# US 2020/0156945 A1 · Novel carbon nanofiber having embedded carbon nanotubes, and method of manufacture

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0156945 A1
- Document ID: US20200156945A1
- Status: Published application
- Kind: A1
- Application number: 16/198,185
- Filed: 2018-11-21
- Published: 2020-05-21
- Earliest claimed: 2018-11-21
- Assignees: Cence Inc.
- Applicants: Cence Inc.
- Inventors: Sunshine HOLMBERG; Stoyan Atanassov RADKOV
- Web page: https://patentgrep.com/patent/US20200156945A1

## CPC

- C01B 32/166: in liquid phase
- D01F 9/22: from polyacrylonitriles
- C01B 32/05: Preparation or purification of carbon not covered by groups C01B32/15, C01B32/20, C01B32/25, C01B32/30
- C01B 32/174: Derivatisation; Solubilisation; Dispersion in solvents
- D01D 5/0038: {the fibre formed by solvent evaporation, i.e. dry electro-spinning}
- D01D 5/0092: {characterised by the electrical field, e.g. combined with a magnetic fields, using biased or alternating fields}
- D01F 1/10: Other agents for modifying properties
- D01F 8/18: from other substances
- D01F 9/12: Carbon filaments; Apparatus specially adapted for the manufacture thereof
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 40/00: Manufacture or treatment of nanostructures
- C01B 2202/22: Electronic properties
- C01B 2202/34: Length
- D01D 10/02: Heat treatment (heating for finishing D02J13/00)
- Y10T 428/30: Self-sustaining carbon mass or layer with impregnant or other layer
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method of producing Stress Activated Pyrolytic Carbon-Carbon NanoTube (SAPC-CNT) fibers is disclosed. The fibers are a composite consisting of a tubular core of pristine graphite planes that include carbon nanotubes (CNTs) surrounded by semi-graphitic carbon material that includes Stress Activated Pyrolytic Carbon (SAPC), the SAPC being characterized by wavy graphite planes ranging from 0.1 nm to 1 nm and oriented parallel to the axis of each fiber, the semi-graphitic carbon material also being characterized by an inclusion of 4 to 10 atomic percent of nitrogen heteroatoms, the nitrogen heteroatoms including an above 60% of quaternary and pyridinic nitrogen groups.

## Claims

### Claim 1

A method of producing one or more Stress Activated Pyrolytic Carbon-Carbon NanoTube (SAPC-CNT) fibers, the fibers being a composite consisting of a tubular core of pristine graphite planes that include carbon nanotubes (CNTs) surrounded by semi-graphitic carbon material that includes Stress Activated Pyrolytic Carbon (SAPC), the SAPC being characterized by wavy graphite planes ranging from 0.1 nm to 1 nm and oriented parallel to the axis of each fiber, the semi-graphitic carbon material also being characterized by an inclusion of 4 to 10 atomic percent of nitrogen heteroatoms, the nitrogen heteroatoms including an above 60% of quaternary and pyridinic nitrogen groups, the method for producing the SAPC-CNT fibers comprising:
preparing a Polyacrylonitrile (PAN) based precursor solution infused with CNTs to produce a PAN-CNT precursor;
providing the PAN-CNT precursor solution to a spinneret;
performing an electrospinning operation on the PAN-CNT precursor solution to create the one or more fibers, wherein the electrospinning operation includes passing the PAN-CNT-based precursor solution from the spinneret to a collector at a distance between 1 cm to 30 cm while providing an Alternating Current (AC) voltage between the spinneret and the collector, the AC voltage having a frequency ranging from 20 Hz to 100,000 Hz and either a Peak-to-Peak (P-P) voltage ranging from 100V to 30,000V or a Root-Mean-Square (RMS) voltage ranging from 100V to 30,000V;
performing a post-electrospinning operation on the one or more fibers, the post-electrospinning operation including a mechanical treatment and a chemical treatment;
performing a stabilizing treatment on the one or more fibers, the stabilizing treatment including heating the one or more fibers; and
after performing the post-electrospinning operation and stabilizing treatment, performing a pyrolysis treatment on the one or more fibers, the pyrolysis treatment including heating the one or more fibers in an inert atmosphere containing less than 1% oxygen.

