# US 2020/0006770 A1 · Transition metal composite hydroxide particles and production method thereof, cathode active material for non-aqueous electrolyte rechargeable battery and production method thereof, and nonaqueous electrolyte rechargeable battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0006770 A1
- Document ID: US20200006770A1
- Status: Published application
- Kind: A1
- Application number: 16/539,170
- Filed: 2019-08-13
- Published: 2020-01-02
- Earliest claimed: 2013-05-10
- Assignees: Sumitomo Metal Mining Co., Ltd.
- Applicants: Sumitomo Metal Mining Co., Ltd.
- Inventors: Yasutaka KAMATA; Taira AIDA; Hiroyuki TOYA
- Web page: https://patentgrep.com/patent/US20200006770A1

## CPC

- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- C01G 53/84: Hydroxides
- C30B 1/04: Isothermal recrystallisation
- C30B 1/10: by solid state reactions or multi-phase diffusion
- C30B 7/14: the crystallising materials being formed by chemical reactions in the solution
- C30B 29/10: Inorganic compounds or compositions
- C30B 29/22: Complex oxides
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 10/052: Li-accumulators
- C01P 2004/03: obtained by SEM
- C01P 2004/20: extending in two dimensions, e.g. plate-like
- C01P 2004/50: Agglomerated particles
- C01P 2004/51: Particles with a specific particle size distribution
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- H01M 2004/028: {Positive electrodes}
- H01M 2220/20: Batteries in motive systems, e.g. vehicle, ship, plane
- H01M 2220/30: Batteries in portable systems, e.g. mobile phone, laptop
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Provided is a cathode active material that can simultaneously improve the capacity characteristics, output characteristics, and cycling characteristics of a rechargeable battery when used as cathode material for a non-aqueous electrolyte rechargeable battery. After performing nucleation by controlling an aqueous solution for nucleation that includes a metal compound that includes at least a transition metal and an ammonium ion donor so that the pH value becomes 12.0 to 14.0 (nucleation process), nuclei are caused to grow by controlling aqueous solution for particle growth that includes the nuclei so that the pH value is less than in the nucleation process and is 10.5 to 12.0 (particle growth process). When doing this, the reaction atmosphere in the nucleation process and at the beginning of the particle growth process is a non-oxidizing atmosphere, and in the particle growth process, atmosphere control by which the reaction atmosphere is switched from this non-oxidizing atmosphere to an oxidizing atmosphere, and is then switched again to a non-oxidizing atmosphere is performed at least one time. Cathode active material is obtained with the composite hydroxide particles that are obtained by this kind of crystallization reaction as a precursor.

## Claims

### Claim 1

A production method for producing transition metal composite hydroxide particles by a crystallization reaction to be a precursor for a cathode active material for a non-aqueous electrolyte rechargeable battery, comprising:
a nucleation process for performing nucleation by controlling an aqueous solution for nucleation that includes a metal compound that includes at least a transition metal and an ammonium ion donor so that the pH value at a standard liquid temperature of 25° C. becomes 12.0 to 14.0; and
a particle growth process for causing nuclei to grow by controlling an aqueous solution for particle growth that includes the nuclei that were obtained in the nucleation process so that the pH value is less than in the nucleation process and is 10.5 to 12.0;
the reaction atmosphere in the nucleation process and at the beginning of the particle growth process being a non-oxidizing atmosphere in which an oxygen concentration is 5% by volume or less; and
in the particle growth process, atmosphere control by which the reaction atmosphere is switched from the non-oxidizing atmosphere to an oxidizing atmosphere in which the oxygen concentration is greater than 5% by volume at timing from the start of the particle growth process within a range of 5% to 35% of the overall particle growth process time, and is then switched from the oxidizing atmosphere to a non-oxidizing atmosphere in which the oxygen concentration is 5% by volume or less so that the crystallization time in the oxidizing atmosphere in the particle growth process is 3% to 20% of the overall particle growth process time being performed at least one time.

### Claim 2

A production method for producing transition metal composite hydroxide particles by a crystallization reaction to be a precursor for a cathode active material for a non-aqueous electrolyte rechargeable battery, comprising:
a nucleation process for performing nucleation by controlling an aqueous solution for nucleation that includes a metal compound that includes at least a transition metal and an ammonium ion donor so that the pH value at a standard liquid temperature of 25° C. becomes 12.0 to 14.0; and
a particle growth process for causing nuclei to grow by controlling an aqueous solution for particle growth that includes the nuclei that were obtained in the nucleation process so that the pH value is less than in the nucleation process and is 10.5 to 12.0;
the reaction atmosphere in the nucleation process and at the beginning of the particle growth process being a non-oxidizing atmosphere in which the oxygen concentration is 5% by volume or less;
in the particle growth process, atmosphere control by which the reaction atmosphere is switched from the non-oxidizing atmosphere to an oxidizing atmosphere in which the oxygen concentration is greater than 5% by volume, and is then switched from that oxidizing atmosphere to a non-oxidizing atmosphere in which the oxygen concentration is 5% by volume or less being performed two times or more; and
the total crystallization reaction time in the oxidizing atmosphere in the particle growth process being 3% to 30% of the total particle growth process time, and the crystallization reaction time during each oxidizing atmosphere being 1% or more of the total particle growth process time.

