# US 2020/0123637 A1 · Thermoelectric alloy, method for producing the same and thermoelectric alloy composite

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0123637 A1
- Document ID: US20200123637A1
- Status: Published application
- Kind: A1
- Application number: 16/234,535
- Filed: 2018-12-27
- Published: 2020-04-23
- Earliest claimed: 2018-10-18
- Assignees: National Sun Yat-Sen University
- Applicants: National Sun Yat-Sen University
- Inventors: Hsin-Jay WU; Wan-Ting YEN; Pai-Chun WEI; Yi-Fen TSAI
- Web page: https://patentgrep.com/patent/US20200123637A1

## CPC

- C22C 28/00: Alloys based on a metal not provided for in groups C22C5/00 - C22C27/00
- C23C 8/20: Carburising
- C22C 1/02: by melting {(C22C1/1036 takes precedence)}
- C22C 12/00: Alloys based on antimony or bismuth
- C23C 8/34: more than one element being applied in more than one step
- C23C 8/44: Carburising
- C23C 8/58: more than one element being applied in more than one step
- C23C 8/64: Carburising
- C23C 8/78: more than one element being applied in more than one step
- H10N 10/01: Manufacture or treatment
- H10N 10/855: comprising compounds containing boron, carbon, oxygen or nitrogen
- H10N 10/8556: {comprising compounds containing germanium or silicon}
- C30B 29/52: Alloys
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

The present invention relates to a thermoelectric alloy and a method for producing the same. A starting material is firstly provided, and an oxidation process is performed to the starting material to obtain an oxidized material composition. Then, the oxidized material composition and a carburizing agent are added into a quartz tube, and a sealing process is performed to the quartz tube. And then, the sealed quartz tube is subjected to a carburization process, thereby obtaining the thermoelectric alloy with excellent thermoelectric figure-of-merit.

## Claims

### Claim 1

A method for producing a thermoelectric alloy, comprising:
providing a starting material, wherein the starting material includes germanium (Ge), tellurium (Te), bismuth (Bi), zinc (Zn), antimony (Sb), selenium (Se), copper (Cu), indium (In), gallium (Ga), silver (Ag), cobalt (Co), iron (Fe) and/or lead (Pb);
performing an oxidation process to the starting material for producing an oxidized material composition, wherein based on the oxidized material composition as 100 atom percent (at %), an oxygen content of the oxidized material composition is 0.001 at % to 10 at %;
adding the oxidized material composition and a carburizing agent into a quartz tube, and performing a sealing process, so as to form a sealed quartz tube; and
performing a carburization process to the sealed quartz tube, thereby producing the thermoelectric alloy.

### Claim 2 (depends on 1)

The method for producing the thermoelectric alloy of claim 1, wherein the carburizing agent is in a form of a solid, a liquid, a gas and/or a plasma.

### Claim 3 (depends on 1)

The method for producing the thermoelectric alloy of claim 1, wherein the operation of adding the oxidized material composition and the carburizing agent into the quartz tube comprises:
adding the carburizing agent into the quartz tube and performing a carbon coating process, so as to form a carbon film on an inner surface of the quartz tube; and
adding the oxidized material composition into the quartz tube having the carbon film.

### Claim 4 (depends on 1)

The method for producing the thermoelectric alloy of claim 1, wherein a vacuum degree of the sealed quartz tube is not larger than 0.03 mbar.

### Claim 5 (depends on 1)

The method for producing the thermoelectric alloy of claim 1, wherein the carburization process includes a heating step, and the heating step is heated from 200° C. to a melting point of the starting material.

### Claim 6 (depends on 5)

The method for producing the thermoelectric alloy of claim 5, wherein a cooling rate of the carburization process is 2° C./hour to 10° C./hour.

### Claim 7 (depends on 1)

The method for producing the thermoelectric alloy of claim 1, after performing the carburization process, further comprising:
performing a crystal growth process to the thermoelectric alloy.

### Claim 8 (depends on 1)

A thermoelectric alloy, produced by a method of claim 1, wherein based on the thermoelectric alloy as 100 wt %, a carbon content of the thermoelectric alloy is 0.005 wt % to 0.05 wt %.

### Claim 9 (depends on 8)

The thermoelectric alloy of claim 8, wherein the thermoelectric alloy includes P-type thermoelectric alloy and N-type thermoelectric alloy.

### Claim 10 (depends on 8)

A thermoelectric alloy composite, comprising:
a thermoelectric alloy of claim 8, wherein based on an amount of the thermoelectric alloy composite as 100 wt %, an amount of the thermoelectric alloy is at least 10 wt %.