# US 2020/0123284 A1 · High purity allylamine (co)polymer and method for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0123284 A1
- Document ID: US20200123284A1
- Status: Published application
- Kind: A1
- Application number: 16/625,666
- Filed: 2018-06-19
- Published: 2020-04-23
- Earliest claimed: 2017-07-05
- Assignees: Nitto Boseki Co., Ltd.
- Applicants: Nitto Boseki Co., Ltd.
- Inventors: Nobuyuki YAMADA; Masaru BUNYA
- Web page: https://patentgrep.com/patent/US20200123284A1

## CPC

- C08F 26/02: by a single or double bond to nitrogen
- C08F 6/02: Neutralisation of the polymerisation mass, e.g. killing the catalyst (short-stopping C08F2/42 ){also removal of catalyst residues}
- C08F 6/06: Treatment of polymer solutions {(C08F6/001, C08F6/006, C08F6/008, C08F6/02, C08F6/04 take precedence)}
- C08F 126/02: by a single or double bond to nitrogen
- C09D 11/106: containing macromolecular compounds obtained by reactions only involving carbon-to-carbon unsaturated bonds
- C09D 139/02: Homopolymers or copolymers of vinylamine
- C09J 139/02: Homopolymers or copolymers of vinylamine
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)

## Abstract

Even when used in applications such as electronic materials, display materials, and inks, in which required standards in terms of coloring prevention, long term stability, low impurity content, and the like, are extremely high, the present invention can meet such required standards. The present invention addresses the problem of providing an allylamine (co)polymer which overcomes the limitations of the prior art, undergoes little coloring, contains little impurities and exhibits excellent long term stability; and a method for producing the same. This problem can be solved by an allylamine (co)polymer which has constituent units derived from allylamine and contains sulfuric acid groups in the structure thereof, in which the proportion of the sulfuric acid groups with respect to the total mass of the allylamine (co)polymer is 20,000 ppm by mass or less.

## Claims

### Claim 1

An allylamine (co)polymer which has constituent units derived from allylamine and contains sulfuric acid groups in the structure thereof, in which the proportion of the sulfuric acid groups with respect to the total mass of the allylamine (co)polymer is 20,000 ppm by mass or less.

### Claim 2 (depends on 1)

The allylamine (co)polymer according to claim 1, wherein the proportion of the sulfuric acid groups with respect to the total mass of the allylamine (co)polymer is 15,000 ppm by mass or less.

### Claim 3 (depends on 1)

The allylamine (co)polymer according to claim 1, wherein the weight average molecular weight is 250 to 2500.

### Claim 4 (depends on 1)

The allylamine (co)polymer according to claim 1, wherein the initial absorbance A510 at the wavelength of 510 nm, which is measured for an aqueous solution of the allylamine (co)polymer prepared to have the concentration of 10 mass % and the pH of 11, is 0.5 or less, and the ratio A′510/A510 between the absorbance A′510 at the wavelength of 510 nm after the aqueous solution is held at 70° C. for 2 days and the initial absorbance A510 is 3 or less.

### Claim 5 (depends on 1)

The allylamine (co)polymer according to claim 1, wherein the proportion of the constituent units derived from the allylamine in all of the constituent units is 10 mol % or more.

### Claim 6

A method for producing an allylamine (co)polymer, comprising:
a) obtaining an allylamine (co)polymer by polymetizing an allylamine monomer;
b) decomposing sulfuric acid groups in the obtained allylamine (co)polymer; and
c) removing a sulfur compound generated by the decomposition of the sulfuric acid groups.

### Claim 7 (depends on 6)

The method for producing an allylamine (co)polymer according to claim 6, wherein, in the step b), the amount of the sulfuric acid groups in the allylamine (co)polymer is reduced to 20,000 ppm by mass or less with respect to the total mass of the allylamine (co)polymer.

### Claim 8 (depends on 6)

The method for producing an allylamine (co)polymer according to claim 6, wherein, in the step b), an amount of the sulfuric acid groups in the allylamine (co)polytner is reduced to 15,000 ppm by mass or less with respect to the total mass of the allylamine (co)polymer.

### Claim 9 (depends on 6)

The method for producing allylamine (co)polymer according to claim 6, wherein, in the step b), the allylamine (co)polymer obtained in the step a) is heated at a temperature of 70° C. or higher for 12 hours or longer.

### Claim 10 (depends on 1)

A papermaking treatment agent, an ink, a paint, or an adhesive comprising the allylamine (co)polymer according to claim 1.

### Claim 11 (depends on 1)

An electrical electronic material or a display material comprising the allylamine (co)polymer according to claim 1.

### Claim 12 (depends on 1)

A light transmitting material comprising the allylamine (co)polymer according to claim 1.

### Claim 13 (depends on 2)

The allylamine (co)polymer according to claim 2, wherein the weight average molecular weight is 250 to 2500.

### Claim 14 (depends on 2)

The allylamine (co)polymer according to claim 2, wherein the initial absorbance A510 at the wavelength of 510 nm, which is measured for an aqueous solution of the allylamine (co)polymer prepared to have the concentration of 10 mass % and the pH of 11, is 0.5 or less, and the ratio A′510/A510 between the absorbance A′510 at the wavelength of 510 nm after the aqueous solution is held at 70° C. for 2 days and the initial absorbance A510 is 3 or less.

### Claim 15 (depends on 3)

The allylamine (co)polymer according to claim 3, wherein the initial absorbance A510 at the wavelength of 510 nm, which is measured for an aqueous solution of the allylamine (co)polymer prepared to have the concentration of 10 mass % and the pH of 11, is 0.5 or less, and the ratio A′510/A510 between the absorbance A′510 at the wavelength of 510 nm after the aqueous solution is held at 70° C. for 2 days and the initial absorbance A510 is 3 or less.

### Claim 16 (depends on 2)

The allylamine (co)polymer according to claim 2, wherein the proportion of the constituent units derived from the allylamine in all of the constituent units is 10 mol % or more.

### Claim 17 (depends on 3)

The allylamine (co)polymer according to claim 3, wherein the proportion of the constituent units derived from the allylamine in all of the constituent units is 10 mol % or more.

### Claim 18 (depends on 4)

The allylamine (co)polymer according to claim 4, wherein the proportion of the constituent units derived from the allylamine in all of the constituent units is 10 mol % or more.

### Claim 19 (depends on 7)

The method for producing allylamine (co)polymer according to claim 7, wherein, in the step b), the allylamine (co)polymer obtained in the step a) is heated at a temperature of 70° C. or higher for 12 hours or longer.

### Claim 20 (depends on 8)

The method for producing allylamine (co)polymer according to claim 8, wherein, in the step b), the allylamine (co)polymer obtained in the step a) is heated at a temperature of 70° C. or higher for 12 hours or longer.