# US 2020/0165729 A1 · Thermal decomposition metallization process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0165729 A1
- Document ID: US20200165729A1
- Status: Published application
- Kind: A1
- Application number: 16/697,731
- Filed: 2019-11-27
- Published: 2020-05-28
- Earliest claimed: 2018-11-27
- Assignees: Glenair, Inc.
- Inventors: Jar-Wha Lee; Zachary Douglas Adams; Mark Andrew Maltese
- Web page: https://patentgrep.com/patent/US20200165729A1

## CPC

- C23C 18/08: characterised by the deposition of metallic material
- B05D 3/101: {Pretreatment of polymeric substrate}
- C23C 18/04: Pretreatment of the material to be coated (C23C18/06 takes precedence)
- C23C 18/10: Deposition of aluminium only
- B05D 2201/02: Polymeric substrate
- B05D 2350/65: metal layer
- B05D 2401/10: Organic solvent (B05D2401/21 takes precedence)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)

## Abstract

A method for forming a conductive metal-polymer composite coated polymer includes providing a polymer substrate and immersing the polymer substrate in a metal solution. The method further includes decomposing the metal solution in a thermally controlled environment and reducing the metal solution to metal such that the metal is deposited on a surface of the polymer substrate. After reducing the metal solution, the method includes treating the surface with a polymer coating to form the metal-polymer composite coated polymer.

## Claims

### Claim 1

A method for forming a conductive metal-polymer composite coated polymer, the method comprising:
providing a polymer substrate;
immersing the polymer substrate in a metal solution;
decomposing the metal solution in a thermally controlled environment;
reducing the metal solution to metal such that the metal is deposited on a surface of the polymer substrate; and
treating the surface with a polymer coating after reducing the metal solution to form the metal-polymer composite coated polymer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the polymer substrate is made of a cellulose-based polymer or a synthetically derived polymer.

### Claim 3 (depends on 2)

The method of claim 2, wherein the cellulose-based polymer is selected from the group consisting of viscose rayon, extra-long staple cotton, lyocell, mercerized cotton, modal, and combinations thereof, and the synthetically derived polymer is selected from the group consisting of porous polytetrafluoroethylene, expanded polytetrafluoroethylene, polyetheretherketone, nylon 6, polyimide, liquid crystal polymer, nylon 6,6, para-aramid, meta-aramid, and combinations thereof.

### Claim 4 (depends on 1)

The method of claim 1, wherein the polymer substrate is made of polyetheretherketone.

### Claim 5 (depends on 1)

The method of claim 1, wherein the metal solution is selected from the group consisting of organic or inorganic salts of copper, silver, aluminum, gold, iron, nickel, and combinations thereof.

### Claim 6 (depends on 1)

The method of claim 1, wherein the metal solution comprises an organometallic silver compound in an organic solvent.

### Claim 7 (depends on 6)

The method of claim 6, wherein the organometallic silver compound is selected from the group consisting of silver acetate, silver octanoate, silver nonanoate, silver neodecanoate, silver undecanoate, silver dodecanoate, silver nitrate, diamminesilver(I), silver(I) hexafluoropentanedionate-cyclooctadiene, silver 2-ethylhexylcarbamate, silver phenolate, and combinations thereof.

### Claim 8 (depends on 1)

The method of claim 1, wherein the metal solution comprises an organic solvent selected from the group consisting of xylene, acetone, toluene, benzene, n-methyl pyrrolidone, ethanol, water, and combinations thereof.

### Claim 9 (depends on 1)

The method of claim 1, wherein the metal solution comprises an organometallic silver compound in toluene.

### Claim 10 (depends on 1)

The method of claim 1, wherein the metal solution comprises an additive selected from the group consisting of ethyl cellulose, graphene nano-platelets, polystyrene-block-poly(ethylene-ran-butylene)-block-polystyrene-graft maleic anhydride, poly(ethylene-co-ethyl acrylate), ethylene-acrylic acid, hexadecyltrimethoxysilane, triethoxy(vinyl)silane, metallic nanoparticles, and combinations thereof.

### Claim 11 (depends on 1)

The method of claim 1, wherein the polymer coating is selected from a group consisting of ethyl cellulose, graphene nano-platelets, polystyrene-block-poly(ethylene-ran-butylene)-block-polystyrene-graft maleic anhydride, poly(ethylene-co-ethyl acrylate), ethylene-acrylic acid, hexadecyltrimethoxysilane, triethoxy(vinyl)silane, low density polyethylene, polyethylene terephthalate, poly(vinyl butryal-co-vinyl alcohol-co-vinyl acetate), poly vinyl butyral, polystyrene-block-polybutadiene-block-polystyrene, polyurethane, and combinations thereof

### Claim 12 (depends on 1)

The method of claim 1, further comprising, prior to immersing the polymer substrate in a metal solution, modifying the surface of the polymer substrate with a pretreatment surface modification solution.

### Claim 13 (depends on 12)

The method of claim 12, wherein pretreatment surface modification solution is selected from a group consisting of sulfuric acid, hydrochloric acid, hydrofluoric acid, nitric acid, phosphoric acid, perchloric acid, lithium hydroxide, sodium hydroxide, potassium hydroxide, rubidium hydroxide, cesium hydroxide, calcium hydroxide, and combinations thereof.

### Claim 14 (depends on 1)

The method of claim 1, wherein decomposing the metal solution comprises a continuous process.

### Claim 15 (depends on 14)

The method of claim 14, wherein the polymer substrate is in contact with the metal solution for about 3 to about 12 seconds and is in the thermally controlled environment for about 40 to about 60 seconds.

### Claim 16 (depends on 14)

The method of claim 14, wherein the polymer substrate is in contact with the metal solution for about 45 to about 55 seconds and is in the thermally controlled environment for about 160 to about 180 seconds.

### Claim 17 (depends on 1)

The method of claim 1, further comprising immersing the polymer substrate in the metal solution, decomposing the metal solution in the thermally controlled environment, and reducing the metal solution to metal such that the metal is deposited on the surface of the polymer substrate more than once before treating the surface with the polymer coating.

### Claim 18 (depends on 17)

The method of claim 17, wherein an average temperature in the thermally controlled environment is lower during a first decomposing step than in a subsequent decomposing step.

### Claim 19 (depends on 1)

The method of claim 1, wherein an average temperature in the thermally controlled environment is in a range of about 90 to about 300° C.

### Claim 20 (depends on 1)

The method of claim 1, wherein decomposing the metal solution in the thermally controlled environment includes maintaining conductive contact between a heating element and the polymer substrate.