# US 2020/0247710 A1 · Method for manufacturing optical fiber parent material, and method for manufacturing optical fiber

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0247710 A1
- Document ID: US20200247710A1
- Status: Published application
- Kind: A1
- Application number: 16/641,778
- Filed: 2018-08-28
- Published: 2020-08-06
- Earliest claimed: 2017-08-31
- Assignees: Sumitomo Electric Industries, Ltd.
- Applicants: Sumitomo Electric Industries, Ltd.
- Inventors: Satoshi TANAKA; Tetsuya HARUNA
- Web page: https://patentgrep.com/patent/US20200247710A1

## CPC

- C03B 37/01815: {Reactant deposition burners or deposition heating means}
- C03B 37/01869: {Collapsing}
- C03B 37/012: Manufacture of preforms for drawing fibres or filaments
- C03B 37/01205: {starting from tubes, rods, fibres or filaments (C03B37/014 takes precedence)}
- C03B 37/018: by glass deposition on a glass substrate, e.g. by {inside-, modified-, plasma- or plasma modified-} chemical vapour deposition {[ICVD, MCVD, PCVD, PMCVD], i.e. by thin layer coating on the inside or outside of a glass tube or on a glass rod} (C03B37/016 takes precedence; surface treatment of glass by coating with glass C03C17/02)
- C03B 37/025: from reheated softened tubes, rods, fibres or filaments {, e.g. drawing fibres from preforms (draw-down of tubes, rods or preforms to reduced diameter preforms C03B37/0124)}
- C03B 37/027: Fibres composed of different sorts of glass, {e.g. glass optical fibres}(C03B37/0253, C03B37/028 take precedence)
- C03C 25/68: by etching
- G02B 6/02: Optical fibres with cladding {with or without a coating}
- C03B 37/01211: {by inserting one or more rods or tubes into a tube}
- C03B 37/014: made entirely or partially by chemical means {, e.g. vapour phase deposition of bulk porous glass either by outside vapour deposition [OVD], or by outside vapour phase oxidation [OVPO] or by vapour axial deposition [VAD] (C03C17/02 takes precedence)}
- C03B 2201/12: doped with fluorine (C03B2201/14 takes precedence)
- C03B 2201/20: doped with non-metals other than boron or fluorine
- C03B 2201/23: doped with hydroxyl groups
- C03B 2201/50: doped with alkali metals
- C03B 2203/23: Double or multiple optical cladding profiles
- C03B 2203/29: Segmented core fibres
- C03B 2207/66: Relative motion
- C03B 2207/90: with vapour generated from solid glass precursors, i.e. by sublimation
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

A method for manufacturing an optical fiber preform including a core part and a cladding part is disclosed. The method includes: adding an alkali metal to an inner surface of a silica-based glass pipe; etching the inner surface of the silica-based glass pipe to which the alkali metal is added; making a glass rod by collapsing the silica-based glass pipe after the etching; and making an optical fiber preform using the glass rod. The silica-based glass pipe is heated in the adding such that a surface temperature of the silica-based glass pipe falls within a temperature range of 1500° C. or higher to lower than 2000° C.

## Claims

### Claim 1

A method for manufacturing an optical fiber preform including a core part and a cladding part, comprising:
adding an alkali metal to an inner surface of a silica-based glass pipe;
etching the inner surface of the silica-based glass pipe to which the alkali metal is added;
making a glass rod by collapsing the silica-based glass pipe after the etching; and
making an optical fiber preform using the glass rod,
wherein the silica-based glass pipe is heated in the adding such that a surface temperature of the silica-based glass pipe falls within a temperature range of 1500° C. or higher to lower than 2000° C.

### Claim 2 (depends on 1)

The method for manufacturing an optical fiber preform according to claim 1, wherein in the adding, the heating time per traverse with which a surface temperature of a predetermined area of the silica-based glass pipe falls within a temperature range of 1500° C. or higher to lower than 2000° C. is 0.5 minute or longer and shorter than 40 minutes.

