# US 2020/0261979 A1 · Method for performing metal injection with counter pressure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0261979 A1
- Document ID: US20200261979A1
- Status: Published application
- Kind: A1
- Application number: 16/853,964
- Filed: 2020-04-21
- Published: 2020-08-20
- Earliest claimed: 2016-04-22
- Assignees: Chung Yuan Christian University
- Applicants: Chung Yuan Christian University
- Inventors: SHIA-CHUNG CHEN; JEN-AN CHANG; YUNG-HSIANG CHANG; KUAN-HUA LEE
- Web page: https://patentgrep.com/patent/US20200261979A1

## CPC

- B22F 3/225: {by injection molding}
- B22F 3/1021: {Removal of binder or filler (removal of binder from ceramics C04B35/638)}
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER

## Abstract

A system for metal injection and counter pressure has: a particle providing assembly; and a forming unit having a melting module, a counter pressure module and a mold module; wherein, the particle providing assembly provides particles with metal powder and a binding agent to the melting module, the particles are formed into melted flow by the melting module, the melted flow is provided to the mold module, the counter pressure module provides a counter gas with predetermined pressure to the mold module, the melted flow forms into a green part inside of the mold module.

## Claims

### Claim 1

A method for metal injection and counter pressure, comprising the steps of:
providing particles; and
enabling a green part to be molded in a manner that the particles are fed into a melting module for melting the particles into a melted flow that is guided to flow into a mold module while having a counter pressure module to apply a counter gas with a predetermined pressure to the mold module during the molding of the green part.

### Claim 2 (depends on 1)

The method of claim 1, wherein the predetermined pressure is ranged between 45 bar and 200 bar.

### Claim 3 (depends on 1)

The method of claim 1, wherein the providing of the particles further comprises a step selected from the group consisting of:
using a particle providing assembly to apply a mixing process, a blending process, a pulverizing process and a granulation process upon particles with metal powder and a binding agent so as to transforming the mixture of the particles with metal powder and the binding agent into the particles; and
using a mixing unit to mix particles with metal powder and a binding agent to form a mixture, and then providing the mixture to a blending unit to be blended into a blend, and then providing the blend to a pulverizing unit to be pulverized into a powder, and then providing the powder to a granulation unit to be granulated into the particles.

### Claim 4 (depends on 3)

The method of claim 3, wherein the mixing unit is operated at 180° C. to 220° C. to mix particles with metal powder.

### Claim 5 (depends on 1)

The method of claim 1, further comprising the steps of:
providing the green part to a debinding unit for applying a debinding process to the green part at a first preset temperature; and
providing the green part after debinding to a sintering unit for applying a sintering process to the green part at a second preset temperature so as to sinter the green part into an end product.

### Claim 6 (depends on 5)

The method of claim 5, wherein the first preset temperature is between 40° C. and 60° C.

### Claim 7 (depends on 5)

The method of claim 5, wherein the debinding of the green part is composed in sequence of a cold debinding procedure and a thermal debinding procedure; and
wherein when the binding agent is a polymer material, the debinding of the green part is performed with an acid gas for removing the polymer material from the green part.

### Claim 8 (depends on 1)

The method of claim 1, wherein the particles comprises metal powder and a binding agent, the binding agent comprises paraffin and a polymer material, the metal particle is 50% to 70%, the polymer material is 19% to 29%, and the paraffin is 11% to 21%.