# US 2020/0108523 A1 · Process for the Production of OSB Wood-Based Boards with Reduced Emission of Volatile Organic Compounds (VOCs)

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0108523 A1
- Document ID: US20200108523A1
- Status: Published application
- Kind: A1
- Application number: 16/497,535
- Filed: 2018-03-12
- Published: 2020-04-09
- Earliest claimed: 2017-04-25
- Assignees: SWISS KRONO Tec AG
- Applicants: SWISS KRONO Tec AG
- Inventors: Norbert Kalwa
- Web page: https://patentgrep.com/patent/US20200108523A1

## CPC

- B27K 1/02: Apparatus
- B27N 1/003: {for reducing formaldehyde gas emission}
- B27K 5/001: {Heating}
- B27K 5/007: {using pressure (B27K3/08 takes precedence)}
- B27L 1/00: Debarking or removing vestiges of branches from trees or logs (debarking by chemical treatment B27L3/00 {; peeling osier rods B27J3/00}); Machines therefor
- B27L 11/007: {Combined with manufacturing a workpiece}
- B27N 1/00: Pretreatment of moulding material
- B27N 3/143: {Orienting the particles or fibres}
- B27K 2200/10: Articles made of particles or fibres consisting of wood or other lignocellulosic material
- B27K 2240/10: Extraction of components naturally occurring in wood, cork, straw, cane or reed
- B27K: PROCESSES, APPARATUS OR SELECTION OF SUBSTANCES FOR IMPREGNATING, STAINING, DYEING, BLEACHING OF WOOD OR SIMILAR MATERIALS, OR TREATING OF WOOD OR SIMILAR MATERIALS WITH PERMEANT LIQUIDS, NOT OTHERWISE PROVIDED FOR (applying liquids or other fluent materials to surfaces in general B05; coating wood or similar material B44D); CHEMICAL OR PHYSICAL TREATMENT OF CORK, CANE, REED, STRAW OR SIMILAR MATERIALS
- B27N: MANUFACTURE BY DRY PROCESSES OF ARTICLES, WITH OR WITHOUT ORGANIC BINDING AGENTS, MADE FROM PARTICLES OR FIBRES CONSISTING OF WOOD OR OTHER LIGNOCELLULOSIC OR LIKE ORGANIC MATERIAL (containing cementitious material B28B; shaping of substances in a plastic state B29C; fibreboards made from fibrous suspensions D21J; drying F26B17/00)
- B27L: REMOVING BARK OR VESTIGES OF BRANCHES (forestry A01G); SPLITTING WOOD; MANUFACTURE OF VENEER, WOODEN STICKS, WOOD SHAVINGS, WOOD FIBRES OR WOOD POWDER

## Abstract

Disclosed is a process for the treatment of wood strands suitable for the manufacture of OSB boards, in which the wood strands are treated with steam without drying after extraction, the steam being passed over the wood strands at a temperature between 80° C. and 120° C. and a pressure between 0.5 bar and 2 bar. Also disclosed is a process for the production of OSB wood-based boards including the steps of a) producing wood strands from suitable wood logs; b) treating at least part of the wood strands with steam; c) drying the steam-treated wood strands; d) gluing the steam-treated and dried wood strands and gluing the non-steam-treated wood strands with at least one binder; e) scattering the glued wood strands onto a conveyor belt; and f) pressing the glued wood strands into an OSB wood-based board.

## Claims

### Claim at position 1

-20. (canceled)

### Claim 21

A process for the treatment of wood strands with steam to reduce the emission of volatile organic compounds from such wood strands, comprising:
treatment of the wood strands with steam for a period of 5 to 2 minutes after extraction without drying, the steam being passed over the wood strands at a temperature of between 80° C. and 120° C. and a pressure of 0.5 bar to 2 bar,
wherein the steam treated wood strands are used to produce oriented strand boards (OSB) with reduced emission of volatile organic compounds.

### Claim 22 (depends on 21)

The process according to claim 21, wherein the steam is passed over the wood strand at a temperature between 90° C. and 110° C. at a pressure between 0.7 bar and 1.5 bar.

