# US 2020/0140277 A1 · Method for manufacturing metal phosphate nanoparticles by sub-and supercritical solvothermal synthesis and nanoparticles obtained by this method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0140277 A1
- Document ID: US20200140277A1
- Status: Published application
- Kind: A1
- Application number: 16/625,180
- Filed: 2018-06-26
- Published: 2020-05-07
- Earliest claimed: 2017-06-26
- Assignees: Centre National De La Recherche Scientifique; Universite De Bordeaux; University of Aarhus
- Applicants: Centre National De La Recherche Scientifique; Université De Bordeaux; University of Aarhus
- Inventors: Cyril AYMONIER; Bo BRUMMERSTEDT IVERSEN; Gilles PHILIPPOT; Nils LAU NYBORG BROGE
- Web page: https://patentgrep.com/patent/US20200140277A1

## CPC

- C01B 25/375: {of iron}
- C01B 25/37: Phosphates of heavy metals
- C01B 25/372: {of titanium, vanadium, zirconium, niobium, hafnium or tantalum}
- C01B 25/377: {of manganese}
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 40/00: Manufacture or treatment of nanostructures
- C01P 2004/64: Nanometer sized, i.e. from 1-100 nanometer
- Y02P 20/54: using solvents, e.g. supercritical solvents or ionic liquids
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for manufacturing metal phosphate hydrate nanoparticles wherein metal reactants are selected from metal precursors of transition metals,phosphate precursors are selected from: Trisodium phosphate Na3PO4, disodium phosphate Na2HPO4, phosphoric acid H3PO4 and hypophosphoric acid H4P2O6, wherein said method comprises the following step of a reaction medium comprising at least a metal reactant, a phosphate precursor and a solvent, is submitted to a solvothermal treatment at a pressure superior to 50 MPa, and at a temperature of from 100 to 350° C.

## Claims

### Claim 1

A method for manufacturing transition metal phosphate hydrate nanoparticles comprising:
selecting metal reactants from transition metals,
selecting phosphate precursors from at least one of: Trisodium phosphate Na3PO4, disodium phosphate Na2HPO4, phosphoric acid H3PO4 and hypophosphoric acid H4P2O6,
submitting a reaction medium comprising at least: the metal reactant, the phosphate precursor and a solvent, to a solvothermal treatment at a pressure greater than 5 MPa, and at a temperature of from 100 to 350° C.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the method is a continuous flow method.

### Claim 3 (depends on 1)

The method according to claim 1, wherein after the submitting step it comprises a step:
conditioning the reaction medium obtained at the end of the submitting step at a temperature below the temperature of the supercritical area of the solvent.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the solvothermal treatment is applied for a length of time less than or equal to 10 seconds.

### Claim 5 (depends on 1)

The method according to claim 1, wherein metal precursors are selected from salts, oxydes, hydroxydes of transition metals, preferably they are selected from salts and oxides of Zn and Fe.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the solvent is selected from water, an alcohol and mixtures of water with an alcohol.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the concentration of the metal precursor in the reaction medium is from 0.0001 mol/l to the solubility limit, in particular from 0.001 mol/l to 0.1 mol/l , more particularly from 0.01 mol/l to 0.1 mol/l.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the concentration of the phosphate precursor in the reaction medium is from 0.0001 mol/l to the solubility limit, in particular from 0.001 mol/l to 0.1 mol/l, more particularly from 0.01 mol/l to 0.1 mol/l.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the temperature of the reaction medium in step (i) is at least 150° C., preferably from 150 to 350° C., in particular from 200° C. to 300° C.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the pressure of the reaction medium in the submitting step is from 10 MPa to 28 MPa, in particular from 20 MPa to 27 MPa.

### Claim 11 (depends on 1)

The method according to claim 1, wherein it comprises a step of pre-heating a solution of the phosphate precursor before the submitting step, preferably the pre-heating temperature is at least 150° C., in particular from 150° C. to 400° C., more particularly from 200° C. to 350° C.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the reaction medium further comprises at least one ligand precursor.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the ligand precursor is an organic ligand comprising a phosphate acid group or a phosphonic acid group.

### Claim 14 (depends on 12)

The method according to claim 12, wherein the molar ratio of ligand precursor/metal precursor in the reaction medium is from 0.05 to 10, in particular from 0.1 to 1, more particularly from 0.15 to 0.2.

### Claim 15 (depends on 12)

Nanoparticles capable of being obtained by a method according to claim 12, wherein they consist of metal phosphate hydrate nanoparticles the surface of which is grafted by at least an organic ligand.