# US 2020/0263359 A1 · Water-based coatings for cellulosic substrates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0263359 A1
- Document ID: US20200263359A1
- Status: Published application
- Kind: A1
- Application number: 16/868,856
- Filed: 2020-05-07
- Published: 2020-08-20
- Earliest claimed: 2017-11-13
- Assignees: Sun Chemical Corporation
- Applicants: Sun Chemical Corporation
- Inventors: Yongping Zha; Vanessa Gordon; Philippe Schottland
- Web page: https://patentgrep.com/patent/US20200263359A1

## CPC

- D21H 19/44: characterised by the other ingredients, e.g. the binder or dispersing agent
- D21H 19/58: Polymers or oligomers of diolefins, aromatic vinyl monomers or unsaturated acids or derivatives thereof
- C09D 7/20: Diluents or solvents
- C09D 7/61: inorganic
- C09D 7/65: macromolecular (C09D7/41-C09D7/48 take precedence)
- C09D 7/68: {Particle size between 100-1000 nm}
- C09D 7/69: {Particle size larger than 1000 nm}
- C09D 133/12: Homopolymers or copolymers of methyl methacrylate
- D21H 19/40: siliceous, e.g. clays
- D21H 19/80: Paper comprising more than one coating (D21H19/02 takes precedence)
- D21H 21/52: Additives of definite length or shape
- D21H 27/10: Packing paper (packaging materials of special type or form B65D65/38)
- Y02W 90/10: Bio-packaging, e.g. packing containers made from renewable resources or bio-plastics
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

The present invention provides water-based coatings that provide liquid resistance when applied to various substrates. In some embodiments, more than one layer of coatings can be applied, using multiple coating stations. The coatings are particularly suitable for cellulosic substrates such as paper or paper board. In addition to liquid resistance, the coatings have good heat sealability, and are resistant to roll blocking. Preferably, the coatings are recyclable and/or repulpable with the substrates to which they are applied. The coating compositions comprise one or more polymer binders, and one or more particles. Preferably, at least one polymer binder has a glass transition temperature (Tg) less than 10° C. Preferably, at least one polymer binder has a heat seal onset temperature of less than 200° C. Preferably, at least one particle has a mean particle size greater than 4 μm. It is also preferable that the particles have a melting point greater than 60° C.

## Claims

### Claim at position 1

1-89. (canceled)

### Claim 90

A water-based coating composition, comprising:
a) one or more polymer binders, in an amount of 25 wt % to 99 wt %, on a solids weight basis; and
b) one or more particles, in an amount of 0.1 wt % to 50 wt %, on a solids weight basis;
wherein at least one polymer binder has a glass transition temperature (Tg) of less than 10° C.;
wherein at least polymer binder has a heat seal onset temperature of less than 200° C.; and
wherein at least one particle has an average particle size of greater than 4 μm.

### Claim 91 (depends on 90)

The water-based coating composition of claim 90, comprising at least one polymer binder with a glass transition temperature (Tg) of −50° C. to 50° C.; and/or comprising at least one polymer binder with a Tg of 0° C. to 200° C.; and/or wherein at least one polymer binder has a heat seal onset temperature of 0° C. to 200° C.; and/or comprising at least one polymer binder with a Tg of less than 0° C.; comprising at least one polymer binder with an acid number of 10 mg KOH/g to 150 mg KOH/g; and/or wherein at least one particle has an average size of greater than 8 μm; and/or wherein at least one particle has a melting temperature (Tm) of greater than 60° C.

### Claim 92 (depends on 90)

The water-based coating composition of claim 90, wherein at least one particle is a talc wherein the talc particles have a median diameter S-D50 of 0.5 μm to 5 μm when measured by the SediGraph method, and/or wherein the talc particles have a median diameter L-D50 of 5 μm to 15 μm when measured by the laser diffraction method.

### Claim 93 (depends on 92)

The water-based coating composition of claim 92, wherein the talc particles have a lamellarity index of greater than 2.0; and/or wherein the talc has a specific surface area of 10 m2/g to 30 m2/g.

### Claim 94 (depends on 90)

The water-based coating composition of claim 90, further comprising a styrene-butadiene copolymer.

### Claim 95 (depends on 94)

The water-based coating composition of claim 94, wherein the styrene-butadiene copolymer has a glass transition temperature (Tg) of −30° C. to 30° C.

### Claim 96 (depends on 90)

The water-based coating composition of claim 90, having a glass transition temperature (Tg) of −50° C. to 50° C.; and/or having an acid value of 10 mg KOH/g to 150 mg KOH/g; and/or having a solids content of 20 wt % to 80 wt %; and/or having a viscosity of 10 cP to 10,000 cP; and/or wherein the total surface energy of the coating is less than 50 N/m; and/or wherein the polar part of the surface energy is less than 10 N/m.

### Claim 97 (depends on 90)

A method of coating a substrate, comprising the steps of:
a) applying the water-based coating composition of claim 90 on a substrate; and
b) drying the water-based coating composition on the substrate

### Claim 98 (depends on 97)

The method of claim 97, wherein the substrate is a cellulosic substrate.

### Claim 99 (depends on 97)

The method of claim 97, wherein a single layer of the water-based coating composition is applied to the substrate; or wherein more than one layer of the water-based coating composition is applied to the substrate.

### Claim 100 (depends on 97)

A coated substrate prepared by the method of claim 97.

