# US 2020/0090937 A1 · Method for manufacturing semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0090937 A1
- Document ID: US20200090937A1
- Status: Published application
- Kind: A1
- Application number: 16/324,220
- Filed: 2017-09-28
- Published: 2020-03-19
- Earliest claimed: 2016-10-13
- Assignees: Mitsubishi Electric Corporation
- Applicants: Mitsubishi Electric Corporation
- Inventors: Kazunari NAKATA
- Web page: https://patentgrep.com/patent/US20200090937A1

## CPC

- H10D 64/0115: {to silicon carbide}
- B23K 26/21: by welding
- H10D 30/0291: {of vertical DMOS [VDMOS] FETs}
- H10D 30/60: Insulated-gate field-effect transistors [IGFET] (H10D30/40 takes precedence)
- H10D 30/66: Vertical DMOS [VDMOS] FETs
- H10D 62/8325: {Silicon carbide}
- H10P 14/47: Electrolytic deposition, i.e. electroplating; Electroless plating
- H10P 52/00: Grinding, lapping or polishing of wafers, substrates or parts of devices
- H10P 72/0448: {Apparatus for applying a liquid, a resin, an ink or the like}
- H10P 72/0604: {Process monitoring, e.g. flow or thickness monitoring}
- H10D 62/127: {of cellular field-effect devices, e.g. multicellular DMOS transistors or IGBTs}
- H10D 62/157: {Impurity concentrations or distributions}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Included herein are, a step of forming an active region for a semiconductor device on a front surface of a SiC substrate, a step of forming a SiC substrate-to-drain electrode bonding region on a back surface of the SiC substrate by grinding it using an abrasive whose average abrasive grain size is within a specified range, a step of depositing a film of a first drain electrode on the SiC substrate-to-drain electrode bonding region, a step of electrically connecting the first drain electrode with the SiC substrate-to-drain electrode bonding region, and a step of depositing a film of a second drain electrode on the first drain electrode, so that a SiC semiconductor device having a high mechanical strength with a reduced energization loss is achieved.

## Claims

### Claim at position 1

1-5. (canceled)

### Claim 6

A method for manufacturing a semiconductor device, comprising:
a first grinding step of grinding, using an abrasive, a back-surface side of a SiC substrate having an active region formed on a front-surface side thereof;
a second grinding step of grinding a back-surface side of the SiC substrate provided after the first grinding step, using an abrasive having an average abrasive grain size of not less than 1 μm and not more than 5 μm;
a step of depositing a film of a first main electrode on an electrode bonding region formed by the second grinding step;
a step of electrically connecting the first main electrode with the electrode bonding region by using laser irradiation; and
a step of depositing a film of a second main electrode on the first main electrode subjected to the laser irradiation,
wherein a grinding amount of the SiC substrate for grinding the back-surface side by the first grinding step and the second grinding step is 250 μm or more; and
wherein a thickness of the SiC substrate becomes not less than 50 μm and not more than 150 μm.

### Claim 7 (depends on 6)

The method for manufacturing a semiconductor device of claim 6, wherein the second grinding step is a last grinding step.

### Claim 8 (depends on 6)

The method for manufacturing a semiconductor device according to claim 6, wherein irradiation energy of a laser that is used at the time of electrically connecting the first main electrode with the electrode bonding region by using the laser irradiation, is not less than 0.5 J/cm2 and not more than 3.0 J/cm2.

### Claim 9 (depends on 7)

The method for manufacturing a semiconductor device according to claim 7, wherein irradiation energy of a laser that is used at the time of electrically connecting the first main electrode with the electrode bonding region by using the laser irradiation, is not less than 0.5 J/cm2 and not more than 3.0 J/cm2.

### Claim 10 (depends on 6)

The method for manufacturing a semiconductor device according to claim 6, wherein the first main electrode has a thickness of not less than 10 nm and not more than 200 nm.

### Claim 11 (depends on 7)

The method for manufacturing a semiconductor device according to claim 7, wherein the first main electrode has a thickness of not less than 10 nm and not more than 200 nm.

### Claim 12 (depends on 8)

The method for manufacturing a semiconductor device according to claim 8, wherein the first main electrode has a thickness of not less than 10 nm and not more than 200 nm.

### Claim 13 (depends on 9)

The method for manufacturing a semiconductor device according to claim 9, wherein the first main electrode has a thickness of not less than 10 nm and not more than 200 nm.

### Claim 14 (depends on 6)

The method for manufacturing a semiconductor device according to claim 6, wherein the second main electrode has a thickness that is not less than 10 times and not more than 50 times that of the first main electrode.

### Claim 15 (depends on 7)

The method for manufacturing a semiconductor device according to claim 7, wherein the second main electrode has a thickness that is not less than 10 times and not more than 50 times that of the first main electrode.

### Claim 16 (depends on 8)

The method for manufacturing a semiconductor device according to claim 8, wherein the second main electrode has a thickness that is not less than 10 times and not more than 50 times that of the first main electrode.

### Claim 17 (depends on 9)

The method for manufacturing a semiconductor device according to claim 9, wherein the second main electrode has a thickness that is not less than 10 times and not more than 50 times that of the first main electrode.

### Claim 18 (depends on 10)

The method for manufacturing a semiconductor device according to claim 10, wherein the second main electrode has a thickness that is not less than 10 times and not more than 50 times that of the first main electrode.

### Claim 19 (depends on 11)

The method for manufacturing a semiconductor device according to claim 11, wherein the second main electrode has a thickness that is not less than 10 times and not more than 50 times that of the first main electrode.

### Claim 20 (depends on 12)

The method for manufacturing a semiconductor device according to claim 12, wherein the second main electrode has a thickness that is not less than 10 times and not more than 50 times that of the first main electrode.

### Claim 21 (depends on 13)

The method for manufacturing a semiconductor device according to claim 13, wherein the second main electrode has a thickness that is not less than 10 times and not more than 50 times that of the first main electrode.

### Claim 22 (depends on 6)

The method for manufacturing a semiconductor device according to claim 6, wherein the first main electrode and the second main electrode are made of nickel.

### Claim 23 (depends on 7)

The method for manufacturing a semiconductor device according to claim 7, wherein the first main electrode and the second main electrode are made of nickel.

### Claim 24 (depends on 8)

The method for manufacturing a semiconductor device according to claim 8, wherein the first main electrode and the second main electrode are made of nickel.

### Claim 25 (depends on 9)

The method for manufacturing a semiconductor device according to claim 9, wherein the first main electrode and the second main electrode are made of nickel.