# US 2020/0232080 A1 · Method for and equipment for suppressing discoloration of al-mg products

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0232080 A1
- Document ID: US20200232080A1
- Status: Published application
- Kind: A1
- Application number: 16/731,136
- Filed: 2019-12-31
- Published: 2020-07-23
- Earliest claimed: 2019-01-17
- Assignees: Norsk Hydro ASA
- Applicants: Norsk Hydro Asa
- Inventors: Alf Inge ROMFO; Snorre RIST; Idar Kjetil STEEN; Geir ØYEN; Øystein BAUGER; Oddvin REISO; Tanja PETTERSEN
- Web page: https://patentgrep.com/patent/US20200232080A1

## CPC

- C21D 11/00: Process control or regulation for heat treatments
- C22F 1/047: of alloys with magnesium as the next major constituent
- C21D 9/0081: {for slabs; for billets}
- C21D 9/70: Furnaces for ingots, i.e. soaking pits
- C22C 21/06: with magnesium as the next major constituent
- C22C 21/08: with silicon
- C22F 1/02: in inert or controlled atmosphere or vacuum (adjusting the composition of the atmosphere C21D1/76)
- C22F 1/05: of alloys of the Al-Si-Mg type, i.e. containing silicon and magnesium in approximately equal proportions
- F27B 5/04: adapted for treating the charge in vacuum or special atmosphere
- F27B 5/16: Arrangements of air or gas supply devices
- F27D 7/02: Supplying steam, vapour, gases or liquids
- F27D 7/06: Forming or maintaining special atmospheres or vacuum within heating chambers (supplying steam, vapour, gases or liquids F27D7/02)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- F27B: FURNACES, KILNS, OVENS OR RETORTS IN GENERAL; OPEN SINTERING OR LIKE APPARATUS
- F27D: DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS OR RETORTS, IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KIND OF FURNACE

## Abstract

Method and means for suppressing discoloration during thermal treatment of a product of a magnesium containing aluminium alloy, the alloy contains in wt. % Mg: 0.45-12.0, with a preferred range of 0.45-6.0 wt %. The product, being either an extrusion billet, a sheet ingot, a cast product, or a forged product is heated to a temperature T where it is prone to surface discoloration and oxidation, wherein during the thermal treatment it is exposed to a suppressing atmosphere comprising 0.5-5.0% CO2 gas with a preference for 0.5-1.5% CO2 gas. FIG. 3 to be published with the abstract

## Claims

### Claim 1

A method for suppressing discoloration during thermal treatment of a product of a magnesium containing aluminium alloy, the alloy containing in wt. %
Mg: 0.45-12.0
where the product, being either an extrusion billet, a sheet ingot or a cast product, is heated to a temperature T where it is prone to surface oxidation,
wherein
it during the thermal treatment is exposed to a suppressing atmosphere comprising 0.5-5.0% CO2 gas.

### Claim 2 (depends on 1)

The method according to claim 1,
wherein
the rest of the suppressing atmosphere comprises natural air.

### Claim 3 (depends on 1)

The method according to claim 1,
wherein
the rest of the suppressing atmosphere comprises a mix of natural air and exhaust gases from combustion of natural gas or other gas compositions.

### Claim 4 (depends on 1)

The method according to claim 1,
wherein
the suppressing atmosphere comprises 0.5-1.5 CO2 gas.

### Claim 5 (depends on 1)

The method according to claim 1,
wherein
the suppressing atmosphere comprises approximately 1.0% CO2 gas.

### Claim 6 (depends on 1)

The method according to claim 1,
wherein
the suppressing atmosphere comprises 1.0% CO2 gas and 99% air.

### Claim 7 (depends on 1)

The method according to claim 1,
wherein
the alloy contains 0.45-6 wt % Mg

### Claim 8 (depends on 1)

The method according to claim 1,
wherein
the cast product has been exposed to various degree of forming or machining between casting and heat treatment.

### Claim 9 (depends on 1)

The method according to claim 1,
wherein
the heat treatment temperature T is between 450° C. and the melting point of the alloy.

### Claim 10 (depends on 1)

The method according to claim 1,
wherein
a holding time of up to 15 hours at the temperature T is applied.

### Claim 11 (depends on 1)

An equipment for facilitating the method according to claim 1, the equipment includes at least one zone or chamber for thermal treatment of the products,
wherein
the zone or chamber is provided with means for bringing a suppressing atmosphere in contact with the surface of the products.

### Claim 12 (depends on 11)

The equipment according to claim 11,
wherein
the equipment is provided with means for controlling the CO2 concentration in the atmosphere, the means comprising a sensor connected to a PLC that controls the outlet of a CO2 source or the outlet of the heating zone or chamber.