# US 2020/0090977 A1 · Temporary bonding method with thermoplastic adhesive incorporating a rigid ring

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0090977 A1
- Document ID: US20200090977A1
- Status: Published application
- Kind: A1
- Application number: 16/570,296
- Filed: 2019-09-13
- Published: 2020-03-19
- Earliest claimed: 2018-09-14
- Assignees: Commissariat A L'energie Atomique Et Aux Energies Alternatives
- Applicants: Commissariat à L'éNergie Atomique Et Aux éNergies Alternatives
- Inventors: Pierre Montmeat; Frank Fournel; Marc Zussy
- Web page: https://patentgrep.com/patent/US20200090977A1

## CPC

- C09J 5/06: involving heating of the applied adhesive
- H10P 72/7402: {Wafer tapes, e.g. grinding or dicing support tapes}
- C09J 5/02: involving pretreatment of the surfaces to be joined
- H10P 52/00: Grinding, lapping or polishing of wafers, substrates or parts of devices
- C09J 2203/326: for bonding electronic components such as wafers, chips or semiconductors
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for the temporary bonding of a substrate of interest to a handle substrate, comprising a step of forming an assembly by placing the bonding faces of the substrate of interest and of the handle substrate into contact with one another via a thermoplastic polymer, and a step of treating the assembly at a treatment temperature that exceeds the glass transition temperature of the thermoplastic polymer. Prior to the assembly forming step, this method comprises: a step of producing, at the bonding face of one of either the substrate of interest or the handle substrate, a central cavity surrounded by a peripheral ring made of a material that is rigid at the treatment temperature, and a step of forming a layer of the thermoplastic polymer filling the central cavity.

## Claims

### Claim 1

A method of temporary bonding of a substrate of interest to a handle substrate, comprising:
a step of forming an assembly by placing bonding faces of the substrate of interest and of the handle substrate into contact with one another via a thermoplastic polymer having a glass transition temperature,
a step of treating the assembly at a treatment temperature that exceeds the glass transition temperature of the thermoplastic polymer,
wherein the method comprises, prior to the step of forming the assembly:
a step of producing, at the bonding face of one of either the substrate of interest or the handle substrate, a central cavity surrounded by a peripheral ring having an upper level and a lower level, the peripheral ring being made of a material that is rigid at the treatment temperature, and
a step of forming a layer of said thermoplastic polymer, said layer filling the central cavity once the assembly has been formed.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the step of producing is carried out such that, once the assembly has been formed, said layer extends above the upper level of the peripheral ring over the entire bonding face having the central cavity and the peripheral ring.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the step of producing comprises thinning of a central part of one of either the substrate of interest or the handle substrate.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the step of producing comprises depositing a band of said rigid material on a peripheral part of one of either the substrate of interest or the handle substrate.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the step of producing comprises forming a layer of said rigid material on one of either the substrate of interest or the handle substrate and thinning a central part of the layer of said rigid material.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the peripheral ring has a width that corresponds to at least 2.5%, preferably at least 5%, of a diameter of the bonding face of the substrate of interest.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the rigid material has a Young's modulus greater than 1 MPa.

### Claim 8 (depends on 1)

The method according to claim 1, further comprising a step of trimming a peripheral part of the substrate of interest.

### Claim 9 (depends on 1)