### Claim 2 (depends on 1)

The method of producing one or more SAPC-CNT fibers of claim 1, wherein the electrospinning operation further includes providing a Direct Current (DC) voltage between the spinneret and the collector at a distance between 1 cm to 30 cm while passing the PAN-CNT-based precursor solution from the spinneret to the collector, the DC voltage ranging from about plus or minus 1,000 V to about plus or minus 30,000 V.

### Claim 3 (depends on 2)

The method of producing one or more SAPC-CNT fibers of claim 2, wherein the electrospinning operation is performed in an atmosphere containing vapor of the precursor solution solvent at a temperature ranging from 10° C. to 100° C. with a percent saturation larger than 10%.

### Claim 4 (depends on 1)

The method of producing one or more nanofibers of an SAPC-CNT-based of claim 1, wherein the PAN-CNT precursor solution includes 6% to 15% PAN by weight and 0.5-3% CNT by weight in a solvent.

### Claim 5 (depends on 4)

The method of producing one or more nanofibers of an SAPC-CNT-based of claim 4, wherein the solvent includes at least one of Dimethylsulfoxide (DMSO) and mixture of DMSO, DMF and/or with less than 5% water

### Claim 6 (depends on 4)

The method of producing one or more SAPC-CNT fibers of claim 4, wherein preparing the PAN-CNT-based precursor solution includes dissolving the PAN in the solvent via a convective mixing operation at a temperature ranging from 25° C. to 130° C. until the PAN is completely dissolved or for 1 hr to 1 week, wherein the PAN has a molecular weight ranging from 100,000 to 500,000.

### Claim 7 (depends on 1)

The method of producing one or more SAPC-CNT fibers of claim 1, wherein the mechanical treatment of the post-electrospinning operation includes one or both of hot-rolling and/or hot-drawing; and
the chemical treatment of the post-electrospinning operation includes dipping the one or more fibers in a 5% to 30% hydrogen peroxide solution followed by removing any remaining solvent and/or any remaining hydrogen peroxide from the one or more fibers.

### Claim 8 (depends on 7)

The method of producing one or more SAPC-CNT fibers of claim 7, wherein
the hot-rolling mechanically compresses the one or more fibers at temperature ranging from 50° C. to 300° C. and a stress ranging from 20 kPa to 2000 kPa; and the hot-drawing stretches the one or more fibers 5%-50% of an original length of the one or more fibers.

### Claim 9 (depends on 7)

The method of producing one or more SAPC-CNT fibers of claim 7, wherein the stabilizing treatment includes heating the one or more fibers at a temperature ranging from 200° C. to 300° C. while performing the mechanical treatment.

### Claim 10 (depends on 1)

The method of producing one or more SAPC-CNT fibers of claim 1, wherein the stabilizing treatment includes:
heating the one or more fibers at a temperature ranging from 200° C. to 400° C.

### Claim 11 (depends on 1)

The method of producing one or more nanofibers of an SAPC-CNT-based of claim 1, wherein the pyrolysis treatment includes:
performing first heating operation of the one or more fibers in the oxygen-free atmosphere at temperature between 200° C. to 400° C. for a time ranging from 1 hour to five hours;
after the first heating operation, performing a second heating operation of the one or more fibers in the oxygen-free atmosphere at temperature between 600° C. to 2000° C. for a time ranging from 1-5 hours; and
after the second heating operation, performing a cooling operation on the one or more fibers to room temperature;
wherein a temperature ramp rate for each operation of the pyrolysis treatment does not exceed 20° C./minute.

### Claim 12 (depends on 1)

The method of producing one or more SAPC-CNT fibers of claim 1, wherein the choice of polymer precursor (PAN) of the electrospinning operation and the pyrolysis temperature is sufficient to cause the percentage of quaternary and pyridinic nitrogen groups to exceed 25%.