### Claim 3 (depends on 2)

The production method for producing transition metal composite hydroxide particles according to claim 2, wherein in the particle growth process, the reaction atmosphere is switched from the non-oxidizing atmosphere to the oxidizing atmosphere at timing from the start of the particle growth process within a range of 5% to 35% of the overall particle growth process time.

### Claim 4 (depends on 1)

The production method for producing transition metal composite hydroxide particles according to claim 1, wherein the transition metal composite hydroxide particles are transition metal composite hydroxide particles that are expressed by the general expression (A): NixMnyCozMt(OH)2+a, where x+y+z+t=1, 0.3≤x≤0.95, 0.05≤y≤0.55, 0≤z≤0.4, 0≤t≤0.1, 0≤a≤0.5, and M is one or more additional element that is selected from among Mg, Ca, Al, Ti, V, Cr, Zr, Nb, Mo, Hf, Ta and W.

### Claim 5 (depends on 4)

The production method for producing transition metal composite hydroxide particles according to claim 4, further comprising a coating process for coating the transition metal composite hydroxide particles with a compound that includes the additional element M after the particle growth process.

### Claim 6

Transition metal composite hydroxide particles that are the precursor for cathode active material for a non-aqueous electrolyte rechargeable battery, comprising secondary particles that are formed by an aggregation of plate-shaped primary particles and fine primary particles that are smaller than the plate-shaped primary particles;
the secondary particles having a center section that is formed by an aggregation of the plate-shaped primary particles, and one layered structure of a low-density section that is formed by an aggregation of the fine primary particles and a high-density section that is formed by an aggregation of the plate-shaped primary particles on the outside of the center section;
the average value of the ratio of the center section outer diameter with respect to the particle size of the secondary particles being 30% to 80%, and the average value of the high-density section radial direction thickness with respect to the particle size of the secondary particles being 5% to 25%; and
the secondary particles having an average particle size of 1 μm to 15 μm, and an index [(d90−d10)/average particle size] that indicates the extent of the particle size distribution of 0.65 or less.

### Claim 7

Transition metal composite hydroxide particles that are the precursor for cathode active material for a non-aqueous electrolyte rechargeable battery, comprising secondary particles that are formed by an aggregation of plate-shaped primary particles and fine primary particles that are smaller than the plate-shaped primary particles;
the secondary particles having a center section that is formed by an aggregation of plate-shaped primary particles, and two or more layered structure of a low-density section that is formed by an aggregation of the fine primary particles and a high-density section that is formed by an aggregation of the plate-shaped primary particles on the outside of the center section; and
the secondary particles having an average particle size of 1 μm to 15 μm, and an index [(d90−d10)/average particle size] that indicates the extent of the particle size distribution of 0.65 or less.

### Claim 8 (depends on 7)

The transition metal composite hydroxide particles according to claim 7, wherein the average value of the ratio of the center section outer diameter with respect to the particle size of the secondary particles is 20% to 70%, and the average value of the high-density section radial direction thickness per layer with respect to the particle size of the secondary particles is 5% to 25%.

### Claim 9 (depends on 6)

The transition metal composite hydroxide particles according to claim 6, wherein the transition metal composite hydroxide particles are transition metal composite hydroxide particles that are expressed by the general expression (A): NixMnyCozMt(OH)2+a, where, x+y+z+t=1, 0.3≤x≤0.95, 0.05≤y≤0.55, 0≤z≤0.4, 0≤t≤0.1, 0≤a≤0.5, and M is one or more additional element that is selected from among Mg, Ca, Al, Ti, V, Cr, Zr, Nb, Mo, Hf, Ta and W).

### Claim 10 (depends on 9)

The transition metal composite hydroxide particles according to claim 9, wherein the additional element is uniformly distributed inside the secondary particles and/or coated on the surface of the secondary particles.

### Claim 11 (depends on 6)

A production method for producing cathode active material for a non-aqueous electrolyte rechargeable battery comprising:
a mixing process for forming a lithium mixture by mixing the transition metal composite hydroxide particles according to claim 6 with a lithium compound; and
a calcination process for performing calcination of the lithium mixture formed in the mixing process at a temperature of 650° C. to 980° C. in an oxidizing atmosphere.

### Claim 12 (depends on 11)

The production method for producing cathode active material for a non-aqueous electrolyte rechargeable battery according to claim 11, wherein in the mixing process the lithium mixture is adjusted so that the ratio of the sum of the number of atoms of metals other than lithium included in the lithium mixture, and the number of atoms of lithium is 1:0.95 to 1.5.

### Claim 13 (depends on 12)

The production method for producing cathode active material for a non-aqueous electrolyte rechargeable battery according to claim 12, further comprising a heat treatment process for heat treating the transition metal composite hydroxide particles at 105° C. to 750° C. before the mixing process.

### Claim 14 (depends on 11)

The production method for producing cathode active material for a non-aqueous electrolyte rechargeable battery according to claim 11, wherein the cathode active material comprises layered hexagonal crystal lithium nickel manganese composite oxide particles that are expressed by the general expression (B): Li1+uNixMnyCozMtO2, where −0.05≤u≤0.50, x+y+z+t=1, 0.3≤x≤0.95, 0.05≤y≤0.55, 0≤z≤0.4, 0≤t≤0.1, and M is one or more additional element that is selected from among Mg, Ca, Al, Ti, V, Cr, Zr, Nb, Mo, Hf, Ta and W.