# US 2020/0189004 A1 · Method for preparing nickel nanopowders and method for making nickel nanopowders into paste

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0189004 A1
- Document ID: US20200189004A1
- Status: Published application
- Kind: A1
- Application number: 16/608,951
- Filed: 2018-04-27
- Published: 2020-06-18
- Earliest claimed: 2017-04-28
- Assignees: Solueta
- Applicants: Solueta Co.,Ltd.
- Inventors: Eui-Hong MIN; Sang-Ho CHO; Buck-Keun CHOI
- Web page: https://patentgrep.com/patent/US20200189004A1

## CPC

- B22F 9/22: using gaseous reductors
- B22F 1/054: Nanosized particles
- B22F 1/10: Metallic powder containing lubricating or binding agents; Metallic powder containing organic material
- B22F 1/102: Metallic powder coated with organic material
- B22F 9/20: starting from solid metal compounds
- B22F 2301/15: Nickel or cobalt
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- H01G 4/008: Selection of materials
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)

## Abstract

Provided is a method for making nickel nanopowders into paste including: (a) preparing a nickel oxide configured in the form of an oxide; (b) preparing nano-sized nickel oxide nanopowders by pulverizing the nickel oxide; (c) a step of drying the nickel oxide nanopowders; (d) a step of preparing natural metal nickel nanopowders by preparing the nickel oxide nanopowders as the natural metal nickel nanopowders through a reduction process in a hydrogen atmosphere and heat-treating the same at the same time; (e) a step of simultaneously performing a step of crushing the natural metal nickel nanopowders prepared by the heat treatment and a nanopowder oxidation preventing coating step of forming an oxidation preventing film on the natural metal nickel nanopowders with an additive; and (f) a step of making the natural metal nickel nanopowders, which have been simultaneously subjected to the crushing and coating steps, into paste.

## Claims

### Claim 1

A method for making a nickel nanopowder into a paste, the method comprising:
(a) a step of preparing a nickel oxide configured in the form of an oxide;
(b) a nickel oxide nanopowder preparation step of pulverizing the nickel oxide to prepare a nano-sized nickel oxide nanopowder;
(c) a step of drying the nickel oxide nanopowder;
(d) a step of preparing the nickel oxide nanopowder into a natural metal nickel nanopowder by a reduction process in a hydrogen atmosphere and heat-treating the nickel oxide nanopowder at the same time to prepare the natural metal nickel nanopowder;
(e) a step of simultaneously performing a step of crushing the natural metal nickel nanopowder produced by the heat-treatment process and a nanopowder oxidation preventing coating step of forming an oxidation preventing film on the crushed natural metal nickel nanopowder with an additive; and
(f) a step of making the natural metal nickel nanopowder which has been formed by simultaneously performing the crushing step and the coating step into the paste.

### Claim 2 (depends on 1)

The method of claim 1, wherein the step (b) includes preparing a nano-sized nickel oxide nanopowder by milling the nickel oxide by a rotating mill using a pulverizing medium.

### Claim 3 (depends on 2)

The method of claim 2, wherein the nickel oxide nanopowder is made into the paste by pulverizing the nickel oxide at a rotation speed of 1,000 to 4,000 rpm for 10 to 30 hours by using beads with a diameter of 0.3 to 3.0 mm as the pulverizing medium and using methanol or ethanol as a solvent.

### Claim 4 (depends on 3)

The method of claim 3, wherein the beads are formed of at least one material selected from SUS (stainless steel), Zr, carbon steel, and steel.

### Claim 5 (depends on 1)

The method of claim 1, wherein the step (d) includes preparing the natural metal nickel nanopowder from the nickel oxide nanopowder by the reduction process in the hydrogen atmosphere, and supplying heat at the same time.

### Claim 6 (depends on 5)

The method of claim 5, wherein the hydrogen reduction process is performed at a hydrogen injection flow rate of 2.5 to 7.0 L/min and a temperature of 250° C. and 400° C. for a process time of 0.5 to 5.0 hr.

### Claim 7 (depends on 1)

The method of claim 1, wherein the step (e) includes performing the crushing process at a rotation speed of 1,000 to 4,000 rpm for 1 to 5 hours using beads with a diameter of 0.3 to 3.0 mm as a crushing medium.

### Claim 8 (depends on 1)

The method of claim 1, wherein the step (e) includes forming an oxidation preventing film on the crushed natural metal nickel nanopowder with an additive, and the additive is triethanolamine (TEA).

### Claim 9 (depends on 1)

The method of claim 1, wherein the step (f) includes performing a vacuum stirring process of stirring any one selected from methanol, ethanol, methyl ethyl ketone, toluene, ethyl acetate, and wax along with the nickel nanopowder in a vacuum state, and performing a vacuum defoaming process at a rotation speed of 500 to 1,500 rpm for 30 to 90 minutes.