Back to results
US 2020/0138241 A1Published application
Process for manufacturing frying pan
AssigneeNingbo Huige Outdoor Products Co., Ltd.
InventorSongcun ZHENG
Life of this patent
Estimating the term…
Abstract
The invention discloses a process for manufacturing a frying pan, which is characterized by comprising the steps of material selecting, cutting, machining and forming, welding, grinding, sanding, cleaning, baking, preparing of a ceramic paint, spraying of a ceramic paint, curing, cooling and the like. The invention has the advantage of simple process and can be used to obtain a finished frying pan with better quality.
Claims10
A process for manufacturing a frying pan, comprising the following steps of:
- (1) material selecting:
- selecting a cold-rolled plate/hot-rolled plate as a basic plate;
- (2) cutting:
- cutting the basic plate into a compliant plate according to a specification required by frying pan machining;
- (3) machining and forming:
- die-cutting and bending the plate to obtain a pre-formed frying pan;
- (4) welding:
- welding side seams present at bends of the pre-formed frying pan, and meanwhile welding a fixed base to the bottom of the pre-formed frying pan;
- (5) grinding:
- grinding burrs, welding bumps and welding marks on the frying pan obtained from the previous step, and shaping uneven parts of the frying pan to keep the frying pan even;
- (6) sanding:
- sanding and blasting six faces of the frying pan ground in Step (5) with brown fused alumina sand;
- (7) cleaning:
- cleaning the sanded frying pan;
- (8) baking:
- baking the frying pan cleaned to remove moisture on the surface of the frying pan;
- (9) preparing a ceramic paint:
- preparing a ceramic paint consisting of a primer and a finish paint, for painting the frying pan;
- (10) spraying of the ceramic paint:
- preheating the frying pan obtained from Step (8) to 70° C., monitoring a surface temperature of the frying pan by using an infrared thermometer, and spraying the frying pan with the primer and the finish paint prepared in Step (9) when detecting that the surface temperature of the frying pan reaches 30-40° C., wherein spraying a layer of the primer at first, leveling after the spraying of the primer, standing for 2-3 minutes, and then spraying the finish paint directly;
- (11) curing:
- after the painted surface of the frying pan is dried, baking and curing the painted surface;
- and
- (12) cooling:
- naturally cooling the frying pan cured to obtain a finished frying pan.
22 more elements
Dependencies are inferred from the claim text.