### Claim 23 (depends on 21)

The process according to claim 21, wherein the wood strands are treated with steam for a period of 10 to 20 minutes.

### Claim 24 (depends on 21)

The process according to claim 21, wherein the steam treatment of the wood takes place in an atmosphere low in oxygen.

### Claim 25 (depends on 21)

The process according to claim 21, wherein the wood strands are continuously guided on an at least one transport device through a steam treatment device.

### Claim 26 (depends on 21)

The process according to claim 21, wherein water vapor is collected as a condensate after passing through the wood strands.

### Claim 27

A process for the production of oriented strand board (OSB) wood-based panels with reduced emission of volatile organic compounds (VOCs) comprising the steps of:
a) producing wood strands from suitable wood logs;
b) treating at least part of the wood strands with steam by a process comprising:
treatment of the wood strands with steam for a period of 5 to 20 minutes after extraction without drying, the steam being passed over the wood strands at a temperature of between 80° C. and 120° C. and a pressure of 0.5 bar to 2 bar,
wherein the steam treated wood strands are used to produce OSB boards with reduced emission of volatile organic compounds;
c) drying the steam-treated wood strands;
d) gluing the steam-treated and dried wood strands and optionally gluing the non-steam-treated wood s-trands with at least one binder;
e) spreading the glued wood strands on a conveyor belt; and
f) pressing the glued wood strands into an OSB wood-based panel.

### Claim 28 (depends on 27)

The process according to claim 27, wherein the steam-treated wood strands, or a mixture of steam-treated wood strands and non-steam-treated wood strands, are used as the middle layer and/or top layer of the OSB wood-based panel.

### Claim 29 (depends on 28)

The process according to claim 28, wherein the steam-treated and non-steam-treated wood strands are glued with a binder in an amount of 1.0 to 5.0% by weight, based on the total amount of the wood strands.

### Claim 30 (depends on 27)

The process according to claim 27, wherein the glued wood strands are pressed at temperatures between 200° C. and 250° C. to form an OSB wood-based panel.

### Claim 31 (depends on 27)

A system for the production of an oriented strand board (OSB) according to the process as in claim 27, comprising:
an at least one device for debarking suitable logs;
an at least one chipper for the chipping of the debarked logs into wood strands;
an at least one device for steam treatment of at least a part of the wood strands, wherein the device for steam treatment comprises at least one housing, at least one transport device running through the housing for transporting the wood strands through the housing, and at least one supply line for the steam provided above the transport device in the housing, wherein at least one spraying means for applying the steam to the wood strands located on the transport device is arranged along the supply line;
an at least one dryer for drying the steam-treated wood strands;
an at least one device for classifying and separating the steam-treated and non-steam-treated wood strands;
an at least one device for gluing wood strands;
an at least one device for spreading the glued wood strands on a conveyor belt; and
an at least one press for pressing the scattered wood strands into OSB boards.

### Claim 32 (depends on 31)

The system according to claim 31, wherein the at least one transport device in the steam treatment device comprises at least one transport belt with perforations.

### Claim 33 (depends on 31)

The system according to claim 31, wherein the at least one means for collecting the condensate is provided below the at least one transport device in the at least one housing of the steam treatment device.

### Claim 34 (depends on 21)

The process according to claim 21, wherein the steam is passed over the wood strand at a temperature of 100° C. at a pressure of 1 bar, i.e. at atmospheric pressure.

### Claim 35 (depends on 21)

The process according to claim 21, wherein the steam treatment of the wood strands takes place for 15 minutes.

### Claim 36 (depends on 28)

The process according to claim 28, wherein the steam-treated and non-steam-treated wood strands are glued with a binder in an amount of 2 to 4% by weight based on the total amount of the wood strands.

### Claim 37 (depends on 28)

The process according to claim 28, wherein the steam-treated and non-steam-treated wood strands are glued with a binder in an amount of 3% by weight, based on the total amount of the wood strands.

### Claim 38 (depends on 27)