# US 2020/0102479 A1 · Hard abrasive particle-free polishing of hard materials method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0102479 A1
- Document ID: US20200102479A1
- Status: Published application
- Kind: A1
- Application number: 16/702,680
- Filed: 2019-12-04
- Published: 2020-04-02
- Earliest claimed: 2017-07-10
- Assignees: Sinmat, Inc.; University of Florida Research Foundation, Inc.
- Applicants: Sinmat, Inc.; University of Florida Research Foundation, Inc.
- Inventors: RAJIV K. SINGH; ARUL ARJUNAN; DEEPIKA SINGH; CHAITANYA GINDE; PUNEET N. JAWALI
- Web page: https://patentgrep.com/patent/US20200102479A1

## CPC

- C09G 1/02: containing abrasives or grinding agents {(abrasives as such C09K3/14; polishing of semi-conductors H10P52/40)}
- B24B 37/00: Lapping machines or devices; Accessories (B24B3/00 takes precedence)
- B24B 37/044: {characterised by the composition of the lapping agent}
- C09G 1/04: Aqueous dispersions (C09G1/02 takes precedence)
- C09K 3/1409: {Abrasive particles per se (preparation of diamond C01B32/25)}
- H10P 52/402: {of semiconductor materials}
- H10P 52/403: {of conductive or resistive materials}
- H10P 90/129: {by polishing}
- C09G: POLISHING COMPOSITIONS (French polish C09F11/00); SKI WAXES
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of chemical mechanical polishing (CMP) includes providing a slurry solution including at least one per-compound permanganate oxidizer in a concentration between 0.01 M and 2 M, with a pH level from 1.5 to 5 or from 8 to 11, and at least one buffering agent. The buffering agent is different from this pure-compound permanganate oxidizer, and comprises a surfactant and/or an alkali metal ion. The slurry solution is exclusive of any added particles. The slurry solution is dispensed on a hard surface having a Vickers hardness >1,000 kg/mm2 and is pressed by a polishing pad with the slurry solution in between while rotating the polishing pad relative to the hard surface.

## Claims

### Claim 1

A method of chemical mechanical polishing (CMP) hard surfaces, comprising:
providing a slurry solution comprising:
an aqueous medium;
at least one per-compound permanganate oxidizer with a concentration between 0.01 M and 2 M;
a pH level from 1.5 to 5 or from 8 to 11;
at least one buffering agent different from the per-compound permanganate oxidizer, the buffering agent comprising at least one of a surfactant and an alkali metal ion;
the slurry solution being exclusive of any added particles,
dispensing the slurry solution on a hard surface having a Vickers hardness>1,000 kg/mm2, and
pressing with a polishing pad with the slurry solution on the hard surface in between while rotating the polishing pad relative to the hard surface.

### Claim 2 (depends on 1)

The method of claim 1, wherein the pH level is 1.5 to 5 and wherein the slurry solution includes in situ soft particles formed by a decomposition of the per-compound permanganate oxidizer to form MnO2 particles that have a Mohs hardness less than or equal to (≤) 3.

### Claim 3 (depends on 1)

The method of claim 1, wherein the hard surface comprises a carbide, a nitride, or a mixture thereof.

### Claim 4 (depends on 1)

The method of claim 1, wherein the slurry solution further comprises transition metal ions in a concentration from 0.03 M to 1 M in addition to any transition metals ions that may be in the per-compound permanganate oxidizer.

### Claim 5 (depends on 1)

The method of claim 1, wherein the polishing pad comprise a polymeric pad having a Shore D hardness less than 100, and wherein a polishing pressure used for the pressing is less than 15 psi.

### Claim 6 (depends on 1)

The method of claim 1, wherein the buffering agent comprises the surfactant, and wherein the surfactant is an anionic surfactant having a concentration from 0.01 grams per liter to 20 grams per liter.

### Claim 7 (depends on 1)

The method of claim 1, wherein the slurry solution further comprises at least one alkali metal ion besides an alkali metal ion in the per-compound permanganate oxidizer if the per-compound permanganate oxidizer includes an alkali metal ion.

### Claim 8

A method of chemical mechanical polishing (CMP) hard surfaces, comprising:
providing a slurry solution comprising:
an aqueous medium,
at least one per-compound permanganate oxidizer with a concentration between 0.01 M and 2 M,
a pH level from 1.5 to 5,
at least one buffering agent different from the per-compound oxidizer, the buffering agent comprising at least one of a surfactant and an alkali metal ion,
the slurry solution being exclusive of any added particles,
dispensing the slurry solution on a hard surface having a Vickers hardness>1,000 kg/mm2,
pressing with a polishing pad with the slurry solution on the hard surface in between while rotating the polishing pad relative to the hard surface, and
wherein the slurry solution includes in situ soft particles formed by a decomposition of the per-compound permanganate oxidizer to form MnO2 particles that have a Mohs hardness less than or equal to (≤) 3.

### Claim 9 (depends on 8)

The method of claim 8, wherein the polishing pad comprise a polymeric pad having a Shore D hardness less than 100, and wherein a polishing pressure used for the pressing is less than 15 psi.

### Claim 10 (depends on 8)

The method of claim 8, wherein the hard surface comprises a carbide, a nitride, or a mixture thereof.

### Claim 11 (depends on 8)

The method of claim 8, wherein the buffering agent comprises the surfactant, and wherein the surfactant is an anionic surfactant having a concentration from 0.01 grams per liter to 20 grams per liter.