# US 2020/0206983 A1 · Method of preparing a biodegradable film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0206983 A1
- Document ID: US20200206983A1
- Status: Published application
- Kind: A1
- Application number: 16/728,080
- Filed: 2019-12-27
- Published: 2020-07-02
- Earliest claimed: 2019-01-02
- Assignees: National Tsing Hua University
- Applicants: National Tsing Hua University
- Inventors: Erh-Yeh Tsou; Ta-Jo Liu; Jane Wang
- Web page: https://patentgrep.com/patent/US20200206983A1

## CPC

- B29C 41/003: {characterised by the choice of material}
- B29C 41/20: incorporating preformed parts or layers, e.g. moulding inserts or for coating articles
- B29C 41/42: Removing articles from moulds, cores or other substrates {(B29C33/444 and B29C37/0017 take precedence)}
- B29C 41/50: Shaping under special conditions, e.g. vacuum
- B29K 2067/00: Use of polyesters {or derivatives thereof}, as moulding material
- B29K 2801/08: Cellulose derivatives
- B29K 2805/00: Use of polysaccharides or derivatives as mould material
- B29K 2995/006: Bio-degradable, e.g. bioabsorbable, bioresorbable or bioerodible
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

Provided is a method of preparing a biodegradable film, which comprises the steps of coating a soluble supporting solution on a substrate, coating a prepolymer solution, pre-drying, crosslinking, and separating. With the technical means, the method can separate the biodegradable film from the substrate smoothly, thereby ensuring the film integrity of the produced biodegradable film.

## Claims

### Claim 1

A method of preparing a biodegradable film comprising:
coating a soluble supporting solution on a substrate to form a soluble supporting layer on the substrate, wherein a material of the soluble supporting solution includes glucose, fructose, galactose, saccharose, maltose, lactose, corn syrup, methyl cellulose, carboxymethyl cellulose, hydroxyethyl cellulose, carboxymethyl hydroxyethylcellulose, hydroxypropyl cellulose, hydroxypropyl methyl cellulose, starch, chitosan, chitin, polyvinyl alcohol or their combinations;
coating a prepolymer solution on the soluble supporting layer to obtain a cross-linkable laminate, the cross-linkable laminate comprising the substrate, the soluble supporting layer and the prepolymer solution in a bottom-up sequence;
pre-drying the cross-linkable laminate to dry the prepolymer solution into a prepolymer layer, so as to obtain a dried cross-linkable laminate, the prepolymer layer containing a prepolymer;
subjecting the prepolymer in the dried cross-linkable laminate to a crosslinking reaction to obtain a cross-linked laminate; and
releasing the biodegradable film from the substrate of the cross-linked laminate.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein a viscosity of the soluble supporting solution is from 5 cP to 100,000 cP.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein the crosslinking reaction includes photo crosslinking reaction, thermal crosslinking or their combinations.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein the crosslinking reaction is performed under an anoxic condition to obtain the cross-linked laminate, and a vacuum degree of the anoxic condition is lower than 1 torr.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein the crosslinking reaction is performed under an anoxic condition to obtain the cross-linked laminate, and the anoxic condition is flowed with gas of nitrogen, argon, helium, neon, krypton, xenon, radon, carbon dioxide or their combinations.

### Claim 6 (depends on 5)

The method as claimed in claim 5, wherein the flow rate of the gas in the anoxic condition is from 0.5 L/min to 1 L/min.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein the prepolymer is prepared by a mixture containing a polyhydric alcohol and a poly acid, and the polyhydric alcohol is selected from the group consisting of glycerol, ethylene glycol, propylene glycol, butanediol, pentanediol, hexanediol, cyclopentanediol, cyclohexanediol and their combinations, and the poly acid is selected from the group consisting of oxalic acid, malonic acid, succinic acid, glutaric acid, adipic acid, pimelic acid, suberic acid, azelaic acid, sebacic acid, butenedioic acid, glutaconic acid, citric acid and their combinations.

### Claim 8 (depends on 1)

The method as claimed in claim 1, wherein a viscosity of the soluble supporting solution is from 500 cP to 46,000 cP.

### Claim 9 (depends on 1)

The method as claimed in claim 1, wherein a temperature for pre-drying the cross-linkable laminate is from 25° C. to 90° C.

### Claim 10 (depends on 1)

The method as claimed in claim 1, wherein a residual solvent contained in the prepolymer layer is less than 40%.

### Claim 11 (depends on 1)

The method as claimed in claim 1, wherein the method includes a water washing step of immersing the cross-linked laminate in water at a temperature between 10° C. and 90° C., so as to release the biodegradable film from the substrate of the cross-linked laminate.

### Claim 12 (depends on 3)

The method as claimed in claim 3, wherein the method includes a water washing step of immersing the cross-linked laminate in water at a temperature between 10° C. and 90° C., so as to release the biodegradable film from the substrate of the cross-linked laminate.

### Claim 13 (depends on 4)

The method as claimed in claim 4, wherein the method includes a water washing step of immersing the cross-linked laminate in water at a temperature between 10° C. and 90° C., so as to release the biodegradable film from the substrate of the cross-linked laminate.

### Claim 14 (depends on 5)

The method as claimed in claim 5, wherein the method includes a water washing step of immersing the cross-linked laminate in water at a temperature between 10° C. and 90° C., so as to release the biodegradable film from the substrate of the cross-linked laminate.

### Claim 15 (depends on 1)

The method as claimed in claim 1, wherein the biodegradable film has Young's modulus ranging from 1 MPa to 2800 MPa, an ultimate tensile strength ranging from 0.25 MPa to 80 MPa, and an elongation at break from 1.5% to 110%.

### Claim 16 (depends on 2)

The method as claimed in claim 2, wherein the biodegradable film has Young's modulus ranging from 1 MPa to 2800 MPa, an ultimate tensile strength ranging from 0.25 MPa to 80 MPa, and an elongation at break from 1.5% to 110%.

### Claim 17 (depends on 3)

The method as claimed in claim 3, wherein the biodegradable film has Young's modulus ranging from 1 MPa to 2800 MPa, an ultimate tensile strength ranging from 0.25 MPa to 80 MPa, and an elongation at break from 1.5% to 110%.

### Claim 18 (depends on 4)

The method as claimed in claim 4, wherein the biodegradable film has Young's modulus ranging from 1 MPa to 2800 MPa, an ultimate tensile strength ranging from 0.25 MPa to 80 MPa, and an elongation at break from 1.5% to 110%.

### Claim 19 (depends on 5)

The method as claimed in claim 5, wherein the biodegradable film has Young's modulus ranging from 1 MPa to 2800 MPa, an ultimate tensile strength ranging from 0.25 MPa to 80 MPa, and an elongation at break from 1.5% to 110%.

### Claim 20 (depends on 11)

The method as claimed in claim 11, wherein the biodegradable film has Young's modulus ranging from 1 MPa to 2800 MPa, an ultimate tensile strength ranging from 0.25 MPa to 80 MPa, and an elongation at break from 1.5% to 110%.