### Claim 3 (depends on 2)

The method for manufacturing an optical fiber preform according to claim 2, wherein in the adding, the heating time per traverse with which the surface temperature of the predetermined area of the silica-based glass pipe falls within a temperature range of 1500° C. or higher to lower than 2000° C. is 1 minute or longer.

### Claim 4 (depends on 2)

The method for manufacturing an optical fiber preform according to claim 2, wherein in the adding, the heating time per traverse with which the surface temperature of the predetermined area of the silica-based glass pipe falls within a temperature range of 1500° C. or higher to lower than 2000° C. is shorter than 20 minutes.

### Claim 5 (depends on 1)

The method for manufacturing an optical fiber preform according to claim 1, wherein in the adding,
the silica-based glass pipe is heated by a heating burner such that the surface temperature of the silica-based glass pipe falls within a temperature range of 1500° C. or higher to lower than 2000° C., and
the width that achieves a temperature zone of 1500° C. or higher in the heating temperature profile of the heating burner is kept to be not more than six times a diameter of the silica-based glass pipe.

### Claim 6 (depends on 1)

The method for manufacturing an optical fiber preform according to claim 1, wherein in the adding, the silica-based glass pipe is heated such that the surface temperature of the silica-based glass pipe falls within a temperature range of 1500° C. or higher to lower than 1800° C.

### Claim 7 (depends on 1)

The method for manufacturing an optical fiber preform according to claim 1, wherein in the adding,
a space in which the silica-based glass pipe is held is kept at a positive pressure, and
the internal pressure in the space is greater than 0 Pa and 20 Pa or less.

### Claim 8 (depends on 1)

The method for manufacturing an optical fiber preform according to claim 1,
wherein the alkali metal added in the adding is potassium, and
wherein the silica-based glass pipe is repeatedly heated in the adding such that the ratio d2/d1 in the optical fiber preform is 1.5 or more and less than 3.0 where d1 is the diameter of an area in which the potassium concentration in the optical fiber preform is 50 [atomic ppm] or more, and d2 is the diameter of an area in which the potassium concentration in the optical fiber preform is 50 [atomic ppm] or less and the chlorine concentration is 1000 [atomic ppm] or less.

### Claim 9 (depends on 1)

A method for manufacturing an optical fiber using an optical fiber preform manufactured by the method for manufacturing an optical fiber preform according to claim 1, the method for manufacturing an optical fiber further comprising drawing the optical fiber preform to manufacture an optical fiber.

### Claim 10 (depends on 2)

The method for manufacturing an optical fiber preform according to claim 2, wherein in the adding,
the silica-based glass pipe is heated by a heating burner such that the surface temperature of the silica-based glass pipe falls within a temperature range of 1500° C. or higher to lower than 2000° C., and
the width that achieves a temperature zone of 1500° C. or higher in the heating temperature profile of the heating burner is kept to be not more than six times a diameter of the silica-based glass pipe.

### Claim 11 (depends on 10)

The method for manufacturing an optical fiber preform according to claim 10, wherein in the adding, the silica-based glass pipe is heated such that the surface temperature of the silica-based glass pipe falls within a temperature range of 1500° C. or higher to lower than 1800° C.

### Claim 12 (depends on 10)

The method for manufacturing an optical fiber preform according to claim 10, wherein in the adding,
a space in which the silica-based glass pipe is held is kept at a positive pressure, and
the internal pressure in the space is greater than 0 Pa and 20 Pa or less.

### Claim 13 (depends on 12)

The method for manufacturing an optical fiber preform according to claim 12,
wherein the alkali metal added in the adding is potassium, and
wherein the silica-based glass pipe is repeatedly heated in the adding such that the ratio d2/d1 in the optical fiber preform is 1.5 or more and less than 3.0 where d1 is the diameter of an area in which the potassium concentration in the optical fiber preform is 50 [atomic ppm] or more, and d2 is the diameter of an area in which the potassium concentration in the optical fiber preform is 50 [atomic ppm] or less and the chlorine concentration is 1000 [atomic ppm] or less.