### Claim 101 (depends on 100)

The coated substrate of claim 100, wherein the Cobb value of water absorption is less than or equal to 20 g/m2 per 30 minutes; and/or wherein a face-to-face heat seal, when made with a sealing bar at 160° C. and 40 psi for 1 sec provides adhesion to the extent of equal to or greater than 80% paper tear; and/or wherein a face-to-back heat seal, when made with a sealing bar at 160° C. and 40 psi for 1 sec provides adhesion to the extent of equal to or greater than 80% paper tear; and/or wherein a face-to-face heat seal, when made with a sealing bar at 121° C. and 50 psi for 3 sec provides adhesion to the extent of equal to or greater than 80% paper tear; and/or wherein a face-to-back heat seal, when made with a sealing bar at 121° C. and 50 psi for 3 sec provides adhesion to the extent of equal to or greater than 80% paper tear; and/or wherein when the coated samples placed face-to-face are conditioned at 50° C., 50 psi and 66% relative humidity (RH), provide roll block resistance to the extent of less than 80% paper tear; and/or wherein when the coated samples placed face-to-back are conditioned at 50° C., 50 psi and 66% relative humidity (RH), provide roll block resistance to the extent of less than 80% paper tear.

### Claim 102 (depends on 100)

An article comprising the coated substrate of claim 100.

### Claim 103

A method of coating a substrate, comprising:
a) providing a substrate;
b) applying two or more coatings to the substrate via flexography;
wherein more than one coating station is used for applying the coatings;
wherein the same or a different coating may be applied at each station;
wherein at least one coating is a water-based coating (A) comprising:
i) one or more polymer binders, in an amount of 25 wt % to 99 wt %, on a solids weight basis; and
ii) one or more particles, in an amount of 0.1 wt % to 50 wt %, on a solids weight basis;
wherein at least one polymer binder has a glass transition temperature (Tg) of less than 10° C.;
wherein at least one polymer binder has a heat seal onset temperature of less than 200° C.; and
wherein at least one particle has an average particle size of greater than 4 μm.

### Claim 104 (depends on 103)

The method of claim 103, wherein the coatings are dried on the substrate; and wherein each coating is dried before applying the next coating; or wherein the coatings are dried at intervals, after a specified number of coatings are applied; or wherein the coatings are dried simultaneously after the last coating is applied.

### Claim 105 (depends on 103)

The method of claim 103, wherein the substrate is a cellulosic substrate.

### Claim 106 (depends on 103)

A coated substrate prepared by the method of claim 103.

### Claim 107 (depends on 106)

The coated substrate of claim 106, wherein the Cobb value of water absorption is less than or equal to 20 g/m2 per 30 minutes; and/or wherein the “kit level” oil and grease resistance, measured according to the TAPPI T559 test protocol, is equal to or greater than 6; and/or wherein a face-to-face heat seal, when made with a sealing bar at 160° C. and 40 psi for 1 sec provides adhesion to the extent of equal to or greater than 80% paper tear; and/or wherein a face-to-back heat seal, when made with a sealing bar at 160° C. and 40 psi for 1 sec provides adhesion to the extent of equal to or greater than 80% paper tear; and/or wherein a face-to-face heat seal, when made with a sealing bar at 121° C. and 50 psi for 3 sec provides adhesion to the extent of equal to or greater than 80% paper tear; and/or wherein a face-to-back heat seal, when made with a sealing bar at 121° C. and 50 psi for 3 sec provides adhesion to the extent of equal to or greater than 80% paper tear; and/or wherein when the coated samples placed face-to-back are conditioned at 50° C., 50 psi and 66% relative humidity (RH), provide roll block resistance to the extent of less than 80% paper tear.

### Claim 108 (depends on 106)

An article comprising the coated substrate of claim 106.

### Claim 109

A method of coating a substrate, comprising:
a) providing a substrate;
b) applying two or more coatings to the substrate via flexography; and
wherein more than one coating station is used for applying the coatings;
wherein the same or a different coating may be applied at each station;

### Claim 110 (depends on 109)

The method of claim 109, wherein the coatings are dried on the substrate; and wherein each coating is dried before applying the next coating; or wherein the coatings are dried at intervals, after a specified number of coatings are applied; or wherein the coatings are dried simultaneously after the last coating is applied.

### Claim 111 (depends on 109)

The method of claim 109, wherein the substrate is a cellulosic substrate.

### Claim 112 (depends on 109)

A coated substrate prepared by the method of claim 109.

### Claim 113 (depends on 112)

The coated substrate of claim 112, wherein the Cobb value of water absorption is less than or equal to 20 g/m2 per 30 minutes; and/or wherein the “kit level” oil and grease resistance, measured according to the TAPPI T559 test protocol, is equal to or greater than 6; and/or wherein a face-to-face heat seal, when made with a sealing bar at 160° C. and 40 psi for 1 sec provides adhesion to the extent of equal to or greater than 80% paper tear; and.or wherein a face-to-back heat seal, when made with a sealing bar at 160° C. and 40 psi for 1 sec provides adhesion to the extent of equal to or greater than 80% paper tear; and/or wherein a face-to-face heat seal, when made with a sealing bar at 121° C. and 50 psi for 3 sec provides adhesion to the extent of equal to or greater than 80% paper tear; and/or wherein a face-to-back heat seal, when made with a sealing bar at 121° C. and 50 psi for 3 sec provides adhesion to the extent of equal to or greater than 80% paper tear; and/or wherein when the coated samples placed face-to-back are conditioned at 50° C., 50 psi and 66% relative humidity (RH), provide roll block resistance to the extent of less than 80% paper tear.

### Claim 114 (depends on 112)

An article comprising the coated substrate of claim 112.