# US 2020/0006736 A1 · Method for producing laminated type battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0006736 A1
- Document ID: US20200006736A1
- Status: Published application
- Kind: A1
- Application number: 16/480,184
- Filed: 2017-12-18
- Published: 2020-01-02
- Earliest claimed: 2017-01-26
- Assignees: Envision AESC Energy Devices Ltd.
- Applicants: Envision AESC Energy Devices Ltd.
- Inventors: Ryota YANAGISAWA
- Web page: https://patentgrep.com/patent/US20200006736A1

## CPC

- H01M 10/0413: {Large-sized flat cells or batteries for motive or stationary systems with plate-like electrodes}
- H01M 50/46: Separators, membranes or diaphragms characterised by their combination with electrodes
- H01M 8/0236: Glass; Ceramics; Cermets
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 50/423: Polyamide resins
- H01M 50/437: Glass
- H01M 50/44: Fibrous material
- H01M 50/463: Separators, membranes or diaphragms characterised by their shape
- H01M 50/434: Ceramics
- H01M 50/443: Particulate material
- H01M 50/489: Separators, membranes, diaphragms or spacing elements inside the cells, characterised by their physical properties, e.g. swelling degree, hydrophilicity or shut down properties
- H01M 50/491: Porosity
- H01M 2220/20: Batteries in motive systems, e.g. vehicle, ship, plane
- Y02E 60/10: Energy storage using batteries
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

There is provided a method for producing a laminated type battery including a separator and electrode sheets arranged in lamination through the separator, the method including subjecting a charged separator to a charge neutralization treatment to thereby reduce a charge voltage thereof, and laminating the separator having the reduced charge voltage on the electrode sheet.

## Claims

### Claim 1

A method for producing a laminated type battery comprising a separator and electrode sheets arranged in lamination through the separator, the method comprising:
subjecting a charged separator to a charge neutralization treatment to thereby reduce a charge voltage thereof; and
laminating the separator having the reduced charge voltage on the electrode sheet.

### Claim 2 (depends on 1)

The method according to claim 1, comprising a step of laminating another electrode sheet on the separator having the reduced charge voltage.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the charge voltage of the separator having the reduced charge voltage is lower than 10 kV.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the charge voltage of the separator having the reduced charge voltage is at least 0.5 kV.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the separator has a relative dielectric constant of 3 or higher.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the separator is an aramid separator or a glass nonwoven fabric separator.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the separator is an aramid separator.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the charge neutralization treatment is carried out by using an ionizer.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the charged separator before the charge neutralization treatment is a separator having been placed in a dry atmosphere having a relative humidity of 5% or lower.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the charged separator before the charge neutralization treatment is a separator having been unwound from a rolled state and having been cut.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the charged separator before the charge neutralization treatment is a separator having been peeled off from a laminated state.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the laminating is carried out in a dry atmosphere having a relative humidity of 5% or lower.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the laminated type battery is a lithium-ion secondary battery.