# US 2020/0165133 A1 · Method for etching a phosphate source using acid

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0165133 A1
- Document ID: US20200165133A1
- Status: Published application
- Kind: A1
- Application number: 16/637,254
- Filed: 2018-08-10
- Published: 2020-05-28
- Earliest claimed: 2017-08-11
- Assignees: Prayon Technologies
- Applicants: Prayon Technologies
- Inventors: Alexandre Wavreille; Livio Lederer; Léon Ninane
- Web page: https://patentgrep.com/patent/US20200165133A1

## CPC

- C01B 25/22: Preparation by reacting phosphate-containing material with an acid, e.g. wet process
- C01B 25/324: {Preparation from a reaction solution obtained by acidifying with an acid other than orthophosphoric acid}
- C01B 25/01: Treating phosphate ores or other raw phosphate materials to obtain phosphorus or phosphorus compounds
- C01B 25/225: Dihydrate process
- C01B 25/226: Hemihydrate process
- C01B 25/322: {Preparation by neutralisation of orthophosphoric acid}
- C01B 25/327: {After-treatment}
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}

## Abstract

Process of acid attack with sulphuric acid of a phosphate source comprising calcium or not comprising calcium for a predetermined time period ranging from 20 to 180 minutes in the conditions wherein the molar ratio of sulphate from the sulphuric acid and possibly from the phosphate source to the calcium present in the phosphate source ranges from 0.6 to 0.8, and the content in P2O5 in the attack tank is of less than 6%.

## Claims

### Claim 1

Process of acid attack of a phosphate source including calcium for the production of a phosphate-based purified compound comprising the steps of:
a) an acid attack using sulphuric acid of said phosphate source, during a predetermined time period ranging from 20 to 180 minutes with the formation of a first suspension containing a first solid matter and a first liquid phase in which the first solid matter is in suspension, said first solid matter comprising at least calcium phosphate and impurities, said first liquid phase comprising phosphoric acid and dissolved monocalcium phosphate, said attack being conducted in input conditions wherein the molar ratio of the sulphate from the sulphuric acid and possibly from the phosphate source to the calcium present in the phosphate source ranges from 0.6 to 0.8 and the P2O5 content is of less than 6,
b) a first filtration of said first slurry with a separation of said first solid matter from said first liquid phase, and
c) a retrieval from said first liquid phase of a purified phosphate-based compound.

### Claim 2 (depends on 1)

Process according to claim 1, wherein said acid attack takes place in 1, 2 or more attack tanks.

### Claim 3 (depends on 1)

Process according to claim 1, wherein the predetermined time period is of less than 120 minutes.

### Claim 4 (depends on 2)

Process according to claims 2, wherein the P2O5 content in the liquid phase in the attack tank or tanks is less than 5%.

### Claim 5 (depends on 2)

Process according to claim 2, wherein said attack is performed at a temperature in the attack tank or tanks of 90° C. or less.

### Claim 6 (depends on 2)

Process according to claim 2, wherein the sulphuric acid is a diluted sulphuric acid, in particular before being added in the attack tank or tanks.

### Claim 7 (depends on 6)

Process according to claim 6, wherein said diluted sulphuric acid features a H2SO4 concentration of 13% or less by weight.

### Claim 8 (depends on 1)

Process according to claim 1, wherein the molar ratio of sulphate from the sulphuric acid and possibly from the phosphate source to the calcium present in the phosphate source ranges from 0.68 and 0.78.

### Claim 9 (depends on 1)

Process according to claim 1, further comprising the addition of a base to said first suspension, prior to filtration.

### Claim 10 (depends on 1)

Process according to claim 1, further comprising, before said step whereby said phosphate-based purified compound is retrieved from said first liquid phase, the addition of a base to said first liquid phase after filtration with the formation of a second suspension comprising a second solid matter in suspension in a second liquid phase and a filtration of said second suspension to separate said second solid matter in suspension from said second liquid phase, said second phosphate-based purified compound thereby being retrieved from said second liquid phase from the first liquid phase with a low content of said second solid matter.

### Claim 11 (depends on 1)

Process according to claim 1, wherein said first solid matter separated from said first liquid phase is recycled by introduction in the first suspension.

### Claim 12 (depends on 1)

Process according to claim 1, wherein said phosphate source containing calcium is chosen from the group made of traditional phosphate rocks, phosphate rocks with a low P2O5 content, of ashes, of sludge from wastewater processing plants, of bone ash, of pig manure, of chicken manure, of ash from the sludge of wastewater processing plants, of sludge from wastewater processing plants, and of any raw material featuring a phosphate content of less than 30% by weight of P2O5 with respect to the total weight of the raw material.

### Claim 13 (depends on 1)

Process according to claim 1, wherein said purified phosphate-based compound is a monocalcium phosphate MCP, a dicalcium phosphate DCP, more particularly a food-grade dicalcium phosphate DCP, a phosphoric acid, such as an acid derived directly from said first liquid phase or a phosphoric acid produced from said DCP.

### Claim 14 (depends on 10)

Process according to claim 10, wherein said second liquid phase is recycled by introduction in said attack tank or tanks.

### Claim 15

A dicalcium phosphate DCP composition comprising:
a) a CaO content of 40% or more by weight with respect to the total weight of dicalcium phosphate;
b) a chloride content of 0.020% or less by weight with respect to the total weight of dicalcium phosphate;
c) a fluoride content of 2% or less by weight with respect to the total weight of dicalcium phosphate; and
d) a Na2O content of 0.15% or less by weight with respect to the total weight of the dicalcium phosphate.