# US 2020/0148947 A1 · Nitride phosphor and method for producing nitride phosphor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0148947 A1
- Document ID: US20200148947A1
- Status: Published application
- Kind: A1
- Application number: 16/743,100
- Filed: 2020-01-15
- Published: 2020-05-14
- Earliest claimed: 2017-07-19
- Assignees: Mitsubishi Chemical Corporation
- Applicants: Mitsubishi Chemical Corporation
- Inventors: Ryo KOIZUMI; Yuhei INATA; Saiko KIYOHARA; Masahito ISAKA; Naoyuki KOMURO; Kohei MATSUDA
- Web page: https://patentgrep.com/patent/US20200148947A1

## CPC

- C09K 11/0883: {Arsenides; Nitrides; Phosphides}
- C01B 21/097: containing phosphorus atoms
- C09K 11/08: containing inorganic luminescent materials
- C09K 11/77746: {Aluminium Nitrides or Aluminium Oxynitrides}
- C09K 11/77747: {Silicon Nitrides or Silicon Oxynitrides}
- C09K 11/77748: {Silicon Aluminium Nitrides or Silicon Aluminium Oxynitrides}
- C09K 11/77926: {Aluminium Nitrides or Aluminium Oxynitrides}
- C09K 11/77927: {Silicon Nitrides or Silicon Oxynitrides}
- C09K 11/77928: {Silicon Aluminium Nitrides or Silicon Aluminium Oxynitrides}
- H10H 20/851: Wavelength conversion means
- H10H 20/8512: {Wavelength conversion materials}
- Y02B 20/00: Energy efficient lighting technologies, e.g. halogen lamps or gas discharge lamps
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- Y02B: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO BUILDINGS, e.g. HOUSING, HOUSE APPLIANCES OR RELATED END-USER APPLICATIONS

## Abstract

Provided is a nitride phosphor having two or more maximum absorption points in a range of 3,200 to 3,300 cm−1 in an infrared absorption (FT-IR) spectrum. The nitride phosphor of the present invention has excellent emission characteristics and is highly reliable when used in devices.

## Claims

### Claim 1

A nitride phosphor having two or more maximum absorption points in a range of 3,200 to 3,300 cm−1 in an infrared absorption (FT-IR) spectrum.

### Claim 2 (depends on 1)

The nitride phosphor according to claim 1, having a maximum absorption point in two or more ranges of 3,220 to 3,250 cm−1, 3,255 to 3,275 cm−1, and 3,280 to 3,300 cm−1.

### Claim 3 (depends on 1)

The nitride phosphor according to claim 1, comprising a crystal phase that has a chemical composition represented by the following Formula (1):
M1xM2yM3z:M4 (1)
wherein
M1 represents at least one element selected from the group consisting of Y, La, Gd and Lu;
M2 represents at least one element selected from the group consisting of Ge, Si, Hf, Zr, Al, Ga and Ti;
M3 comprises N as an essential element and represents at least one element selected from the group consisting of N, O, F and Cl;
M4 represents at least one activation element selected from the group consisting of Eu, Ce, Pr, Cr, Nd, Sm, Tb, Dy, Ho, Er, Tm, Yb and Mn;
x satisfies 2.0≤x≤4.0;
y satisfies 5.0≤y≤7.0; and
z satisfies 10.0≤z≤12.0.

### Claim 4 (depends on 3)

The nitride phosphor according to claim 3, wherein in Formula (1), M1 is at least one element selected from the group consisting of Y, La and Gd, and M2 comprises Si as an essential element.

### Claim 5 (depends on 3)

The nitride phosphor according to claim 3, wherein in Formula (1), x satisfies 2.7≤x≤3.3, and y satisfies 5.4≤y≤6.6.

### Claim 6 (depends on 1)

The nitride phosphor according to claim 1, having a maximum absorption point in a range of 3,720 to 3,760 cm−1 in the infrared absorption (FT-IR) spectrum.

### Claim 7

A nitride phosphor comprising a crystal phase that has a chemical composition represented by the following Formula (2),
wherein when the value of a difference between a minimum ionic strength and a maximum ionic strength in a range of 200 to 400° C. in a detection chart for a molecular weight (m/z) of 44 measured by TPD-MS analysis is defined as 1, the value of a difference between a minimum ionic strength and a maximum ionic strength in a range of 500 to 650° C. is 0.5 or larger:
MpSiqNr:Z (2)
wherein
M represents a rare-earth element, excluding an element used as an activator;
Z represents the activator;
p satisfies 2.7≤p≤3.3;
q satisfies 5.4≤q≤6.6; and
r satisfies 10≤r≤12.

### Claim 8 (depends on 7)

The nitride phosphor according to claim 7, wherein the value of the difference between the minimum ionic strength and the maximum ionic strength in the range of 500 to 650° C. is 2.0 or larger.

### Claim 9 (depends on 7)

The nitride phosphor according to claim 7, wherein in Formula (2), M is at least one element selected from the group consisting of La, Y, Gd and Lu.

### Claim 10 (depends on 3)

The nitride phosphor according to claim 3, wherein the crystal phase that has the chemical composition represented by Formula (1) or (2) is a tetragonal crystal.

### Claim 11 (depends on 7)

The nitride phosphor according to claim 7, wherein the crystal phase that has the chemical composition represented by Formula (1) or (2) is a tetragonal crystal.

### Claim 12

A method of producing a nitride phosphor comprising a crystal phase that has a chemical composition represented by the following Formula (2), wherein the method comprises:
the step of preparing a raw material mixture of the nitride phosphor comprising the crystal phase that has the chemical composition represented by the following Formula (2);
the firing step of firing the raw material mixture; and
the heating step of heating a fired product obtained by the firing step in an atmosphere having an oxygen content of 10,000 ppm or less,
wherein the crystal phase is a tetragonal crystal or an orthorhombic crystal:
MpSiqNr:Z (2)
wherein
M represents a rare-earth element, excluding an element used as an activator;
Z represents the activator;
p satisfies 2.7≤p≤3.3;
q satisfies 5.4≤q≤6.6; and
r satisfies 10≤r≤12.

### Claim 13 (depends on 12)

The method according to claim 12, wherein in the heating step, the fired product is heated in an atmosphere having a water content of 10.0% by volume or less.

### Claim 14 (depends on 12)

The method according to claim 12, wherein in the heating step, the atmosphere having an oxygen content of 10,000 ppm or less is realized by supplying a nitrogen gas and/or a noble gas into a heating furnace where heating is performed.

### Claim 15 (depends on 12)

The method according to claim 12, wherein in the heating step, the fired product is heated at 500° C. to 1,300° C.

### Claim 16 (depends on 1)

A light-emitting device comprising:
a semiconductor light-emitting element that emits a UV light or a visible light; and
the nitride phosphor according to claim 1.

### Claim 17 (depends on 16)

A lighting apparatus comprising the light-emitting device according to claim 16 as a light source.

### Claim 18 (depends on 16)

An image display device comprising the light-emitting device according to claim 16 as a light source.

### Claim 19 (depends on 7)

A light-emitting device comprising:
a semiconductor light-emitting element that emits a UV light or a visible light; and
the nitride phosphor according to claim 7.

### Claim 20 (depends on 19)

A lighting apparatus comprising the light-emitting device according to claim 19 as a light source.

### Claim 21 (depends on 19)

An image display device comprising the light-emitting device according to claim 19 as a light source.