# US 2020/0206575 A1 · Golf ball and method of manufacture

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0206575 A1
- Document ID: US20200206575A1
- Status: Published application
- Kind: A1
- Application number: 16/725,002
- Filed: 2019-12-23
- Published: 2020-07-02
- Earliest claimed: 2018-12-27
- Assignees: Bridgestone Sports Co., Ltd.
- Applicants: Bridgestone Sports Co., Ltd.
- Inventors: Jun SHINDO
- Web page: https://patentgrep.com/patent/US20200206575A1

## CPC

- A63B 37/0054: {Substantially rigid, e.g. metal}
- C08K 5/098: Metal salts of carboxylic acids
- A63B 37/006: {Physical properties}
- C08K 5/14: Peroxides
- C08K 5/3477: Six-membered rings
- A63B 37/0039: {characterised by the material}
- A63B 37/0075: {Three piece balls, i.e. cover, intermediate layer and core}
- A63B 37/0076: {Multi-piece balls, i.e. having two or more intermediate layers}
- A63B 45/00: Apparatus or methods for manufacturing balls (working of plastics or substances in a plastic state B29)
- C08K 5/36: Sulfur-, selenium-, or tellurium-containing compounds {(C08K5/0091 takes precedence)}
- A63B: APPARATUS FOR PHYSICAL TRAINING, GYMNASTICS, SWIMMING, CLIMBING, OR FENCING; BALL GAMES; TRAINING EQUIPMENT (apparatus for passive exercising, massage A61H)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A golf ball having a center core, one or more envelope layer encasing the center core and one or more cover layer is provided wherein at least one envelope layer is formed of a rubber composition that includes (a) a diene rubber, (b) a tetrazine compound of a specific formula or a metal salt thereof, (c) an α,β-unsaturated carboxylic acid metal salt and (d) an organic peroxide. A method for manufacturing the golf ball is also provided. The golf ball has a high rebound and durability. The manufacturing method, by eliminating the need to furnish equipment for a bonding step, lowers production costs and is industrially advantageous.

## Claims

### Claim 1

A golf ball comprising a center core, one or more envelope layer encasing the center core and one or more cover layer, wherein at least one envelope layer is formed of a rubber composition comprising:
(a) a diene rubber;
(b) a tetrazine compound of the following general formula or a metal salt thereof
(wherein X1 and X2 are mutually like or unlike heterocyclic groups, at least one of which is a pyridyl group or a pyridazinyl group);
(c) an α,β-unsaturated carboxylic acid metal salt; and
(d) an organic peroxide.

### Claim 2 (depends on 1)

The golf ball of claim 1, wherein the heterocyclic group in the component (b) formula is a 2-pyridyl group.

### Claim 3 (depends on 2)

The golf ball of claim 2, wherein component (b) is 3,6-bis(2-pyridyl)-1,2,4,5-tetrazine.

### Claim 4 (depends on 1)

The golf ball of claim 1, wherein the unsaturated carboxylic acid metal salt of component (c) is a zinc salt.

### Claim 5 (depends on 1)

The golf ball of claim 1, wherein the rubber composition further comprises an organosulfur compound.

### Claim 6 (depends on 1)

The golf ball of claim 1, wherein the rubber composition prior to vulcanization has a Mooney viscosity at 30° C. and a Mooney viscosity at 80° C. with a difference therebetween of at least 40 points.

### Claim 7

A method for manufacturing golf balls that includes fabricating a core member having a center core encased by an envelope layer, which method comprises the steps of:
pre-molding, as a material for forming the envelope layer, a rubber composition that includes (a) a diene rubber, (b) a tetrazine compound of the following general formula or a metal salt thereof
(wherein X1 and X2 are mutually like or unlike heterocyclic groups, at least one of which is a pyridyl group or a pyridazinyl group), (c) an α,β-unsaturated carboxylic acid metal salt and (d) an organic peroxide into a cup-like shape at a temperature at or below the 10-hour half-life temperature of component (d) so as to give an unvulcanized cup-shaped molded material; and
encasing the center core with the unvulcanized cup-shaped molded material and molding under applied heat.

### Claim 8 (depends on 7)

The manufacturing method of claim 7 wherein the rubber composition prior to vulcanization has a Mooney viscosity at 30° C. and a Mooney viscosity at 80° C. with a difference therebetween of at least 40 points.

### Claim 9 (depends on 7)

The manufacturing method of claim 7, wherein component (b) in the rubber composition is reacted with component (a), forming a polymer that is included thereafter within the rubber composition.