# US 2020/0255965 A1 · Coating Laminated Body and Method for Producing the Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0255965 A1
- Document ID: US20200255965A1
- Status: Published application
- Kind: A1
- Application number: 16/650,626
- Filed: 2018-05-08
- Published: 2020-08-13
- Earliest claimed: 2017-09-27
- Assignees: Hitachi, Ltd.
- Applicants: Hitachi, Ltd.
- Inventors: Toshinori KAWAMURA; Hiroshi KANEMOTO
- Web page: https://patentgrep.com/patent/US20200255965A1

## CPC

- B32B 15/01: all layers being exclusively metallic {(making layered metal workpieces by pressure cladding B23K20/22; making coatings with a metallic material characterised by its composition C23C30/00)}
- C25D 5/14: two or more layers being of nickel or chromium, e.g. duplex or triplex layers
- C25D 5/50: by heat-treatment
- C25D 5/611: {Smooth layers}
- C25D 5/617: {Crystalline layers}
- B32B 15/04: comprising metal as the main or only constituent of a layer, {which is} next to another layer of {the same or of} a {different material (next to a bituminous or tarry layer B32B11/08; next to a water-setting substance layer B32B13/06; next to a glass layer B32B17/061; next to a cellulosic plastic layer B32B23/042)}
- C25D 3/562: {containing more than 50% by weight of iron or nickel or cobalt}
- Y10T 428/12049: Nonmetal component
- Y10T 428/12069: Plural nonparticulate metal components
- Y10T 428/12076: Next to each other
- Y10T 428/12083: Nonmetal in particulate component
- Y10T 428/12118: Nonparticulate component has Ni-, Cu-, or Zn-base
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

An object of the invention is to provide a coating laminated body in which coatings not containing hexavalent chromium which is an environmental concern material, and excellent in corrosion resistance and wear resistance are laminated on a base material, and to provide a method for producing the same. The coating laminated body according to the invention is a laminated body in which a multiple-layer coating is laminated on a base material. The multiple-layer coating includes: a plurality of layers of S-containing Ni alloy coatings; and a sulfur concentrated layer that is formed between the plurality of layers of S-containing Ni alloy coatings and has an S concentration higher than an S concentration of the S-containing Ni alloy coatings. Each of the plurality of layers of S-containing Ni alloy coatings has a Ni concentration of 90% or more by mass, and a difference in Ni concentration between the coatings is within 1% by mass.

## Claims

### Claim 1

A coating laminated body comprising:
a base material; and
a multiple-layer coating laminated on the base material, wherein
the multiple-layer coating includes a plurality of layers of sulfur-containing nickel alloy coatings; and a sulfur concentrated layer that is formed between the plurality of layers of sulfur-containing nickel alloy coatings, and has a sulfur concentration higher than a sulfur concentration of the sulfur-containing nickel alloy coatings, and
each of the plurality of layers of sulfur-containing nickel alloy coatings has a nickel concentration of 90% or more by mass, and a difference in the nickel concentration between the sulfur-containing nickel alloy coatings is within 1% by mass.

### Claim 2 (depends on 1)

The coating laminated body according to claim 1, wherein the sulfur concentration of the sulfur concentrated layer is 102% or more of the sulfur concentration of the plurality of sulfur-containing nickel alloy coatings.

### Claim 3 (depends on 1)

The coating laminated body according to claim 1, wherein
each of the plurality of layers of sulfur-containing nickel alloy coatings has an identical thickness.

### Claim 4 (depends on 1)

The coating laminated body according to claim 1, wherein
each of the plurality of layers of sulfur-containing nickel alloy coatings has a thickness of 300 nm or more and 1000 nm or less.

### Claim 5 (depends on 1)

The coating laminated body according to claim 1, wherein
each of the plurality of layers of sulfur-containing nickel alloy coatings further contains phosphorus.

### Claim 6 (depends on 1)

The coating laminated body according to claim 1, wherein
each of the plurality of layers of sulfur-containing nickel alloy coatings has an average crystal grain size of 8 nm or less.

### Claim 7 (depends on 1)

A method for producing the coating laminated body according to claim 1, comprising:
a nickel alloy coating plating treatment step being performed for a plurality of times; and
an annealing treatment step, wherein
the annealing treatment step is performed at an annealing temperature of 300° C. or less.

### Claim 8 (depends on 7)

The method for producing the coating laminated body according to claim 7, wherein
a plating treatment stop step is interposed between the plurality of nickel alloy coating plating treatment steps.