# US 2020/0266165 A1 · Copper pillars having improved integrity and methods of making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0266165 A1
- Document ID: US20200266165A1
- Status: Published application
- Kind: A1
- Application number: 16/866,709
- Filed: 2020-05-05
- Published: 2020-08-20
- Earliest claimed: 2018-02-21
- Applicants: Rohm and Haas Electronic Materials LLC
- Inventors: Ravi POKHREL; Michael K. Gallagher
- Web page: https://patentgrep.com/patent/US20200266165A1

## CPC

- C25D 3/38: of copper
- C25D 5/022: {using masking means}
- C25D 5/10: Electroplating with more than one layer of the same or of different metals (for bearings C25D7/10)
- C25D 5/18: Electroplating using modulated, pulsed or reversing current
- C25D 7/123: {Semiconductors first coated with a seed layer or a conductive layer}
- C25D 3/60: containing more than 50% by weight of tin
- H10W 72/01235: {by plating, e.g. electroless plating or electroplating}
- H10W 72/01238: {in gaseous form, e.g. by CVD or PVD}
- H10W 72/01255: {by using masks}
- H10W 72/01257: {by reflowing}
- H10W 72/0198: {batch processes}
- H10W 72/07255: {changes in materials}
- H10W 72/222: {Multilayered bumps, e.g. a coating on top and side surfaces of a bump core}
- H10W 72/224: {Bumps having multiple side-by-side cores}
- H10W 72/232: {Plan-view shape, i.e. in top view}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/2528: {Intermetallic compounds}
- H10W 72/90: Bond pads, in general
- H10W 95/00: Packaging processes not covered by the other groups of this subclass
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

The copper pillars have improved integrity such that they can readily withstand the harsh reflow conditions of post solder bump application without readily failing. The method of making the copper pillars having the improved integrity involves a two-step electroplating process of varying current densities.

## Claims

### Claim at position 1

1-3. (canceled)

### Claim at position 2

4: A method of electroplating copper pillars comprising:
a) providing a substrate comprising a layer of photoresist, wherein the layer of photoresist comprises a plurality of apertures;
b) providing a first copper electroplating bath comprising one or more sources of copper ions, one or more acids, one or more sources of chloride, one or more levelers, one or more accelerators; and one or more suppressors;
c) immersing the substrate comprising the layer of photoresist with the plurality of apertures in the first copper electroplating bath;
d) electroplating a first section of a copper pillar in each of the plurality of apertures at a first current density followed by electroplating a second section of the copper pillar in each of the plurality of apertures at a lower current density than the first current density with the first copper electroplating bath or, in the alternative, electroplating the second section of the copper pillar in each of the plurality of apertures at the lower current density with a second copper electroplating bath consisting of water, one or more sources of copper ions, one or more acids, and, optionally, one or more sources of chloride, one or more levelers, one or more accelerators and one more suppressors;
e) depositing a tin or tin alloy solder bump on a top of the second section of each copper pillar;
f) stripping the photoresist from the substrate leaving an array of copper pillars with tin or tin alloy solder bumps on the top of the second section of each copper pillar; and
g) reflow the array.

### Claim at position 3 (depends on 4)

5: The method of claim 4, wherein the first current density is greater than 10 ASD.

### Claim at position 4 (depends on 4)

6: The method of claim 4, wherein the second current density is 10 ASD or less.