Back to results
US 2020/0038841 A1Published application
NOx Trap Catalyst Support Material Composition
AssigneeSasol Germany GmbH
InventorsMarcos Schoneborn, Dirk Niemeyer, Thomas Harmening, Sandra Fibikar
Life of this patent
Estimating the term…
Abstract
The present invention relates to a method of making a support material composition comprising an Mg/Al oxide, a cerium oxide and at least another rare earth element oxide, to a support material composition and to the use of the support material composition as a nitrogen oxide storage component within a catalyst for treating exhaust gases to reduce NOx content.
Claims18
A method of preparing a support material composition, the composition comprising two phases:
- a first phase comprising a Mg/Al mixed oxide;
- and
- a second phase comprising a cerium based oxide, and rare-earth element(s) based oxide other than cerium oxide, wherein the second phase is a solid-solution;
- the method comprising the following steps:
- i) preparing an aqueous suspension of a Mg/Al mixed oxide precursor;
- ii) preparing an aqueous solution of a cerium salt;
- iii) preparing an aqueous solution of one or more rare-earth element oxides salt(s) other than cerium salts;
- iv) combining, in any order, at least the aqueous suspension in step i), with the aqueous solution in step ii), and the aqueous solution of step iii) to form an aqueous mixture;
- v) dying the aqueous mixture to form a dried particulate material;
- and
- vi) calcining the dried particulate material;
- wherein the content of the one or more rare-earth element salt(s) other than cerium is between 5 and 50 wt. %, relative to the sum of
- the cerium salts from the aqueous solution of step ii) and
- the rare earth element salt(s) other than cerium salts from the aqueous solution of step iii) and,
- wherein each of the salts are calculated as their oxides.
12 more elements
A support material composition comprising two phases:
- i) a first phase comprising a Mg/Al mixed oxide;
- and
- ii) a second phase comprising a cerium based oxide, and rare-earth element(s) based oxide other than cerium oxide, wherein the second phase is a solid-solution;
- the content of the first phase being at least 50 wt. % of the total support material composition,
- wherein the amount of Mg in the first phase is between 1 and 40 wt. %, calculated as MgO based on the weight of the first phase, calculated as MgO and Al2O3;
- and wherein the content of the rare-earth element(s) oxide other than cerium oxide in the second phase is between 5 and 50 wt. %,
- calculated as the rare earth element(s) oxide other than cerium relative to the total second phase.
4 more elements
Dependencies are inferred from the claim text.