# US 2020/0184936 A1 · Guitar and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0184936 A1
- Document ID: US20200184936A1
- Status: Published application
- Kind: A1
- Application number: 16/787,340
- Filed: 2020-02-11
- Published: 2020-06-11
- Earliest claimed: 2017-08-11
- Assignees: Guangzhou Lava Music Info Tech Ltd.
- Applicants: Guangzhou Lava Music Info Tech Ltd.
- Inventors: ZI-TIAN LU; RUI ZHONG
- Web page: https://patentgrep.com/patent/US20200184936A1

## CPC

- G10D 3/22: Material for manufacturing stringed musical instruments; Treatment of the material
- B29C 45/76: Measuring, controlling or regulating {(measuring in general G01; controlling or regulating in general G05)}
- B29C 45/77: of velocity or pressure of moulding material
- B29C 45/78: of temperature
- C08K 7/02: Fibres or whiskers
- C08K 7/06: Elements
- C08K 7/14: Glass
- G10D 1/08: Guitars
- G10D 3/04: Bridges
- G10D 3/06: Necks; Fingerboards, e.g. fret boards
- B29C 2045/0096: {drying the moulding material before injection, e.g. by heating}
- B29C 2945/76732: Mould
- B29L 2031/758: {Musical equipment}
- C08K 2201/004: Additives being defined by their length
- G10D: STRINGED MUSICAL INSTRUMENTS; WIND MUSICAL INSTRUMENTS; ACCORDIONS OR CONCERTINAS; PERCUSSION MUSICAL INSTRUMENTS; AEOLIAN HARPS; SINGING-FLAME MUSICAL INSTRUMENTS; MUSICAL INSTRUMENTS NOT OTHERWISE PROVIDED FOR (organs, harmoniums or similar wind musical instruments with associated blowing apparatus G10B; pianos, harpsichords, spinets or similar stringed musical instruments with one or more keyboards G10C; automatic musical instruments G10F; electrophonic musical instruments in which tones are generated by electromechanical means G10H)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

A guitar includes fibers of lengths between 0.2 millimeters to 3 millimeters. The guitar further includes a guitar body, a headstock board, a soundboard, a fretboard, and a guitar bridge. Each of the guitar body, the headstock board, the soundboard, the fretboard, and the guitar bridge is a continuous and single structure. The disclosure also relates to a guitar and a method for manufacturing a guitar. The guitar is superior to the traditional acoustic guitars in terms of volume and mechanical performance, so that a service life of the guitar of the application can be increased by 2 to 3 times compared with traditional acoustic guitars and durable.

## Claims

### Claim 1

A guitar comprising:
fibers of lengths between 0.2 millimeters to 3 millimeters; and
polymer base materials.

### Claim 2 (depends on 1)

The guitar of claim 1, wherein the fibers are at least one of glass fibers, wood fibers and carbon fibers; and the and polymer base materials are at least one of acrylonitrile-butadiene-styrene copolymer, acrylate-styrene-acrylonitrile copolymer, and polycarbonate.

### Claim 3 (depends on 1)

The guitar of claim 1, the guitar comprising:
a guitar body;
a headstock board;
a soundboard;
a fretboard; and
a guitar bridge, wherein each of the guitar body, the headstock board, the soundboard, the fretboard, and the guitar bridge is a continuous and single structure.

### Claim 4 (depends on 3)

The guitar of claim 3, wherein the guitar body comprises a headstock, a neck, a bottom deck, and body sides, the a headstock, the neck, the bottom deck, and the body sides are integrally formed the guitar body; and a bucket body is defined by the bottom deck and the body sides.

### Claim 5 (depends on 4)

The guitar of claim 4, wherein the soundboard is connected to the bucket body of the guitar body; the headstock board is formed on the headstock; the fretboard is formed on the neck of the guitar body; and the guitar bridge is installed on the soundboard.

### Claim 6

A manufacturing method for a guitar, comprising:
mixing raw materials by stirring, granulating the mixed raw materials, and drying the granulated raw materials at a temperature ranging from 60° C. to 80° C.; wherein the raw materials comprise fibers having lengths between 0.2 millimeters to 3 millimeters;
injecting the dried and granulated raw materials into each of a guitar body mold, a headstock board mold, a soundboard mold, a fretboard mold, and a guitar bridge mold to form a guitar body, a headstock board, a soundboard, a fretboard, and a guitar bridge, respectively; and
assembling, sanding, spraying, and installing the guitar body, the headstock board, the soundboard, the fretboard, and the guitar bridge to form a guitar.

### Claim 7 (depends on 6)

The manufacturing method of claim 6, wherein, the fibers are at least one of glass fibers, wood fibers and carbon fibers.

### Claim 8 (depends on 6)

The manufacturing method of claim 6, wherein a method for injecting the dried and granulated raw materials comprises:
melting the raw materials at a temperature ranging from 190° C. to 230° C. to form barrel materials;
maintaining the barrel materials at a temperature ranging from 180° C. to 230° C. for a preset period of time; and
injecting the barrel materials into the guitar body mold, the headstock board mold, the soundboard mold, the fretboard mold, and the guitar bridge mold at a temperature ranging from 60° C. to 120° C.

### Claim 9 (depends on 8)

The manufacturing method of claim 8, wherein maintaining the barrel materials a temperature ranging from 180° C. to 230° C. for a preset period of time further comprising:
maintaining the barrel materials a temperature ranging from 180° C. to 200° C.;
maintaining the barrel materials a temperature ranging from 190° C. to 220° C.; and
maintaining the barrel materials a temperature ranging from 200° C. to 230° C.

### Claim 10 (depends on 6)

The manufacturing method of claim 6, wherein a method of injecting the dried and granulated raw materials further comprising:
controlling an injection pressure between 50 MPa to 180 MPa, and
controlling a molding time between 90 seconds to 180 seconds.

### Claim 11 (depends on 6)

The manufacturing method of claim 6, wherein before mixing the raw materials, the method further comprising:
pre-drying the raw materials in a temperature between 60° C. to 80° C. for 3 hours to 5 hours.

### Claim 12 (depends on 6)

The manufacturing method of claim 6, wherein a method of assembling the guitar body, the headstock board, the soundboard, the fretboard, and the guitar bridge comprises:
connecting the soundboard to the guitar body;
gluing the headstock board and the fretboard on the guitar body after the soundboard is connected to the guitar body; and
installing the guitar bridge on the soundboard.

### Claim 13 (depends on 12)

The manufacturing method of claim 12, wherein the guitar body comprising a headstock, a neck, a bottom deck, and body sides, and a bucket body is defined by the bottom deck and the body sides.

### Claim 14 (depends on 13)

The manufacturing method of claim 13, further comprising:
connecting the soundboard to the bucket body of the guitar body;
forming the headstock board on the headstock;
forming the fretboard on the neck of the guitar body; and
installing the guitar bridge is installed on the soundboard.

### Claim 15 (depends on 6)

The manufacturing method of claim 6, wherein a process for sanding and spraying comprises:
sanding surfaces of the assembled guitar with a sander,
filling gaps between the guitar body, the headstock board, the soundboard, the fretboard, and the guitar bridge with a filler material; and
painting the surface of the guitar by spray painting.

### Claim 16 (depends on 6)

The manufacturing method of claim 6, before injecting, further comprising:
keeping the guitar body mold, the headstock board mold, the soundboard mold, the fretboard mold, and the guitar bridge mold warm.