oxide particle is 2 μm to 25 μm.

### Claim 10 (depends on 2)

The positive-electrode active material for a nonaqueous electrolyte secondary battery according to claim 2, wherein the content of the oxide containing lithium and aluminum relative to the lithium transition metal composite oxide particle is 0.13 mol % to 0.5 mol % in terms of aluminum.

### Claim 11 (depends on 2)

The positive-electrode active material for a nonaqueous electrolyte secondary battery according to claim 2, wherein a volume average particle diameter of the lithium transition metal composite oxide particle is 2 μm to 25 μm.

### Claim 12 (depends on 11)

The positive-electrode active material for a nonaqueous electrolyte secondary battery according to claim 11, wherein the content of the oxide containing lithium and aluminum relative to the lithium transition metal composite oxide particle is 0.13 mol % to 0.5 mol % in terms of aluminum.

### Claim 13

A method for manufacturing a positive-electrode active material for a nonaqueous electrolyte secondary battery comprising:
providing a mixture containing a lithium transition metal composite oxide particle having a layered structure and containing nickel, a lithium compound, an aluminum compound, and a boron compound; and
heat-treating the provided mixture, wherein
the lithium transition metal composite oxide particle comprises a secondary particle formed by aggregation of primary particles, and wherein
the aluminum compound has a volume-based particle diameter distribution in which a total volume percentage of particles having a particle diameter of 0.4 μm to 3.0 μm is greater than 54%.

### Claim 14 (depends on 13)

The method according to claim 13, wherein a temperature of the heat treatment is 500° C. to 800° C.

### Claim 15 (depends on 13)

The method according to claim 13, wherein
the lithium transition metal composite oxide particle has a composition in which a ratio of a number of moles of nickel to a total number of moles of metal other than lithium is 0.33 or more and 0.95 or less.

### Claim 16 (depends on 13)

The method according to claim 13, wherein
the lithium transition metal composite oxide particle has a composition comprising cobalt, and wherein a ratio of a number of moles of cobalt to a total number of moles of metal other than lithium in the composition is 0.02 or more and 0.33 or less.

### Claim 17 (depends on 13)

The method according to claim 13, wherein
the lithium transition metal composite oxide particle has a composition comprising manganese, and wherein a ratio of a number of moles of manganese to a total number of moles of metal other than lithium in the composition is 0.01 or more and 0.33 or less.

### Claim 18 (depends on 13)

The method according to claim 13, wherein
an oxide containing lithium and aluminum adhering to a surface of the lithium transition metal composite oxide particle after the heat treatment has a volume-based particle diameter distribution in which a total volume percentage of particles having a particle diameter of 0.4 μm to 3.0 μm is greater than 50%.

### Claim 19 (depends on 13)

The method according to claim 13, wherein a volume average particle diameter of the lithium transition metal composite oxide particle is 2 μm to 25 μm.

### Claim 20 (depends on 18)

The method according to claim 18, wherein a volume average particle diameter of the lithium transition metal composite oxide particle is 2 μm to 25 μm.