### Claim 13 (depends on 12)

The method of producing or more SAPC-CNT fibers of claim 12, wherein the choice of polymer precursor (PAN) of the electrospinning operation and the pyrolysis temperature is sufficient to cause the percentage of quaternary and pyridinic nitrogen groups to exceed 90%.

### Claim 14 (depends on 12)

The method of producing one or more SAPC-CNT fibers of claim 12, wherein the percentage of PAN to CNTs in the PAN-CNT precursor is between 0.5% to 5% by weight.

### Claim 15

A carbon-based composition; comprising:
one or more Stress Activated Pyrolytic Carbon-Carbon NanoTube (SAPC-CNT) based fibers, wherein
the SAPC-CNT fibers are a composite consisting of a tubular core of pristine graphite planes that include carbon nanotubes (CNTs) surrounded by semi-graphitic carbon material that includes Stress Activated Pyrolytic Carbon (SAPC), the SAPC being characterized by wavy graphite planes ranging from 0.1 nm to 1 nm and oriented parallel to the axis of each fiber, the semi-graphitic carbon material also being characterized by an inclusion of 4 to 10 atomic percent of nitrogen heteroatoms, the nitrogen heteroatoms including an above 60% of quaternary and pyridinic nitrogen groups, the method for producing the SAPC-CNT fibers.

### Claim 16 (depends on 15)

The carbon-based composition of claim 15, wherein the percentage of quaternary and pyridinic nitrogen groups of the nitrogen heteroatoms exceeds 80%.

### Claim 17 (depends on 16)

The carbon-based composition of claim 16, wherein the percentage of quaternary and pyridinic nitrogen groups of the nitrogen heteroatoms exceeds 90%.

### Claim 18

A method of producing one or more Stress Activated Pyrolytic Carbon-Carbon NanoTube (SAPC-CNT) based fibers, the fibers being a composite consisting of a tubular core of pristine graphite planes that include carbon nanotubes (CNTs) surrounded by semi-graphitic carbon material that includes Stress Activated Pyrolytic Carbon (SAPC), the SAPC being characterized by wavy graphite planes ranging from 0.1 nm to 1 nm and oriented parallel to the axis of each fiber, the semi-graphitic carbon material also being characterized by an inclusion of 4 to 10 atomic percent of nitrogen heteroatoms, the nitrogen heteroatoms including an above 60% of quaternary and pyridinic nitrogen groups, the method for producing the SAPC-CNT fibers comprising:
preparing a Polyacrylonitrile (PAN) based precursor solution infused with CNTs to produce a PAN-CNT precursor;
providing the PAN-CNT precursor solution to a spinneret;
performing an electrospinning operation on the PAN-CNT-based precursor solution to create the one or more fibers, wherein the electrospinning operation includes passing the PAN-CNT-based precursor solution from the spinneret to a collector while providing an Alternating Current (AC) voltage between the spinneret and the collector, the AC voltage having a frequency ranging from 1 Hz to 100,000 Hz and either a Peak-to-Peak (P-P) voltage ranging from 100V to 30,000V or a Root-Mean-Square (RMS) voltage ranging from 100V to 30,000V;
performing a post-electrospinning operation on the one or more fibers, the post-electrospinning operation including a mechanical treatment and a chemical treatment;
performing a stabilizing treatment on the one or more fibers, the stabilizing treatment including heating the one or more fibers; and
after performing the post-electrospinning operation and stabilizing treatment, performing a pyrolysis treatment on the one or more fibers, the pyrolysis treatment including heating the one or more fibers in an oxygen-free atmosphere.

### Claim 19 (depends on 18)

The carbon-based composition of claim 18, wherein the percentage of quaternary and pyridinic nitrogen groups of the nitrogen heteroatoms exceeds 90%.

### Claim 20 (depends on 18)

The carbon-based composition of claim 18, wherein the percentage of PAN to CNTs in the PAN-CNT precursor is between 0.5% to 5% by weight.

### Claim at position 21 (depends on 2)

1. The method of producing one or more SAPC-CNT fibers of claim 2, wherein the electrospinning operation is performed in an ambient atmosphere at a temperature ranging from 10° C. to 100° C. with minimum humidity 45%.