# US 2020/0266101 A1 · Integrated circuit devices and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0266101 A1
- Document ID: US20200266101A1
- Status: Published application
- Kind: A1
- Application number: 16/868,811
- Filed: 2020-05-07
- Published: 2020-08-20
- Earliest claimed: 2018-05-23
- Assignees: Samsung Electronics Co., Ltd.
- Applicants: Samsung Electronics Co., Ltd.
- Inventors: Jin-yeong JOE; Seok-hoon KIM; Jeong-ho YOO; Seung-hun LEE; Geun-hee JEONG
- Web page: https://patentgrep.com/patent/US20200266101A1

## CPC

- H10D 30/6219: {characterised by the source or drain electrodes}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10D 84/834: {comprising FinFETs}
- H10W 20/43: Layouts of interconnections
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 30/6211: {having fin-shaped semiconductor bodies integral with the bulk semiconductor substrates}
- H10W 20/40: Interconnections external to wafers or substrates, e.g. back-end-of-line [BEOL] metallisations or vias connecting to gate electrodes
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

An integrated circuit device includes a fin-type active region extending on a substrate in a first direction parallel to a top surface of the substrate; a gate structure extending on the fin-type active region and extending in a second direction parallel to the top surface of the substrate and different from the first direction; and source/drain regions in a recess region extending from one side of the gate structure into the fin-type active region, the source/drain regions including an upper semiconductor layer on an inner wall of the recess region, having a first impurity concentration, and including a gap; and a gap-fill semiconductor layer, which fills the gap and has a second impurity concentration that is greater than the first impurity concentration.

## Claims

### Claim 1

A method of manufacturing an integrated circuit device, the method comprising:
forming a fin-type active region extending in a first direction on a substrate;
removing a portion of the fin-type active region to form a recess region extending into the fin-type active region;
forming an upper semiconductor layer, which includes a gap and is doped with a first impurity at a first impurity concentration, on an inner wall of the recess region; and
forming a gap-fill semiconductor layer, which fills the gap and is doped with the first impurity at a second impurity concentration higher than the first impurity concentration, on the upper semiconductor layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein,
in the forming of the upper semiconductor layer, a growth rate of the upper semiconductor layer in the first direction from a sidewall of the recess region is greater than a growth rate of the upper semiconductor layer in a third direction perpendicular to a top surface of the substrate from a bottom portion of the recess region.

### Claim 3 (depends on 1)

The method of claim 1, wherein,
in the forming of the upper semiconductor layer, the gap is formed in a center portion of the upper semiconductor layer and the gap extends in a third direction perpendicular to a top surface of the substrate.

### Claim 4 (depends on 1)

The method of claim 1, wherein,
in the forming of the upper semiconductor layer, the upper semiconductor layer covers a top surface of the gap-fill semiconductor layer and fills an upper portion of the recess region.

### Claim 5 (depends on 1)

The method of claim 1, wherein the forming of the upper semiconductor layer and the forming of the gap-fill semiconductor layer are performed at a process pressure from about 100 Torr to about 400 Torr.

### Claim 6 (depends on 1)

The method of claim 1, wherein,
in the forming of the upper semiconductor layer, the first impurity is in-situ doped in the upper semiconductor layer,
the first impurity concentration ranges from about 1E20 atoms/cm3 to about 1E22 atoms/cm3.

### Claim 7 (depends on 6)

The method of claim 6, wherein,
the second impurity concentration ranges from about 110% to about 150% of the first impurity concentration.

### Claim 8 (depends on 1)

The method of claim 1, further comprising:
prior to the forming of the upper semiconductor layer, forming a lower semiconductor layer, which is doped with the first impurity at a third impurity concentration, on the inner wall of the recess region,
wherein the forming of the upper semiconductor layer comprises forming the upper semiconductor layer on the lower semiconductor layer, which is disposed on the inner wall of the recess region.

### Claim 9 (depends on 8)

The method of claim 8, wherein,
the forming of the lower semiconductor layer comprises forming the lower semiconductor layer through an epitaxy process using a sidewall of the fin-type active region exposed at the inner wall of the recess region as a seed layer, and
the forming of the upper semiconductor layer comprises forming the upper semiconductor layer through an epitaxy process using a sidewall of the lower semiconductor layer exposed at the inner wall of the recess region as a seed layer.

### Claim 10 (depends on 1)

The method of claim 1, further comprising:
forming a capping semiconductor layer conformally on the upper semiconductor layer.

### Claim 11 (depends on 1)

The method of claim 1, further comprising:
forming a first gate structure and a second gate structure on portions of the fin-type active region at both sides of the recess region, the first and second gate structures extending in a second direction parallel to the top surface of the substrate and different from the first direction.

### Claim 12

A method of manufacturing an integrated circuit device, the method comprising:
forming a fin-type active region extending in a first direction on a substrate;
removing a portion of the fin-type active region to form a recess region extending into the fin-type active region;
forming a lower semiconductor layer on an inner wall of the recess region; and
forming an upper semiconductor layer, which includes a gap and is doped with a first impurity at a first impurity concentration, on the lower semiconductor layer exposed at the inner wall of the recess region, wherein
in the forming of the upper semiconductor layer, a gap-fill semiconductor layer, which fills the gap and is doped with the first impurity at a second impurity concentration higher than the first impurity concentration, is formed.

### Claim 13 (depends on 12)

The method of claim 12, wherein,
in the forming of the upper semiconductor layer, a growth rate of the upper semiconductor layer in the first direction from a sidewall of the recess region is greater than a growth rate of the upper semiconductor layer in a third direction perpendicular to a top surface of the substrate from a bottom portion of the recess region.

### Claim 14 (depends on 12)

The method of claim 12, wherein,
in the forming of the upper semiconductor layer, the gap is formed in a center portion of the upper semiconductor layer and the gap extends in a third direction perpendicular to a top surface of the substrate.

### Claim 15 (depends on 12)

The method of claim 12, wherein,
in the forming of the upper semiconductor layer, the upper semiconductor layer covers a top surface of the gap-fill semiconductor layer and fills an upper portion of the recess region.

### Claim 16 (depends on 12)

The method of claim 12, wherein the forming of the upper semiconductor layer is performed at a process pressure from about 100 Torr to about 400 Torr.

### Claim 17 (depends on 12)

The method of claim 12, wherein,
in the forming of the upper semiconductor layer, the first impurity is in-situ doped in the upper semiconductor layer,
the first impurity concentration ranges from about 1E20 atoms/cm3 to about 1E22 atoms/cm3.

### Claim 18 (depends on 12)

The method of claim 12, wherein the second impurity concentration ranges from about 110% to about 150% of the first impurity concentration.

### Claim 19 (depends on 12)

The method of claim 12, wherein
the forming of the lower semiconductor layer comprises forming the lower semiconductor layer through an epitaxy process using a sidewall of the fin-type active region exposed at the inner wall of the recess region as a seed layer, and
the forming of the upper semiconductor layer comprises forming the upper semiconductor layer through an epitaxy process using a sidewall of the lower semiconductor layer exposed at the inner wall of the recess region as a seed layer.

### Claim 20 (depends on 12)

The method of claim 12, further comprising:
forming a capping semiconductor layer conformally on the upper semiconductor layer; and
forming a first gate structure and a second gate structure on portions of the fin-type active region at both sides of the recess region, the first and second gate structures extending in a second direction parallel to the top surface of the substrate and different from the first direction.